摘要
采用蒸发诱导自组装法制备了介孔氧化钨(m-WO3),担载Pt后应用于催化甘油氢解制1,3-丙二醇.结果表明,与商业氧化钨(c-WO3)相比,m-WO3具有高比表面积和易还原的优点,从而使得Pt纳米粒子高度分散于其上.在180oC和5.5MPaH2下反应12h,Pt/m-WO3催化剂上甘油转化率和1,3-丙二醇的选择性分别为18.0%和39.2%,明显高于Pt/c-WO3催化剂.
esoporous tungsten trioxide (m-WO3) was prepared using an evaporation-induced self-assembly method and was used as the support of Pt for hydrogenolysis of glycerol to produce 1,3-propanediol. In comparison with commercial WO3, the m-WO3 presents a much larger surface area and better reducibility, which make the Pt particles highly dispersed on the support. At a reaction condition of 180 ℃, 5.5 MPa H2, and reaction time of 12 h, the Pt/m-WO3 catalyst afforded 18.0% conversion of glycerol and 39.2% selectivity for 1,3-propanediol, both of which are much higher than those on commercial Pt/WO3 catalyst.
出处
《催化学报》
SCIE
EI
CAS
CSCD
北大核心
2012年第8期1257-1261,共5页
基金
国家自然科学基金(21176235)~~
关键词
介孔氧化钨
铂
甘油
氢解
1
3-丙二醇
mesoporous tungsten trioxide
platinum
glycerol
hydrogenolysis
1,3-propanediol
作者简介
通讯联系人.电话:(0411)84379015;电子信箱:taozhang@dicp.ac.cn