                    以柳钢360m^(2)烧结机实际生产为基础,针对烧结工序能耗偏高,从厚料层烧结工艺升级、微负压烧结改造,降低煤气用量、减少台车漏风率,提高环冷机密封性等方面作出优化调整后,使得料层厚度由750mm提高至820mm。结果表明:经改造后烧结矿转鼓强度提高了0.76%,返矿率降低了2.19%,工序能耗由51.93kgce/t降低至40.51kgce/t。
                
                Based on the actual production of Liusteel 360 m^(2)sintering machine,aiming at the high energy consumption of sintering process,the thickness of the material layer was increased from 750 mm to 820 mm after optimization and adjust-ment from the upgrading of sintering process of thick material layer,the transformation of micro-negative pressure sintering,the reduction of gas consumption,the reduction of air leakage rate of the truck,and the improvement of sealing property of the ring cooler.The results show that the rotary drum strength of the sinter is increased by O.76%,the return rate is reduced by 2.19%,and the process energy consumption is reduced from 51.93 kgce/t to 40.51 kgce/t.
    
    
                作者
                    赵书清
                    宋阳
                    刘巍
                    徐忱
                    杨鹏晟
                ZHAO Shuqing;SONG Yang;LIU Wei;XU Chen;YANG Pengsheng(Liuzhou Iron&Steel Co.Ltd.,Sintering Plant,Liuzhou 505000,China)
     
    
    
                出处
                
                    《甘肃冶金》
                        
                        
                    
                        2024年第2期18-20,共3页
                    
                
                    Gansu Metallurgy
     
    
                关键词
                    工序能耗
                    厚料层烧结
                    微负压烧结
                    转鼓强度返矿率
                
                        process energy consumption
                        thick layer sintering
                        micro-negative pressure sintering
                        drum strength
                        rate of minereturn
                
     
    
    
                作者简介
赵书清(1997-),女,贵州省从江县人,助理工程师,本科。主要从事烧结球团工作。