摘要
提出了一种全新的纳米材料制备方法—支撑液膜法。常温常压条件下,在0.2mol/L的CuCl_2溶液和0.2mol/L的Na_2S溶液、以及含邻菲罗啉载体的支撑液膜组成的共同反应体系中进行反应,成功制备出Cu_7S_4纳米晶。经XRD、TEM等表征,产物的粒径范围为5~10nm,结构为六方晶型,晶胞参数为a=15.475、c=13.356.本文还对其光学性质及产物形成机理进行了初步探讨.
A novel fabrication method of Cu7S4 nano-crystals by supported liquid membrane (SLM) system was investigated. SLM consists of CHCl3 as solvent, o-phenanthroline as a mobile carrier and polymer membrane as supported template. The results indicated that Cu7S4 which has hexagonal structure with cell constant of a=15.475Angstrom and C=13.356Angstrom can be prepared at room temperature with 0.2mol/L CuCl2 and 0.2mol/L Na2S as reactants. The average size of Cu7S4 is about 7nm. In addition, the forming mechanism and optical properties of Cu7S4 were discussed.
出处
《无机材料学报》
SCIE
EI
CAS
CSCD
北大核心
2004年第3期487-491,共5页
Journal of Inorganic Materials
基金
国家自然科学基金(20071025)
上海市科技发展基金纳米专项(0259nm021
0114nm004)
关键词
支撑液膜
纳米晶
Cu7S4
流动载体
supported liquid membrane
nano-crystals
Cu7S4
mobile carrier