摘要 针对冷镦钢SWRCH35K盘条开裂情况,通过对冶炼、轧制等生产工艺和产品质量进行跟踪,同时采用盘条表面酸洗及金相检验等手段对开裂盘条进行了宏观和金相组织观察,分析出连铸坯表面存在角部裂纹是造成开裂的主要因素,并提出了减少盘条表面裂纹的解决措施。 Because of the circumstance that SWRCH35K steel wire rod cracking of cold heading steel occurred,we did the tracking of quality,smelting,rolling and the other production processes,at the same time,we did acid pickling and metallographic testing and the other manners on wire strip surface,we also did the observation on macroscopic and metallographic organization of cracking steel wire rod,therefore,we analyzed the major reason of cracking is corner cracking occurred on the surface of continuous casting billet,and we proposed the resolutions for decreasing the surface cracking of steel wire rod.
作者 陆继欢 陶群南 赵满堂 史杨 林作津 刘志勇 LU Ji-huan;TAO Qun-nan;ZHAO Man-tang;SHI Yang;LIN Zuo-jin;LIU Zhi-yong(Wuhu Xinxing Ductile Iron Pipes Co.,Ltd.,Wuhu,Anhui 241000,China)
出处 《云南冶金》 2022年第1期91-95,共5页 Yunnan Metallurgy
关键词 冷镦钢 SWRCH35K 开裂 盘条 cold heading steel SWRCH35K cracking steel wire rod
作者简介 陆继欢(1989-),男,云南曲靖人,工程师,主要从事冷镦钢产品开发及产品质量提升工作。
  • 相关文献

参考文献4

二级参考文献17

共引文献11

同被引文献14

引证文献2

二级引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部