摘要
陶粒混凝土地面最易出现表面不平、起砂、空鼓和裂缝等质量通病。经过多年工程实践,找到了质量通病的具体原因及防治措施。对陶粒混凝土地面的质量标准提出了建议。同时介绍了陶粒混凝土地面的具体施工工艺、成品保护措施及需注意的质量问题。
Ceramisite concrete ground has common quality defects of uneven surface, sugaring, empty and tympanic and cracks. Through several years' practical experience, specific causes and prevention measures on the common quality defects are found out. The authors put forward some advices for quality standards on ceramisite concrete ground. And at the same time, construction process, finished product protection measures and quality problems need to be paid attention on ceramisite concrete ground are introduced.
出处
《施工技术》
CAS
北大核心
2009年第11期104-106,共3页
Construction Technology
关键词
地面
陶粒混凝土
质量通病
预防措施
ground
ceramisite concrete
common quality defect
prevention measure
作者简介
蒋学茂,中国新兴保信建设总公司总工程师,北京市丰台区永定门外东铁营顺八条9号100079,电话:(010)67660078,E-mail:jiangxuemao@126.com