低温烧结高钨高比重合金的特性及其抗腐蚀性能 被引量:7

CHARACTERISTICS AND CORROSION RESISTANT PROPERTY OF HIGH TUNGSTEN HEAVY ALLOY SINTERED AT LOW TEMPERATURE
在线阅读 下载PDF
导出
摘要 研究了以高活性W、Ni、Cu复合粉末为原料,钨含量为93%(Wt)的高比重合金的低温烧结工艺特性、形变与断裂特性、强度与抗腐蚀性能。合金在1240℃的温度下进行低温烧结后,抗拉强度可高达950MPa,钨晶粒平均粒径小于5μm,具有明显的晶粒尺寸效应,有利于提高合金的强度、密度及其均匀性;合金还具有较好的抗腐蚀性能。 The paper has studied the technological characteristics, deformation, fracture, strengthand corrosion resistence of heavy alloy with high activity composite powder of W,Ni and Cu asraw material and with93% (wt) of tungsten content. After the alloy is sintered at a low temperature of 1240℃,its high tensile strenght as high as 950MPa can be obtained with an average grainsize of tungsten below 5μm which produce obvious grain sire effect,aiding in the improvement ofstrenth,density and homogeneity of alloy and also betterment of the corrosion resistence of alloy.
机构地区 中南工业大学
出处 《粉末冶金技术》 EI CSCD 北大核心 1996年第1期37-43,共7页 Powder Metallurgy Technology
关键词 低温烧结 高比重合金 耐蚀性 钨基合金 粉末 sintering at low temperature heavy alloy corrosion resistence
  • 相关文献

参考文献1

  • 1黄建忠,稀有金属材料与工程,1983年,5卷,10期

同被引文献54

引证文献7

二级引证文献57

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部