Oxidation Behavior of Yb_(2)Si_(2)O_(7)Modified SiC/SiC Mini-composites
1
作者 MU Shuang MA Qin +3 位作者 ZHANG Yu SHEN Xu YANG Jinshan DONG Shaoming 《无机材料学报》 北大核心 2025年第3期323-328,共6页
Silicon-carbide-fiber-reinforced silicon-carbide-ceramic-based matrix(SiC/SiC)composites possess excellent properties such as low density,high strength and high temperature resistance,showing a potential application f... Silicon-carbide-fiber-reinforced silicon-carbide-ceramic-based matrix(SiC/SiC)composites possess excellent properties such as low density,high strength and high temperature resistance,showing a potential application for structural components in the aerospace field,but their oxidation behavior remains largely unknown.In this study,Yb_(2)Si_(2)O_(7)modified SiC/SiC(SiC/SiC-Yb_(2)Si_(2)O_(7))mini-composites were prepared by introducing Yb_(2)Si_(2)O_(7)as anti-oxidation phase into SiC fiber bundles via Sol-Gel and depositing SiC matrix by chemical vapor deposition(CVD).Influence of Yb_(2)Si_(2)O_(7)on microstructure,mechanical property and oxidation behavior of SiC/SiC mini-composites was investigated.The results showed that after oxidation in air at 1200 and 1400℃for 50 h,the tensile strength retentions of SiC/SiC mini-composites were 77%and 69%,respectively,and the fracture morphology exhibited flat.The Yb_(2)Si_(2)O_(7)introduced by Sol-Gel partially distributed in layers,contributing to the toughening of the material.On the fracture surface,there was interlayer debonding,which extended energy dissipation mechanism of SiC/SiC mini-composites.Tensile strength of SiC/SiC-Yb_(2)Si_(2)O_(7)mini-composites at room temperature was 484 MPa.After oxidation in air at 1200 and 1400℃for 50 h,the tensile strengths decreased to 425 and 374 MPa,resulting in retention rates of 88%and 77%,respectively.It displayed typical non-brittle fracture characteristics.The interface oxygen content of SiC/SiC mini-composites at the fracture surface was higher than that of SiC/SiC-Yb_(2)Si_(2)O_(7)mini-composites,indicating that introduction of Yb_(2)Si_(2)O_(7)could alleviate oxygen diffusion towards the interface,and therefore improve the oxidation resistance of SiC/SiC-Yb_(2)Si_(2)O_(7)mini-composites. 展开更多
关键词 SiC/SiC mini-composite matrix modification Yb_(2)Si_(2)O_(7) oxidation behavior
在线阅读 下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部