摘要 采用电冶重熔法 ,并引入稀土改性制备RE WC 钢基复合材料 ,研究了复合材料的显微缺陷、硬质相的存在状态、合金性能。实验结果显示 :RE WC 钢基复合材料中未观察到脏孔和游离石墨 ,与未加稀土的WC 钢基合金相比孔隙率明显下降 ,WC颗粒的孤立度提高 。 The RE-WC-steel composite was prepared with secondary electrowinning by modifying the property of rare earth. The micro-defect of composite, the state of hard phase and property of alloy all have been studied. The result shows that no dirty vent and free graphite had been found in the RE-WC-steel composite. Compared with the alloy without rare earth element, the porosity of the RE-WC-steel composite was obviously lower, and the solitarity of WC particles had been enhanced and the wearability had been improved.
出处 《矿冶工程》 CAS CSCD 北大核心 2005年第1期68-71,共4页 Mining and Metallurgical Engineering
基金 合肥工业大学基础研究基金 (0 4 0 30 4F)
关键词 钢基复合材料 稀土元素 显微缺陷 耐磨性 电冶重熔 steel-base composite rare earth element micro-defect wearability secondary electrowinning
  • 相关文献

参考文献10

  • 1杜挺.稀土元素在金属材料中的一些物理化学作用[J].金属学报,1997,33(1):69-77. 被引量:178
  • 2杨庆祥,姚枚,魏雅娟.稀土氧化物对中高碳钢堆焊金属中夹杂物变质作用的热力学分析[J].中国稀土学报,2001,19(5):439-442. 被引量:11
  • 3Lou D, Hellman J, Luhulima D. Interactions between tungsten carbide (WC) particulates and metal matrix in WC-reinforced comosites[J]. Materials Science and Engineering, 2003, A340:155 - 162.
  • 4Pagounis E. Structure and properties of hot work tool steel matrix compos ites made by HIP[ J]. Metal Powder Report, 1998,53 (2):39.
  • 5Pagounis E, Lindroos V K. Processing and properties of particulate reinforced steel matrix composites[J]. Mater Sci Eng, 1998,A246:221 - 234.
  • 6杜晓东,尤显卿,郑玉春.一种新型钢结硬质合金初探[J].硬质合金,1997,14(2):74-77. 被引量:12
  • 7游兴河.WC系钢结硬质合金断裂过程与断裂机理研究[J].粉末冶金技术,1988,(3):18-25.
  • 8Chermant J L. Fracture toughness and fracture of WC-Co composition[ J]. J of Materials Science, 1976,11:1157 - 1162.
  • 9Exner H E. A view of parameters influencing some mechanical properties of tungsten carbide-cobalt alloys[J]. J of Materials Science, 1970,5:769 - 772.
  • 10Degnan C C. Elevated temperature sliding wear behaviour of TiC-reinforced steel matrix composites[J]. Wear, 2001,250:1444- 1451.

二级参考文献43

共引文献198

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部