裂解升温速率对聚碳硅烷先驱体转化制备C_f/SiC材料弯曲性能的影响 被引量:7
1
作者 简科 陈朝辉 +2 位作者 陈国民 马青松 郑文伟 《材料工程》 EI CAS CSCD 北大核心 2003年第11期11-13,共3页
以聚碳硅烷 (PCS) /二乙烯基苯 (DVB)为先驱体制备了 3D- B Cf/ Si C复合材料 ,研究先驱体转化过程中不同裂解升温速率对材料力学性能的影响。结果表明 :随着裂解升温速率的提高 ,材料致密度增加 ,界面结合变弱 ,从而陶瓷基复合材料的... 以聚碳硅烷 (PCS) /二乙烯基苯 (DVB)为先驱体制备了 3D- B Cf/ Si C复合材料 ,研究先驱体转化过程中不同裂解升温速率对材料力学性能的影响。结果表明 :随着裂解升温速率的提高 ,材料致密度增加 ,界面结合变弱 ,从而陶瓷基复合材料的力学性能明显提高。以 15℃ / min裂解升温速率制得的陶瓷基复合材料的室温弯曲强度达到5 5 6 .7MPa,130 0℃真空下测试 ,材料的弯曲强度达到 6 80 .3MPa。 展开更多
关键词 CF/SIC复合材料 聚碳硅烷 弯曲强度 界面
在线阅读 下载PDF
新型耐热级苯酚-淀粉模塑料(PF2C4)的研制 被引量:5
2
作者 陈国民 陈朝辉 《化工学报》 EI CAS CSCD 北大核心 2004年第2期341-343,共3页
A new heat resisting phenol-starch moulding material (PF2C4) was prepared.Its typical raw materials formulation, preparative technology and moulding technology were determined.The method of its quatity control was put... A new heat resisting phenol-starch moulding material (PF2C4) was prepared.Its typical raw materials formulation, preparative technology and moulding technology were determined.The method of its quatity control was put forward and its properties and economic advantage were analyzed. The results show that typical raw materials formulation(mass percent)of the product is phenol-starch is phenol starch resin∶hexamethylene-tetramine∶wood flour∶calcium carbonate∶magnesium oxide∶zinc stearate∶stearic acid∶Oil Aniline Black∶ultramarine=37.0∶6.4∶30.0∶24.0∶0.6∶0.6∶0.4∶0.5∶0.5.The preparative technological parameters of the product were mixed time ≥60?min, temperature of the working roller 90—100?℃, temperature of the idle roller 145—155?℃, distance of the two rollers 2.0—2.5?mm, warm-up time 4—5?min.combining batch time≥45?min.The moulding, technological parameters of the product were preheating temperature 100—110?℃, preheating time 10—15?min, moulding pressure≥25?MPa, moulding temperature 180—185?℃, moulding time 0.8—1.0?min·mm -1 , exhaust ≥3 times. The quality of the product was controlled by bright outward appearance of sheet material of moulding material and Raschig flow property 80—120?mm of moulding material.The properties of the product came up to the national standard of raw heat resisting phenol-for maldehyde material (PF2C4), specifically its heat properties (thermal deformation temperature 174?℃) and electric properties (insulating resistance 6.0×10 12 ?Ω, dielectric strength 6.7?MV·m -1 , dielectric loss tangent 0.03)surpassed greatly the national standard.It showed very good electric properties in moist environment.By comparison with raw heat resisting thermoplastic phenol-formaldehyde moulding material(PF2C4),the cost of raw materials consumption reduced by is 20.9%. 展开更多
关键词 苯酚-淀粉模塑料(PF2C4) 配方 工艺 经济优势
在线阅读 下载PDF
苯酚-淀粉树脂及其模塑料工业化设计研究
3
作者 陈国民 陈朝辉 《化学工程》 CAS CSCD 北大核心 2004年第2期73-76,共4页
以生产能力410t/a树脂、1000t/a模塑料,工作时24h/d、工作日250d/a,间歇生产法和连续生产法并举为设计要求,对苯酚 淀粉树脂及其模塑料工业化生产进行设计,介绍了原料消耗定额、主要设备及工装、厂房、电力及水源、设备布局、岗位定员... 以生产能力410t/a树脂、1000t/a模塑料,工作时24h/d、工作日250d/a,间歇生产法和连续生产法并举为设计要求,对苯酚 淀粉树脂及其模塑料工业化生产进行设计,介绍了原料消耗定额、主要设备及工装、厂房、电力及水源、设备布局、岗位定员、投资概算、产品技术指标及出厂检验项目、安全防护及三废处理等设计内容。生产证明本工业化设计切实可行。 展开更多