对造成板坯浸入式水口穿钢的原因进行了分析,从耐材材质、水口烘烤及作业规范上提出了相应的改进措施。改进后,水口穿钢现象明显减少,取得了良好效果。
In the paper the causes for SEN leakage are analyzed and some countermeasures are stipulated according to refractory quality,preheating effect,process operation and production normal.As a result,the SEN leakage times are simply reduced,and notable effectiveness is achieved.
出处
《河南冶金》
2010年第4期40-42,共3页
Henan Metallurgy
关键词
耐火材料
连铸
性能分析
refractory continue casting properties analysis.