摘要 综述了聚硅氧烷热老化机理和提高热稳定性的途径。聚硅氧烷的老化机理主要来源于热解聚和热氧化降解过程。提高聚硅氧烷耐热性的途径主要是改变端基、主链的分子结构,也可以在聚硅氧烷体系中添加耐热添加剂。 The thermal aging mechanism of polysiloxanes and methods applicable for improving their thermal stabil- ities were reviewed. The thermal aging conduct was resulted from thermal depolymerization and thermo-oxidative degrada- tion process. The thermal stabilities of polysiloxanes could be enhanced either by structure modification initiated from vari- ation of terminal group for polymer molecule and the molecule structure of main chain, or by the addition of some kinds of heat-resistant additives.
出处 《化工新型材料》 CAS CSCD 北大核心 2010年第1期17-19,43,共4页 New Chemical Materials
基金 教育部2008年重点科研项目(208183) 浙江省自然科学基金项目(Y4080264)资助
关键词 聚硅氧烷 热稳定性 热解聚 热氧化降解 polysiloxane, thermal stability, thermal depolymerization, thermo-oxidative degradation
作者简介 作者简介:金晶(1983-),女,在读硕士研究生,研究方向为有机硅化学及材料。
  • 相关文献

参考文献29

  • 1Grassie N, Macfarlane I G. The thermal degradation of polysiloxanes- I : poly(dimethylsiloxane) [J]. Eur Polym J, 1978,14 (11) :875-884.
  • 2Bannister D J, Semlyen J A. Studies of cyclic and linear poly (dimethyl siloxanes) : 6. Effect of heat[J]. Polymer, 1981, 22 :377-381.
  • 3Patnode W, Wilcock D F. Methylpolysiloxanes[J]. J Am Chem Soc, 1946, 68 (3):358-363.
  • 4Thomas H, Kendrick T C. Thermal analysis of polydimethylsiloxanes. I. Thermal degradation in controlled atmospheres[J]. Journal of Polymer Science Part A-2: Polymer Physics, 1969,7 ( 3): 537-549.
  • 5Grassie N, Macfarlane I G, Franeey K F. The thermal degradation of polysiloxanes-Ⅱ : poly (methylphe-nylsiloxane) [J]. Eur Polym J, 1979,15(5): 415- 422.
  • 6Grassie N, Francey K. F. The thermal degradation of polysiloxanes Part3: poly ( dimethyl/methylphenyl-siloxane ) [ J ]. Polym Degrad Stab, 1980,2 (1): 53-66.
  • 7Grassie N, Macfarlane I G, Franeey K F. The thermal degradation of polysiloxanes Part 4: poly (dimethyl/diphenylsiloxane) [J]. Polym Degrad Stab, 1980,2 (1) :67-83.
  • 8Rakhakrishan T S. New method for evaluation of kinetic parameters and mechanism of degradation from pyrolysis-GC Studies:Thermal Degradation of Polydimethylsiloxanes[J]. J Appl Polym Sci, 1999,73(3) : 441-450.
  • 9李拥有,盘毅,谢凯.端环氧基聚二甲基硅氧烷的合成及表征[J].精细化工中间体,2004,34(1):23-25. 被引量:11
  • 10伍川,金晶,蒋剑雄,来国桥,邱化玉.甲基二苯基封端硅油的制备及其热性能研究[J].有机硅材料,2007,21(5):258-262. 被引量:15

二级参考文献35

共引文献160

同被引文献187

引证文献15

二级引证文献110

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部