摘要
针对某热液蚀变的接触变质原生硫化铜矿床矿石进行了选矿合理工艺流程和药剂制度的研究。试验研究表明,采用两次粗选、三次精选、两次扫选工艺流程可以获得含铜22.66%、回收率89.14%的技术指标。该工艺流程简单,铜的品位和回收率指标高,且易于工业化生产。
The reasonable technological flow sheet and reagent regime of processing the copper sulphide ore form a certain hydrothermal altered and contact metamorphic primary copper sulphide deposit were researched. The experimental research indicated that such technical indexes as copper content of 22.66% in concentrate and recovery of copper of 89. 14% can be obtained by adopting the technological flow sheet of two - stage roughing, three -stage cleaning and two- stage scavenging. This flow sheet is simple, can achieve high technical indexes ineluding copper concentrate grade and recovery ratio of copper, and is easy to be industrialized.
出处
《矿业研究与开发》
CAS
北大核心
2006年第4期36-38,共3页
Mining Research and Development
关键词
硫化铜矿石
细粒嵌布
浮选
工艺流程
捕收剂
Finely- disseminated copper sulphide ore, Flota- tion, Technological flow sheet, Collector