锌焙砂含有少量难溶的铁酸锌 ,通过还原焙烧可以降低铁酸锌含量。本文主要探讨还原焙烧温度、时间和煤粉用量对可溶锌含量的影响。
Zinc calcine contains a small amount of refractory zinc ferrite that can be reduced by reduction roasting. This paper explores mainly the influence of reduction roasting temperature, time and pulverized coal consumption on content of soluble zinc.