摘要
The feasibility and technologies of comprehensive recovery of tin, zinc, arsenic and iron from the complex iron ores by selective chlorination roasting were studied by thermodynamic analysis and roasting experiments. Investigation shows that the product pellets with the compression strength of 2625N/P, the tumble index of 97.26%, the abrasion index of 1.35%, tin, arsenic and zinc residue of 0.043%, 0.046% and 0.058% respectively can be achieved if balling a concentrate containing 0.39% tin, 0.40% arsenic and 0.28% with addition of 8% coke breeze and 0.5% CaCl2 and roasting the pellets at 10601080℃ for 40min. The volatilization of tin, arsenic and zinc is 91.75%, 93.42% and 81.12% respectively. The performances of the product pellets are able to meet the requirements of blast furnace ironmaking.
The feasibility and technologies of comprehensive recovery of tin, zinc, arsenic and iron from the complex iron ores by selective chlorination roasting were studied by thermodynamic analysis and roasting experiments. Investigation shows that the product pellets with the compression strength of 2 625 N/P, the tumble index of 97. 26%, the abrasion index of 1. 35%, tin, arsenic and zinc residue of 0. 043%, 0. 046% and 0.058% respectively can be achieved if bailing a concentrate containing 0.39 % tin, 0.40% arsenic and 0.28% with addition of 8% coke breeze and 0. 5% CaCl2 and roasting the pellets at 1 060 - 1 080℃ for 40 min. The volatilization of tin, arsenic and zinc is 91.75 %, 93.42 % and 81.12 % respectively. The performances of the product pellets are able to meet the requirements of blast furnace ironmaking.
出处
《中国有色金属学会会刊:英文版》
EI
CSCD
2005年第4期902-907,共6页
Transactions of Nonferrous Metals Society of China
关键词
锡
锌
炼铁工艺
氯化处理
选择性
矿石处理
selective chlorination
comprehensive recovery
tin
zinc
complex iron ore
作者简介
JIANG Tao, PhD, Tel: +86-731-8830542; E-mail jiangtao@mail.csu.edu.cn.