摘要
将亚麻打成麻以 9.5mm、15 .8mm的长度切断后 ,经过脱胶漂白及梳理机梳理后 ,亚麻短纤维手感柔软、松散、洁白 ,与木浆纤维以 5 0∶5 0的比例混合经造纸工艺无纺布成形。另可根据不同切断长度 ,与棉、毛、丝、化纤等混纺或无纺布工艺成形。
The raw flax was cut in 9.5 mm and 15.8 mm fiber length,then was cooked and bleached at the same time.After drying and carding,the flax fiber were blended with wood pulp at 50∶50 ratio to produce non woven sheet on paper machine.