摘要 抽油杆是有杆抽油中三抽设备的关键部件之一。其服役寿命直接影响油井的产量、失效概率以及修井作业的成本,准确预测其疲劳寿命具有十分重要的意义。对直井和定向井分别建立了计算抽油杆轴向载荷的数学模型,计算出了抽油杆所受的轴向力。同时,建立了疲劳寿命的预测模型,计算了不同形状裂纹的几何形状因子和应力强度因子。并根据以上理论,编写了计算机程序,能计算有初始裂纹和无初始裂纹抽油杆柱的疲劳寿命。采用Form an模型预测抽油杆疲劳寿命,其特点是在Paris模型的基础上考虑了应力比R,计算结果更加准确。同时,分析比较计算结果可得:裂纹初始长度对抽油杆柱的使用寿命影响较大。文中给出的方法简单,精度较高,便于工程应用。 Sucker rod is the key component of the rod pumping system. Its service life has something to do with the quantity of the production,failure rate and work over,and it is very important to predict the fatigue life of sucker rod.The mathematic models to calculate the forces of vertical and deviated well were established.At the same time,the model to calculate the fatigue life was also established.The stress intensity factor of different cracks was calculated in this paper,and developed correspond software,which can succeed in predicting of service life of sucker rod with initial crack or without initial crack.The Forman model is used to predict the fatigue life,compared to the Paris model,the stress ratio is taken into account,so the result is more exact than Paris model,and can get following result,the initial length of the crack has a great affectation on the life of the rod,and it is easy to calculate the fatigue life of rod exactly.
出处 《石油钻采工艺》 CAS CSCD 北大核心 2005年第6期66-69,共4页 Oil Drilling & Production Technology
基金 中国石油天然气集团公司2005年中青年石油创新基金资助项目(编号:05e7044)
关键词 疲劳 抽油杆 裂纹 寿命预测 fatigue sucker rod crack fatigue life prediction
作者简介 林元华,1971年生。1999年毕业于西南石油学院油气井工程专业,获博士学位,主要从事石油管线、石油钻井工艺方面的科研和教学工作,副教授。电话:028-83033964。E-mail:yhlin28@163.com。
  • 相关文献

参考文献7

二级参考文献19

  • 1高德利,高宝奎,耿瑞平.钻柱涡动特性分析[J].石油钻采工艺,1996,18(6):9-13. 被引量:22
  • 2覃成锦.含盐膏层井及大位移井套管柱优化设计研究.石油大学博士后出站报告[R].北京:石油大学(北京)油气井工程研究所,2003-04..
  • 3[1]Baryshnikov A, Calderoni A, Ligrone A, Ferrara P. A New Approach to the Analysis of Drillstring Fatigue Behavior. SPE 30 524
  • 4[2]Dale B A. An Experimental Investigation of Fatigue Crack Growth in Drillstring Tubulars. SPE 15 559
  • 5[4]Howard J A, Halbert M E, Arthur Lubinski. Systematic Tracking of Fatigue and Crack Growth to Optimize Drillstring Reliability. SPE/IADC 25 775
  • 6[5]Jiang Wu. Drill - pipe Bending and Fatigue in Rotary Drilling of Horizontal Wells. SPE 37 353
  • 7[8]Macpherson J D, Mason J S. Surface Measurement and Analysis of Drillstring Vibrations While Drilling. SPE 25777
  • 8Maidla E E, Wojtanowicz A K. Prediction of Casing Running koads in Directional Wells. In: 20th Annual OTC in Houston, Texas, May2-5, 1988.OTC5791.
  • 9Juvkam - Wold H C, Jiang Wu. Casing Deflection and Centralizer Spacing Calculations. SPE Drilling Engineering, 273-274, 1992 - 12.
  • 10Chen Y, Adnan S, Buckling of Pipe and Tubing Constrained Inside Inclined Wells. OTC 7323, 1993.

共引文献81

同被引文献107

引证文献16

二级引证文献58

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部