Flotation performance of anisic hydroxamic acid as new collector for tungsten and tin minerals 被引量:8
1
作者 ZHAO Gang ZHOU Xiao-tong +2 位作者 LI Fang-xu FU Guang-qin SHANG Xing-ke 《Journal of Central South University》 SCIE EI CAS CSCD 2022年第11期3645-3655,共11页
In order to improve the recovery of tungsten ores containing tin minerals,anisic hydroxamic acid(p-methoxy benzohydroxanic acid,PMOB)was synthesized and introduced as novel collector in the flotation of scheelite,wolf... In order to improve the recovery of tungsten ores containing tin minerals,anisic hydroxamic acid(p-methoxy benzohydroxanic acid,PMOB)was synthesized and introduced as novel collector in the flotation of scheelite,wolframite and cassiterite.The flotation performance and adsorption mechanism were investigated by micro/batch flotation,zeta potential measurements and density functional theory(DFT).The micro flotation results showed that the recoveries of scheelite,wolframite and cassiterite using PMOB as collector are 97.45%,95.77% and 90.08%,respectively,and the corresponding recoveries are 91.00%,84.30% and 84.67% for benzohydroxamic acid(BHA).The batch flotation results revealed that the collector dosage could be reduced by about 45% for PMOB compared with BHA,in the case of similar flotation indicators.Zeta potential measurements indicated that PMOB could be adsorbed on the mineral surfaces by chemisorption.Moreover,density functional theory(DFT)calculation results showed that the substituent group—OCH_(3)endues PMOB stronger electron donation ability and hydrophobicity compared with benzohydroxamic acid(BHA),pmethyl benzohydroxamic acid(PMB)and p-hydroxyl benzohydroxamic acid(PHB). 展开更多
关键词 FLOTATION hydroxamic acid SCHEELITE WOLFRAMITE CASSITERITE
在线阅读 下载PDF
钨渣吸附剂的制备及其对含铅废水的吸附 被引量:6
2
作者 魏渤函 薛志远 +4 位作者 杨裕东 钟晓聪 任如山 王瑞祥 张魁芳 《Journal of Central South University》 SCIE EI CAS CSCD 2023年第6期1841-1855,共15页
为实现钨冶炼渣的资源化利用,通过正交试验和静态吸附试验,研究了钨渣-膨润土颗粒吸附剂制备的最佳成分比例和工艺条件。结果表明,颗粒吸附剂制备的最佳条件为:钨渣与膨润土的质量比为5:1,颗粒粒径为2 mm,烧结工艺为800℃,2 h。使用X射... 为实现钨冶炼渣的资源化利用,通过正交试验和静态吸附试验,研究了钨渣-膨润土颗粒吸附剂制备的最佳成分比例和工艺条件。结果表明,颗粒吸附剂制备的最佳条件为:钨渣与膨润土的质量比为5:1,颗粒粒径为2 mm,烧结工艺为800℃,2 h。使用X射线衍射仪和扫描电镜验证吸附剂主要形态为颗粒状的铁锰氧化物,其表面有大量的孔洞。在溶液pH为6,吸附剂用量为15 g/L,铅初始浓度为300 mg/L,吸附时间为200 min的条件下,吸附剂对废水中Pb2+的去除率达99.95%。该吸附剂对Pb2+的吸附过程符合准二级动力学方程,吸附等温线符合Langmuir方程,对Pb2+的吸附属于单分子层的特异性化学吸附。 展开更多