摘要
针对金选厂磨机衬板磨损快、浮选柱作业故障率高、碎磨电能损耗较高、精矿浓密沉降效果差及采矿疏干水未利用等问题,采取了针对性措施,不仅技术指标提高,而且经济效益增加349.93万元/a,有利减少碳排放。
The mill lining of the gold dressing plant wears out quickly,the flotation column has a high operation failure rate,high electric energy loss for crushing and grinding,poor sedimentation effect of concentrate thickening and unutilized deposit drainage water,so the corresponding measures were taken,then not only the technical indicators were increased,and the economic benefits were increased by¥3.4993 million yuan per year,it is conducive to reducing carbon emissions.
作者
刘泽洪
白俊智
刘显华
李欢
曾继祥
LIU Ze-hong;BAI Jun-Zhi;LIU Xian-hua;LI Huan;ZENG Ji-xiang(Wenshan Malipo Zijin Tungsten Group Co.,Ltd.,Malipo,Yunnan 663600,China;Zijin Mining Group Co.,Ltd,Shanghang,Fujian 364200,China)
出处
《云南冶金》
2024年第2期166-170,180,共6页
Yunnan Metallurgy
关键词
金选厂
节能降耗
磨机衬板
无功补偿
浮选柱
精矿浓密
采矿疏干水
gold dressing plant
energy conservation and consumption reduction
mill lining
reactive power compensation
flotation column
concentrate thickening
deposit drainage water
作者简介
刘泽洪(1978-),男,江西南康人,工程师,主要从事选矿技术研究与生产管理工作;通信作者:白俊智(1977-),男,河北南皮人,高级工程师,从事金属与非金属矿山选矿技术研究及生产管理工作,E-mail:baijz2007@163.com。