摘要 利用上海御桥垃圾焚烧厂的焚烧飞灰为主要原料,通过添加SiO2、Al2O3、NaOH组分在实验室研制成功了以硅灰石(wollastonite)为主晶相的微晶玻璃.该体系微晶玻璃制备的最佳工艺条件为:熔融温度1500℃、熔融时间1h,核化温度为920℃,核化时间1.5h,晶化温度为1150~1180℃,晶化时间为2h.研究结果表明,硅灰石为主晶相的微晶玻璃对Pb、Cr和Cd重金属具有很强的稳定束缚能力. By utilizing fly ash from the Shanghai Yuqiao municipal solid waste (MSW) incineration plant as the main raw matefial,wollastonite-based glass-ceramics were successfully synthesized in the laboratory by doping with SiO2 , Al2O3, NaOH as chemical conditioner. The optimum preparation condition for the glass-ceramics is as follows:melting at 1500℃ for 1 hour, nucleating at 920℃ for 90 mins, and crystallization at 1150 - 1180℃ for 120 mins. It is indicated that the wollastonite-based glass-ceramics made from MSW fly ash has a strong fixing capacity for heavy metals such as lead (Pb), chromium( Cr), cadmium(Cd)
出处 《环境科学学报》 CAS CSCD 北大核心 2006年第6期936-943,共8页 Acta Scientiae Circumstantiae
基金 国家科技部创新基金(No.03C26213100902) 上海市重点科研攻关项目(No.0323120432)~~
关键词 城市垃圾焚烧飞灰 微晶玻璃 硅灰石 重金属浸出率 MSW fly ash glassi-ceramic wollastonite leaching rate of heavy metals
作者简介 宋玉(1979-),男,硕士,E-mail:toad1023@263.net,通讯作者
  • 相关文献

参考文献5

二级参考文献9

共引文献50

同被引文献99

引证文献7

二级引证文献33

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部