Frothers facilitate the reduction of bubbles size by preventing bubbles coalescence and produce more stable froths.The collision probability of the bubbles and particles substantially increases by decreasing bubble si...Frothers facilitate the reduction of bubbles size by preventing bubbles coalescence and produce more stable froths.The collision probability of the bubbles and particles substantially increases by decreasing bubble size.For the same volume system,fewer bubbles result from a distribution of large-sized bubbles,and more bubbles result from a distribution of small-sized bubbles.In this research,fundamental two-phase frother characterization parameters were aimed to link with three-phase coal and talc flotation behavior.For this purpose,the effect of single and dual frother systems on inhibiting bubble coalescence was investigated with methyl isobutyl carbinol(MIBC),isooctanol(2 ethyl hexanol),pine oil,and Dowfroth 250.Based on the results of single frothers,isooctanol at the lowest critical coalescence concentration(CCC)value of 6×10^(−6) achieved the smallest bubbles with Sauter mean diameter of 0.80 mm.By blending Dowfroth 250 and pine oil,the bubbles size decreased significantly,reaching 0.45 mm.While the highest recoveries in coal flotation were obtained in single and frother blends where the bubbles size was measured as the smallest in two-phase system,and such a relationship was not found for talc flotation.展开更多
In light of the problems of low-quality and low degree of comprehensive utilization of Guangdong muscovite-type kaolin, the reasons affecting the quality of kaolin were found to be a small amount of maroon powdery goe...In light of the problems of low-quality and low degree of comprehensive utilization of Guangdong muscovite-type kaolin, the reasons affecting the quality of kaolin were found to be a small amount of maroon powdery goethite adhering to the surface of kaolin and minor muscovite affecting the firing whiteness of products. The ores were dealt with by using the new combined process of attritioning-classifieation-bleaching and flotation. The separation of kaolin from muscovite, quartz and feldspar can come true through the new process. The high-quality kaolin with the firing whiteness of 91% can be obtained, and the muscovite is comprehensively recovered by adopting the key technology of flotation. The content of high-purity muscovite produced is over 99%. The muscovite discarded by original process can be comprehensively recovered.展开更多
基金Project(ID42787)supported by the Istanbul Technical University,BAP(Scientific Research Project)Department,Turkey。
文摘Frothers facilitate the reduction of bubbles size by preventing bubbles coalescence and produce more stable froths.The collision probability of the bubbles and particles substantially increases by decreasing bubble size.For the same volume system,fewer bubbles result from a distribution of large-sized bubbles,and more bubbles result from a distribution of small-sized bubbles.In this research,fundamental two-phase frother characterization parameters were aimed to link with three-phase coal and talc flotation behavior.For this purpose,the effect of single and dual frother systems on inhibiting bubble coalescence was investigated with methyl isobutyl carbinol(MIBC),isooctanol(2 ethyl hexanol),pine oil,and Dowfroth 250.Based on the results of single frothers,isooctanol at the lowest critical coalescence concentration(CCC)value of 6×10^(−6) achieved the smallest bubbles with Sauter mean diameter of 0.80 mm.By blending Dowfroth 250 and pine oil,the bubbles size decreased significantly,reaching 0.45 mm.While the highest recoveries in coal flotation were obtained in single and frother blends where the bubbles size was measured as the smallest in two-phase system,and such a relationship was not found for talc flotation.
文摘In light of the problems of low-quality and low degree of comprehensive utilization of Guangdong muscovite-type kaolin, the reasons affecting the quality of kaolin were found to be a small amount of maroon powdery goethite adhering to the surface of kaolin and minor muscovite affecting the firing whiteness of products. The ores were dealt with by using the new combined process of attritioning-classifieation-bleaching and flotation. The separation of kaolin from muscovite, quartz and feldspar can come true through the new process. The high-quality kaolin with the firing whiteness of 91% can be obtained, and the muscovite is comprehensively recovered by adopting the key technology of flotation. The content of high-purity muscovite produced is over 99%. The muscovite discarded by original process can be comprehensively recovered.