期刊文献+
共找到6篇文章
< 1 >
每页显示 20 50 100
一种新的橙红色长余辉荧光材料Y_2O_2S∶Sm^(3+) 被引量:26
1
作者 雷炳富 刘应亮 +2 位作者 唐功本 叶泽人 石春山 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 2003年第2期208-210,共3页
A new Sm 3+ doped yttrium oxysulfide phosphor, which has the long-lasting phosphorescence, was synthesized by flux fusion method. The phosphors showed three typical transitions of Sm 3+ ( 4G 5/2→ 6H J, J=5/2,7/2,9/2)... A new Sm 3+ doped yttrium oxysulfide phosphor, which has the long-lasting phosphorescence, was synthesized by flux fusion method. The phosphors showed three typical transitions of Sm 3+ ( 4G 5/2→ 6H J, J=5/2,7/2,9/2), and the emission peaks located at 570, 606 and 659 nm respectively. A prominent luminescence and phosphorescence in orange-red can be seen in this phosphor when illuminated with UV light or visible light. The synthesized phosphors were characterized by X-ray diffraction, the excitation and photoluminescence spectra, and the after-glow intensity decay curve. The result shows that the Y 2O 2S∶ Sm 3+ phosphor is another efficient orange-red phosphor. 展开更多
关键词 橙红色长余辉荧光材料 Y2O2S 硫氧化钇 钐离子 掺杂 荧光材料
在线阅读 下载PDF
微波法合成橙红色长余辉磷光粉Gd_2O_2S:Sm^(3+) 被引量:20
2
作者 宋春燕 刘应亮 +5 位作者 张静娴 黄浪欢 袁定胜 容建华 石春山 雷炳富 《暨南大学学报(自然科学与医学版)》 CAS CSCD 2003年第5期93-96,共4页
 首次采用微波法合成橙红色长余辉磷光粉:Gd2O2S:Sm3+,并表征了其结构,激发、发射光谱和余辉衰减曲线.XRD分析证实其为单相的硫氧化钆.光致发光光谱显示Sm3+的3个特征发射(4G5/2→6HJ,J=5/2,7/2,9/2).该磷光粉经紫外和可见光激发后呈...  首次采用微波法合成橙红色长余辉磷光粉:Gd2O2S:Sm3+,并表征了其结构,激发、发射光谱和余辉衰减曲线.XRD分析证实其为单相的硫氧化钆.光致发光光谱显示Sm3+的3个特征发射(4G5/2→6HJ,J=5/2,7/2,9/2).该磷光粉经紫外和可见光激发后呈现出长时间明亮的余辉发射,是一种性能良好的新型长余辉发光材料. 展开更多
关键词 微波法 长余辉 硫氧化钆 钐离子
在线阅读 下载PDF
离子液体[C8mim]PF6对水生生物的毒性作用 被引量:19
3
作者 牧辉 彭新晶 +2 位作者 戴宁 陈继 张凤君 《中国环境科学》 EI CAS CSCD 北大核心 2009年第11期1196-1201,共6页
运用评价化学品对水生生物毒性的标准试验方法,探讨离子液体1-辛基-3-甲基-咪唑六氟磷酸盐([C8mim]PF6)对普通小球藻、大型蚤和斑马鱼的毒性影响.结果表明,[C8mim]PF6在实验浓度下,对普通小球藻的生长和叶绿素a的产生均有抑制作用,浓度... 运用评价化学品对水生生物毒性的标准试验方法,探讨离子液体1-辛基-3-甲基-咪唑六氟磷酸盐([C8mim]PF6)对普通小球藻、大型蚤和斑马鱼的毒性影响.结果表明,[C8mim]PF6在实验浓度下,对普通小球藻的生长和叶绿素a的产生均有抑制作用,浓度越高抑制作用越明显,且对叶绿素a含量的影响更为显著.高浓度组(200mg/L)可致死部分小球藻细胞;[C8mim]PF6对大型蚤的48hLC50为4.47mg/L,属于高毒性;[C8mim]PF6对斑马鱼的96hLC50为126.08mg/L,属于低毒性.[C8mim]PF6对这3种水生生物的抑制率/致死率(EC50/LC50)随时间呈规律性变化.[C8mim]PF6与藻类的亲和性及其亲脂特性可能是其对水生生物存在潜在毒性的2个主要原因. 展开更多
关键词 [C8mim]PF6 毒性 普通小球藻 大型蚤 斑马鱼
在线阅读 下载PDF
Eu^(3+)在La_2O_2S中的长余辉发光 被引量:8
4
作者 宋春燕 雷炳富 +4 位作者 刘应亮 石春山 张静娴 黄浪欢 袁定胜 《无机化学学报》 SCIE CAS CSCD 北大核心 2004年第1期89-93,共5页
The new Eu 3+ doped lanthanum oxysulfide phosphors,which have the orange-red long afterg low emission,were synthesized by solid-state reaction method.The synthesized phosphors were characterized by X-ray diffraction.T... The new Eu 3+ doped lanthanum oxysulfide phosphors,which have the orange-red long afterg low emission,were synthesized by solid-state reaction method.The synthesized phosphors were characterized by X-ray diffraction.The excitation and emission spectra,afterglow spectra and afterglow decay curves were examined.XRD confirm ed the phosphor as pure phase La 2 O 2 S.The phosphors showed typical transitions 5 D J (J=0,1) → 7 F J (J=0,1,2,3,4)of Eu 3+ .The photoluminescence spectra and afterglow spectra presented the regular alteration with various Eu 3+ concentration,due to cross relaxation between energy levels of Eu 3+ .In addition,we studied the effects of activator concentration and dopants species on the afterglow property.The data showed afterglow result was the bes t with2%Eu 3+ and doped with Mg 2+ and Zr 4+ .A prominent phosphorescence can be seen in this phosphor after illuminated with UV light. 展开更多
关键词 EU^3+ La2O2S 长余辉发光 硫氧化镧 铕离子 发光材料 磷光粉
在线阅读 下载PDF
(Ce_(0.9)Nd_(0.1))_(1-x)Mo_xO_(2-δ)(0.00≤x≤0.10)的合成、表征与电性能(英文) 被引量:3
5
作者 夏燕杰 周德凤 孟健 《物理化学学报》 SCIE CAS CSCD 北大核心 2009年第7期1415-1420,共6页
采用溶胶-凝胶法合成(Ce0.9Nd0.1)1-xMoxO2-δ(x=0.00、0.02、0.05、0.10)氧化物,通过X射线衍射(XRD)、场发射扫描电镜(FESEM)等手段对氧化物进行结构表征,交流阻抗谱测试电性能.结果表明:所有样品均为单一萤石立方结构;少量MoO3的加入... 采用溶胶-凝胶法合成(Ce0.9Nd0.1)1-xMoxO2-δ(x=0.00、0.02、0.05、0.10)氧化物,通过X射线衍射(XRD)、场发射扫描电镜(FESEM)等手段对氧化物进行结构表征,交流阻抗谱测试电性能.结果表明:所有样品均为单一萤石立方结构;少量MoO3的加入提高了材料的致密性,降低了材料的总电阻、晶界电阻和晶界电阻在总电阻中所占比例,提高了材料的电导率.1200℃烧结样品24h,测试温度700℃时,(Ce0.9Nd0.1)1-xMoxO2-δ(x=0.00)总电导率和晶界电导率分别为0.05和0.19S·m-1,掺Mo材料(Ce0.9Nd0.1)1-xMoxO2-δ(x=0.02)的总电导率和晶界电导率分别为2.42和3.96S·m-1. 展开更多
关键词 钕掺杂氧化铈 氧化钼 微观结构 晶界电导率
在线阅读 下载PDF
MgO掺杂Ce_(0.9)Sm_(0.1)O_(2-δ)固体电解质的结构和电性能 被引量:2
6
作者 宁德争 周德凤 +2 位作者 夏燕杰 赵桂春 孟健 《物理化学学报》 SCIE CAS CSCD 北大核心 2010年第5期1202-1206,共5页
采用溶胶-凝胶法合成SiO2含量为5.0×10-4(w)的Ce0.9Sm0.1O2-δ(SDC)粉体(SDCSi),并将0-3.0%(x)MgO分别加入到SDCSi陶瓷粉体中,用X射线衍射(XRD)和场发射扫描电子显微镜(FE-SEM)对材料进行表征,用交流阻抗谱(AC)测试材料的电性能.... 采用溶胶-凝胶法合成SiO2含量为5.0×10-4(w)的Ce0.9Sm0.1O2-δ(SDC)粉体(SDCSi),并将0-3.0%(x)MgO分别加入到SDCSi陶瓷粉体中,用X射线衍射(XRD)和场发射扫描电子显微镜(FE-SEM)对材料进行表征,用交流阻抗谱(AC)测试材料的电性能.结果表明:MgO掺杂能使SDCSi的烧结温度降低100-200℃,提高陶瓷材料的致密度;清除或降低陶瓷材料晶界处SiO2杂质的有害影响,显著提高晶粒/晶界电导率和总电率;MgO掺杂到SDCSi具有烧结助剂和晶界杂质清除剂的双重作用. 展开更多
关键词 固体电解质 MgO掺杂 清除剂 电导率
在线阅读 下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部