                    汶川地震断裂带科学钻探项目二号孔(WFSD-2)钻探施工过程中,地层破碎,坍塌、掉块严重,钻进过程中发生多次井漏。为防止固井过程中发生漏失影响固井质量,采用低密度防漏水泥浆常规单级固井工艺。经过多次水泥浆性能试验,调配出了既具有良好流动性、又具有触变性的低密度纤维防漏水泥浆配方。该低密度纤维防漏水泥浆体系在WFSD-2孔168.3 mm套管固井中施工顺利,应用效果良好。
                
                Due to the broken stratum, wall collapsing, landslide accidents and lost circulation happened frequently in the drilling of the second hole of Wenchuan earthquake fault scientific drilling project ( WFSD - 2). For preventing lost circu- lation during cementing, anti-leakage cementing technology with low density slurry was selected. Through multiple perform- ance experiment of slurry, the formulation of low density slurry for anti-leak was optimized. This formulation was successful- ly adopted to cement the 13168.3 casing in WFSD - 2.
    
    
    
    
                出处
                
                    《探矿工程(岩土钻掘工程)》
                        
                        
                    
                        2012年第9期39-40,44,共3页
                    
                
                    Exploration Engineering:Rock & Soil Drilling and Tunneling
     
            
                基金
                    科技部科技支撑计划专项"汶川地震断裂带科学钻探(WFSD)"项目之"科学钻探与科学测井"课题
            
    
                关键词
                    汶川地震
                    地震断裂带
                    科学钻探
                    低密度水泥浆
                    防漏
                    固井
                
                        Wenchuan earthquake 
                         earthquake fault 
                         scientific drilling 
                         low-density slurry 
                         anti-leakage 
                         cementation
                
     
    
    
                作者简介
李前贵(1979-),男(土家族),湖南桑植人,中国地质科学院探矿工艺研究所,石油工程专业,博士,从事钻探工程工作,四川省成都市郫县成都现代工业港(北区)港华路139号,liqiangui@163.com。