期刊文献+
共找到1,790篇文章
< 1 2 90 >
每页显示 20 50 100
Mechanical properties and damage evolution law of cemented-gangue-fly-ash backfill modified with different contents of recycled steel fibers
1
作者 CHE Chi-yuan CAO Sheng-gen +5 位作者 ZHANG Yun LIU Yang ZHAO Chang-zheng DU Shu-yu LI Jiang SHAN Chang-hao 《Journal of Central South University》 2025年第7期2661-2678,共18页
The cemented-gangue-fly-ash backfill(CGFB)prepared from coal-based solid waste materials commonly exhibits high brittleness,leading to an increased susceptibility to cracking.Uniaxial compressive strength(UCS),acousti... The cemented-gangue-fly-ash backfill(CGFB)prepared from coal-based solid waste materials commonly exhibits high brittleness,leading to an increased susceptibility to cracking.Uniaxial compressive strength(UCS),acoustic emission(AE),and scanning electron microscopy tests were conducted on CGFB samples with recycled steel fiber(RSF)contents of 0,0.5%,1.0%and 1.5%to assess the mechanical properties and damage evolution law of the CGFB.The research findings indicate that:1)When RSF contents were 0.5%,1%,and 1.5%,respectively,compared to samples without RSF,the UCS decreased by 3.86%,6.76%,and 15.59%,while toughness increased by 69%,98%,and 123%;2)The addition of RSFs reduced the post-peak stress energy activity and increased the fluctuations in the b-value;3)As the RSF dosage increased from 0 to 1.5%,the per unit dissipated strain energy increased from 5.84 to 21.51,and the post-peak released energy increased from 15.07 to 33.76,indicating that the external energy required for the CGFB sample to fail increased;4)The hydration products,such as C-S-H gel,ettringite,and micro-particle materials,were embedded in the damaged areas of the RSFs,increasing the frictional force at the interface between the RSF and CGFB matrix.The shape variability of the RSFs caused interlocking between the RSFs and the matrix.Both mechanisms strengthened the bridging effect of the RSFs in the CGFB,thereby improving the damage resistance capability of CGFB.The excellent damage resistance occurred at an RSF content of 0.5%;thus,this content is recommended for engineering applications. 展开更多
关键词 recycled steel fibers cemented-gangue-fly-ash backfill acoustic emission crack development energy evolution
在线阅读 下载PDF
Performance of multi-layer steel fiber-reinforced mortar panels with air gaps against high-velocity bullets and successive firing
2
作者 Apisit Techaphatthanakon Buchit Maho +5 位作者 Sittisak Jamnam Pochara Kruavit Manote Sappakittipakorn Phattharachai Pongsopha Gritsada Sua-iam Piti Sukontasukkul 《Defence Technology(防务技术)》 2025年第7期290-306,共17页
This research addresses the growing demand for high-performance protective materials against high-velocity projectile impacts.The performance of multi-layered steel fiber-reinforced mortar(SFRM)panels with varying thi... This research addresses the growing demand for high-performance protective materials against high-velocity projectile impacts.The performance of multi-layered steel fiber-reinforced mortar(SFRM)panels with varying thicknesses and air gaps,was experimentally investigated under single and repeated impacts of 7.62×51 mm bullets fired from a distance of 50 m.The impact events were recorded using a high-speed camera at 40000 fps.Panel performance was assessed in terms of failure modes,kinetic energy absorption,spalling diameter,and percentage of back-face damage area,and weight loss.Results showed that panel configuration significantly influenced performance.Panel P10,with 70 mm SFRM thickness and 20 mm air gaps,provided the highest resistance,dissipating 5223 J of kinetic energy and preventing back-face damage.In contrast,P7,which absorbed 4476 J,presented a back damage area percentage of 8.93%after three impacts.Weight loss analysis further confirmed durability improvements,with P10 showing only 1.53%cumulative loss compared to 3.26%in P7.The inclusion of wider air gaps enhanced energy dissipation and reduced damage.Comparison between single and repeated impacts demonstrated the sustained resistance of high-performance panels,with P10 maintaining minimal degradation across three consecutive impacts.These findings highlight the potential of multi-layer SFRM panels to enhance ballistic resistance,making them suitable for military,security,and civilian protective applications requiring long-term durability. 展开更多
关键词 Bullet resistance steel fiber reinforced mortar Multilayer Impact behavior Failure mode
在线阅读 下载PDF
Experimental investigation of axially loaded steel fiber reinforced high strength concrete-filled steel tube columns 被引量:10
3
作者 卢亦焱 李娜 +1 位作者 李杉 梁鸿骏 《Journal of Central South University》 SCIE EI CAS CSCD 2015年第6期2287-2296,共10页
An experimental study on the compressive behavior of steel fiber reinforced concrete-filled steel tube columns is presented. Specimens were tested to investigate the effects of the concrete strength, the thickness of ... An experimental study on the compressive behavior of steel fiber reinforced concrete-filled steel tube columns is presented. Specimens were tested to investigate the effects of the concrete strength, the thickness of steel tube and the steel fiber volume fraction on the ultimate strength and the ductility. The experimental results indicate that the addition of steel fibers in concrete can significantly improve the ductility and the energy dissipation capacity of the concrete-filled steel tube columns and delay the local buckling of the steel tube, but has no obvious effect on the failure mode. It has also been found that the addition of steel fibers is a more effective method than using thicker steel tube in enhancing the ductility, and more advantageous in the case of higher strength concrete. An analytical model to estimate the load capacity is proposed for steel tube columns filled with both plain concrete and steel fiber reinforced concrete. The predicted results are in good agreement with the experimental ones obtained in this work and literatures. 展开更多
关键词 concrete-filled steel tube (CFST) zolumns steel fiber high strength concrete axial load DUCTILITY load capacity
在线阅读 下载PDF
Complete splitting process of steel fiber reinforced concrete at intermediate strain rate 被引量:1
4
作者 罗章 李夕兵 赵伏军 《Journal of Central South University of Technology》 EI 2008年第4期569-573,共5页
The complete splitting process of steel fiber reinforced concrete (SFRC) at intermediate strain rate was studied by experiment. The basic information of a self-developed SFRC dynamic test system matching with lnstro... The complete splitting process of steel fiber reinforced concrete (SFRC) at intermediate strain rate was studied by experiment. The basic information of a self-developed SFRC dynamic test system matching with lnstron 1342 materials testing machine was given, and the experiment principle and the loading mode of cubic split specimen were introduced. During the experiment, 30 cubes of 150 mm×150 mm×150 mm and 36 cubes of 100 mm×100 mm×100 mm, designed and prepared according to C20 class SFRC with different volume fractions of steel fiber (0, 1%, 2%, 3%, 4%) were tested and analyzed. At the same time, the size effect of SFRC at intermediate strain rate was investigated. The experimental study indicates that SFRC size effect is not influenced by the loading speed or strain rate. When the steel fiber content increases from 0 to 4%, the splitting strength of SFRC increases from 100% to 261%, i.e. increasing by 161% compared with that of the common concrete. The loading rate increases from 1.33 kN/s to 80.00 kN/s, and the splitting tensile strength increases by 43.55%. 展开更多
关键词 steel fiber reinforced concrete intermediate strain rate splitting test size effect
在线阅读 下载PDF
Sintering behaviors of porous 316L stainless steel fiber felt
5
作者 冯萍 刘咏 +3 位作者 王岩 李昆 赵秀云 汤慧萍 《Journal of Central South University》 SCIE EI CAS CSCD 2015年第3期793-799,共7页
Isothermal sintering experiments were performed on the 316 L stainless steel fiber felts with fiber diameters of 8 μm and20 μm. Surface morphologies of the sintered specimens were investigated by using scanning elec... Isothermal sintering experiments were performed on the 316 L stainless steel fiber felts with fiber diameters of 8 μm and20 μm. Surface morphologies of the sintered specimens were investigated by using scanning electron microscopy(SEM) and optical microscopy. The results show that the amount of the sintering necks and the relative densities of the fiber felt increase with the increasing of both the sintering temperature and the sintering time. And the activation energies estimated present a decline at high relative densities for both 8 μm and 20 μm fiber felts. Moreover, the sintering densification of the fiber felts is dominated by volume diffusion mechanism at low temperature and relative densities. As more grain boundaries are formed at higher temperature and relative density, grain boundary diffusion will also contribute to the densification of the specimen. 展开更多
关键词 316L stainless steel fiber felt sintering activation energy diffusion
在线阅读 下载PDF
Projectile impact and drop weight resistance of functionally graded fiber-reinforced magnetite aggregate concrete
6
作者 Abbas Abbaspour Behnoud Ganjavi Mahdi Nematzadeh 《Defence Technology(防务技术)》 2025年第10期1-23,共23页
Many researchers have focused on the behavior of fiber-reinforced concrete(FRC)in the construction of various defensive structures to resist against impact forces resulting from explosions and projectiles.However,the ... Many researchers have focused on the behavior of fiber-reinforced concrete(FRC)in the construction of various defensive structures to resist against impact forces resulting from explosions and projectiles.However,the lack of sufficient research regarding the resistance of functionally graded fiber-reinforced concrete against projectile impacts has resulted in a limited understanding of the performance of this concrete type,which is necessary for the design and construction of structures requiring great resistance against external threats.Here,the performance of functionally graded fiber-reinforced concrete against projectile impacts was investigated experimentally using a(two-stage light)gas gun and a drop weight testing machine.For this objective,12 mix designs,with which 35 cylindrical specimens and 30 slab specimens were made,were prepared,and the main variables were the magnetite aggregate vol%(55%)replacing natural coarse aggregate,steel fiber vol%,and steel fiber type(3D and 5D).The fibers were added at six vol%of 0%,0.5%,0.75%,1%,1.25%,and 1.5%in 10 specimen series(three identical specimens per each series)with dimensions of 40×40×7.5 cm and functional grading(three layers),and the manufactured specimens were subjected to the drop weight impact and projectile penetration tests by the drop weight testing machine and gas gun,respectively,to assess their performance.Parameters under study included the compressive strength,destruction level,and penetration depth.The experimental results demonstrate that using the magnetite aggregate instead of the natural coarse aggregate elevated the compressive strength of the concrete by 61%.In the tests by the drop weight machine,it was observed that by increasing the total vol%of the fibers,especially by increasing the fiber content in the outer layers(impact surface),the cracking resistance and energy absorption increased by around 100%.Note that the fiber geometry had little effect on the energy absorption in the drop weight test.Investigating the optimum specimens showed that using 3D steel fibers at a total fiber content of 1 vol%,consisting of a layered grading of 1.5 vol%,0 vol%,and 1.5 vol%,improved the penetration depth by 76%and lowered the destruction level by 85%.In addition,incorporating the 5D steel fibers at a total fiber content of 1 vol%,consisting of the layered fiber contents of 1.5%,0%,and 1.5%,improved the projectile penetration depth by 50%and lowered the damage level by 61%compared with the case of using the 3D fibers. 展开更多
关键词 steel fiber Projectile impact Gas gun Drop weight MAGNETITE fiber-reinforced concrete(FRC)
在线阅读 下载PDF
A comparative evaluation of microstructural and mechanical behavior of fiber laser beam and tungsten inert gas dissimilar ultra high strength steel welds 被引量:1
7
作者 Jaiteerth R. JOSHI Mastanaiah POTTA +2 位作者 Kumar ADEPU Ramesh Kumar KATTA Madhusudhan Reddy GANKIDI 《Defence Technology(防务技术)》 SCIE EI CAS CSCD 2016年第6期464-472,共9页
The influence of different welding processes on the mechanical properties and the corresponding variation in the microstructural features have been investigated for the dissimilar weldments of 18% Ni maraging steel 25... The influence of different welding processes on the mechanical properties and the corresponding variation in the microstructural features have been investigated for the dissimilar weldments of 18% Ni maraging steel 250 and AISI 4130 steel. The weld joints are realized through two different fusion welding processes, tungsten inert arc welding(TIG) and laser beam welding(LBW), in this study. The dissimilar steel welds were characterized through optical microstructures, microhardness survey across the weldment and evaluation of tensile properties. The fiber laser beam welds have demonstrated superior mechanical properties and reduced heat affected zone as compared to the TIG weldments. 展开更多
关键词 TIG WELDING fiber LASER AISI 4130 steel LASER beam WELDING Maraging steel
在线阅读 下载PDF
基于主成分方法研究钢纤维增强混凝土劈裂破坏的损伤机制 被引量:2
8
作者 李涛 任会兰 +2 位作者 宁建国 宋水舟 檀日晶 《振动与冲击》 北大核心 2025年第1期221-231,共11页
研究钢纤维混凝土劈裂破坏的细观损伤机制,对在役钢纤维混凝土结构的健康检测具有重要意义。通过多通道声发射系统,采集混凝土和钢纤维混凝土试件(钢纤维含量分别为15和45 kg/m 3)劈裂破坏过程中的声发射信号,并结合主成分分析法和k-me... 研究钢纤维混凝土劈裂破坏的细观损伤机制,对在役钢纤维混凝土结构的健康检测具有重要意义。通过多通道声发射系统,采集混凝土和钢纤维混凝土试件(钢纤维含量分别为15和45 kg/m 3)劈裂破坏过程中的声发射信号,并结合主成分分析法和k-means聚类算法,对混凝土和钢纤维混凝土的损伤特征进行分析。结果表明,钢纤维的加入抑制了混凝土中裂纹扩展,有效地改善了混凝土的峰后韧性;声发射计数和能量参数变化特征反映了钢纤维混凝土试件宏观变形、破坏的细观损伤演化过程。最后,识别出了钢纤维混凝土中砂浆基体开裂和钢纤维拉拔的两种损伤机制。与砂浆基体开裂相比,钢纤维拉拔产生的声发射信号具有计数高、幅值高、能量强和持续时间长的特征。 展开更多
关键词 钢纤维增强混凝土(SFRC) 声发射技术 主成分分析(PCA) K-MEANS聚类
在线阅读 下载PDF
纳米二氧化硅与钢纤维对再生混凝土力学性能的影响 被引量:3
9
作者 王俊波 申贺文 +1 位作者 王永贵 黄旭阳 《武汉科技大学学报》 北大核心 2025年第2期121-132,共12页
为提高再生混凝土的力学性能,通过掺入纳米SiO_(2)与钢纤维对其进行改性。以再生骨料取代率、纳米SiO_(2)及钢纤维掺量为控制参数,利用力学性能试验,分析了不同参数对再生混凝土破坏形态、力学性能、弯曲韧性的影响。结果表明,掺入钢纤... 为提高再生混凝土的力学性能,通过掺入纳米SiO_(2)与钢纤维对其进行改性。以再生骨料取代率、纳米SiO_(2)及钢纤维掺量为控制参数,利用力学性能试验,分析了不同参数对再生混凝土破坏形态、力学性能、弯曲韧性的影响。结果表明,掺入钢纤维有利于改善再生混凝土力学性能,尤其能明显提高混凝土的劈裂抗拉强度及抗折强度。掺入纳米SiO_(2)可使再生混凝土力学性能均有所提高,同时可改善钢纤维再生混凝土延性。与单一掺入钢纤维或纳米SiO_(2)相比,复合掺入纳米SiO_(2)与钢纤维对再生混凝土各项力学性能的提升效果更显著,最佳的纳米SiO_(2)与钢纤维掺量分别为1%、1.5%。掺入纳米SiO_(2)可提高钢纤维再生混凝土的弯曲韧性,复合掺入纳米SiO_(2)与钢纤维对混凝土弯曲韧性的提升效果要优于单独掺入纳米SiO_(2)或钢纤维。建议采用JG/T 472—2015《钢纤维混凝土》标准评价纳米SiO_(2)与钢纤维增强再生混凝土的弯曲韧性。 展开更多
关键词 再生混凝土 再生骨料 纳米SiO_(2) 钢纤维 破坏形态 力学性能 弯曲韧性
在线阅读 下载PDF
基于损伤比强度理论的约束钢纤维混凝土塑性-损伤模型及应用 被引量:6
10
作者 丁发兴 邓亦南 吴霞 《东南大学学报(自然科学版)》 北大核心 2025年第1期89-97,共9页
为建立钢纤维混凝土(SFRC)三轴塑性-损伤模型(CDP),采用普通混凝土三轴塑性-损伤模型构建方法,对已有钢纤维混凝土单轴力学性能试验数据库进行整理分析,提出适用于不同钢纤维体积分数下混凝土立方体抗压强度、轴心抗压强度、轴心抗拉强... 为建立钢纤维混凝土(SFRC)三轴塑性-损伤模型(CDP),采用普通混凝土三轴塑性-损伤模型构建方法,对已有钢纤维混凝土单轴力学性能试验数据库进行整理分析,提出适用于不同钢纤维体积分数下混凝土立方体抗压强度、轴心抗压强度、轴心抗拉强度、弹性模量、受压峰值应变与受拉峰值应变的统一计算公式以及钢纤维混凝土单轴受压、受拉应力-应变骨架曲线和卸载刚度表达式。根据钢纤维混凝土损伤比强度理论,推荐了塑性-损伤模型中的三轴强度及其他参数,提出约束钢纤维混凝土三轴塑性-损伤模型。结果表明,在钢筋钢纤维混凝土简支梁静力加载、短柱轴压加载以及悬臂柱低周反复加载的有限元模型分析中,所提模型的计算结果与试验结果符合良好。 展开更多
关键词 钢纤维混凝土 力学性能 塑性-损伤模型 有限元分析
在线阅读 下载PDF
钢纤维地聚物再生混凝土力学性能及强度指标换算 被引量:1
11
作者 董硕 郑立森 +2 位作者 史奉伟 王来 刘哲 《材料导报》 北大核心 2025年第7期96-103,共8页
以再生粗骨料替换率(0%~100%)和钢纤维体积掺量(0%~1.5%)为主要变量,设计制作了240个钢纤维地聚物再生混凝土(SFGRC)试件,并进行各项基本力学性能试验及微观形貌观测。研究结果表明:采用再生粗骨料替换天然骨料,混凝土的各项基本力学性... 以再生粗骨料替换率(0%~100%)和钢纤维体积掺量(0%~1.5%)为主要变量,设计制作了240个钢纤维地聚物再生混凝土(SFGRC)试件,并进行各项基本力学性能试验及微观形貌观测。研究结果表明:采用再生粗骨料替换天然骨料,混凝土的各项基本力学性能均会降低。当钢纤维体积掺量为1.0%时,采用再生粗骨料100%替换天然骨料的SFGRC,其立方体和轴心抗压强度、弹性模量、劈裂抗拉和抗折强度分别降低15%、9%、25%、15%和15%,峰值应变增加24%。除了弹性模量外,钢纤维的掺入可显著提高混凝土的各项力学性能,试件破坏呈延性模式;当再生粗骨料替换率为100%时,掺入1.5%钢纤维的SFGRC后,其立方体和轴心抗压强度、峰值应变、劈裂抗拉和抗折强度分别增加15%、9%、10%、65%、39%。根据试验结果并综合考虑再生粗骨料替换率和钢纤维体积掺量的影响,提出了SFGRC基本强度指标的计算公式及换算关系。 展开更多
关键词 地聚物混凝土 钢纤维 再生粗骨料 力学性能 强度指标 经验公式
在线阅读 下载PDF
型钢-钢纤维混凝土局部组合梁受力性能 被引量:2
12
作者 伍凯 杨毅恒 +3 位作者 诸睿哲 张雁杰 梁庆庆 王世龙 《哈尔滨工业大学学报》 北大核心 2025年第2期153-163,共11页
为解决型钢混凝土结构的施工困难,充分发挥各部分材料的性能优势,将钢筋笼离散化为随机分布的钢纤维,并将钢纤维混凝土集中应用于受压区,形成型钢-钢纤维混凝土局部组合梁。对18根不同钢纤维体积率(ρ_(sf))、剪跨比(λ)、型钢受压翼缘... 为解决型钢混凝土结构的施工困难,充分发挥各部分材料的性能优势,将钢筋笼离散化为随机分布的钢纤维,并将钢纤维混凝土集中应用于受压区,形成型钢-钢纤维混凝土局部组合梁。对18根不同钢纤维体积率(ρ_(sf))、剪跨比(λ)、型钢受压翼缘上下部混凝土保护层厚度(C_(ss)、C_(sv))和型钢规格(I_(s))的组合梁试件进行四点弯试验。分析试验参数对破坏模式、荷载-挠度曲线以及破坏对称性的影响。结果表明:增大ρ_(sf)对小剪跨比试件(λ为1.5或1.7)的界面黏结性能具有积极改善作用,试件破坏模式由界面破坏转为弯扭破坏;混凝土保护层厚度须随I_(s)同步增大,确保混凝土保护层对型钢提供足够的“握裹效应”,避免或削弱弯扭变形的不利影响。通过高斯分布拟合,得到试件整体性能开始出现严重退化时的挠度退化系数,进而对构件整体性能开始出现严重退化时的挠度进行预测。 展开更多
关键词 组合结构 型钢混凝土 钢纤维混凝土 破坏模式 荷载-挠度曲线 能量耗散
在线阅读 下载PDF
BFRP筋与混杂钢纤维超高性能混凝土黏结性能分析 被引量:1
13
作者 范小春 郭浩宇 +1 位作者 张澳 张浩 《河海大学学报(自然科学版)》 北大核心 2025年第5期154-161,共8页
为研究玄武岩纤维增强复合材料(BFRP)筋与混杂钢纤维超高性能混凝土(UHPC)的黏结性能,采用拉拔试验对BFRP筋与混杂钢纤维UHPC的黏结性能进行了试验研究,分析了回收轮胎钢纤维(RTSF)掺量、UHPC保护层厚度、UHPC龄期及不同纤维掺入比例对B... 为研究玄武岩纤维增强复合材料(BFRP)筋与混杂钢纤维超高性能混凝土(UHPC)的黏结性能,采用拉拔试验对BFRP筋与混杂钢纤维UHPC的黏结性能进行了试验研究,分析了回收轮胎钢纤维(RTSF)掺量、UHPC保护层厚度、UHPC龄期及不同纤维掺入比例对BFRP筋-UHPC结构黏结破坏模式、黏结滑移响应和黏结强度的影响。结果表明:BFRP筋-UHPC结构有拔出破坏、劈裂破坏和拔出且劈裂破坏3种黏结破坏形态;BFRP筋-UHPC结构的极限黏结强度随着UHPC保护层厚度、UHPC龄期的增大而增大,且RTSF掺量由0%提升至3%时极限黏结强度提升了42.3%,但随着RTSF掺量的增大提升效果逐渐减弱。基于试验结果提出了BFRP筋-UHPC结构的黏结滑移本构模型,模型模拟曲线与试验曲线吻合较好。 展开更多
关键词 BFRP筋 超高性能混凝土 钢纤维 拉拔试验 黏结滑移曲线
在线阅读 下载PDF
钢纤维对SAP内养护混凝土动态压缩和弯曲性能的影响
14
作者 司政 宋健 +3 位作者 刘润 杜晓奇 黄灵芝 张飞跃 《应用力学学报》 北大核心 2025年第3期609-619,共11页
为了研究外掺钢纤维对内养护混凝土力学性能的影响,采用高吸水性聚合物(super absorbent polymer,SAP)作为内养护材料,开展了普通混凝土(normal concrete,NC)、内养护混凝土(internal curing concrete,ICC)和钢纤维内养护混凝土(steel f... 为了研究外掺钢纤维对内养护混凝土力学性能的影响,采用高吸水性聚合物(super absorbent polymer,SAP)作为内养护材料,开展了普通混凝土(normal concrete,NC)、内养护混凝土(internal curing concrete,ICC)和钢纤维内养护混凝土(steel fiber internal cured concrete,SFRICC)的动态抗压试验以及四点弯曲梁试验。使用核磁共振仪(nuclear magnetic resonance,NMR)和扫描电子显微镜(scanning electron microscope,SEM)研究混凝土内部孔隙结构和微观结构特征,揭示SAP和钢纤维对混凝土力学性能影响机理。结果表明:SFRICC残余强度随钢纤维掺量增加呈现增大趋势;钢纤维显著降低了SAP对混凝土力学性能的削弱作用;SFRICC的力学性能随钢纤维掺量的增加呈现先增大后减小趋势,钢纤维体积含量为1.5%时的SFRICC力学性能增强效果最好。混凝土力学性能呈现出明显的应变率效应。在高应变速率下,钢纤维掺量与SFRICC的动态增强因子(dynamic increase factor,DIF)呈负相关。SAP在促进水泥水化反应的同时,增大混凝土孔隙率和孔径,减少混凝土结构面有效面积,而钢纤维桥接纤维两侧的裂缝,增强了混凝土的完整性,弥补了SAP对混凝土的强度损失,两种材料可以发挥良好的耦合作用。 展开更多
关键词 混凝土 钢纤维 SAP 力学性能 微观机理
在线阅读 下载PDF
纤维自密实再生混凝土力学性能及早期抗裂性能研究
15
作者 张丽娟 何萌 +1 位作者 赵军 王志 《建筑科学与工程学报》 北大核心 2025年第5期105-114,共10页
将钢纤维和聚丙烯纤维掺入自密实再生混凝土中制备试件,通过试验研究了纤维对其坍落扩展度、抗压强度、劈拉强度的影响;基于ASTM C1579设计了一种小型平板开裂模具,使用该模具测试了自密实再生混凝土的早期抗裂性能;对比分析了两种纤维... 将钢纤维和聚丙烯纤维掺入自密实再生混凝土中制备试件,通过试验研究了纤维对其坍落扩展度、抗压强度、劈拉强度的影响;基于ASTM C1579设计了一种小型平板开裂模具,使用该模具测试了自密实再生混凝土的早期抗裂性能;对比分析了两种纤维对自密实再生混凝土力学性能的影响,建立了纤维自密实再生混凝土抗压强度和劈拉强度的计算公式。结果表明:使用再生骨料使自密实混凝土坍落扩展度降低2.4%,平均裂缝宽度增加15.9%,裂缝变异系数增大58.8%;两种纤维的掺入进一步降低了再生自密实混凝土的流动性,但改善了其早期抗裂性能;钢纤维和聚丙烯纤维的裂缝降低系数最高分别达到65.4%和53%,并使自密实再生混凝土的裂缝变异系数减小了55.6%和66.7%;纤维对自密实再生混凝土抗压强度的增强效果较弱,对劈拉强度的增强效果较为明显,钢纤维和聚丙烯纤维的掺入使劈拉强度最高增幅分别达到了127%和26%。 展开更多
关键词 纤维自密实再生混凝土 钢纤维 聚丙烯纤维 流动性 力学性能 早期抗裂性能
在线阅读 下载PDF
混杂纤维-硅溶胶改性再生混凝土性能试验
16
作者 王兴国 柳志炫 +3 位作者 王永贵 姜茂林 宋广明 程朝霞 《铁道工程学报》 北大核心 2025年第5期98-103,共6页
研究目的:再生混凝土的界面过渡区较薄弱,微孔隙较多,导致力学性能下降,严重危害混凝土结构的安全性和耐久性。为研究纳米SiO_(2)溶液对再生碎石料预浸泡的浓度、混掺钢-聚乙烯醇纤维量等因素对再生混凝土力学性能的影响,拟采用正交试验... 研究目的:再生混凝土的界面过渡区较薄弱,微孔隙较多,导致力学性能下降,严重危害混凝土结构的安全性和耐久性。为研究纳米SiO_(2)溶液对再生碎石料预浸泡的浓度、混掺钢-聚乙烯醇纤维量等因素对再生混凝土力学性能的影响,拟采用正交试验,设计16组纳米SiO_(2)改性骨料-钢/PVA纤维再生混凝土试块测试各因素对其抗压强度、劈裂抗拉强度的影响规律。研究结论:(1)掺入纤维可以改善再生混凝土内部的应力状态,使破坏后的试件仍保持一定的整体性;(2)纳米SiO_(2)溶液可以改善再生混凝土的界面过渡区性能,使混凝土内部更加致密化;(3)钢纤维掺量对混凝土抗压强度和劈裂抗拉强度影响最大且呈正向影响,PVA纤维掺量对混凝土抗压强度和劈裂抗拉强度影响较小,而再生粗骨料取代率对混凝土抗压强度和劈裂抗拉强度具有负向影响;(4)提出的纳米SiO_(2)改性骨料-钢/PVA纤维再生混凝土抗压强度和劈裂抗拉强度预测模型,对再生混凝土工程应用有一定参考价值。 展开更多
关键词 再生混凝土 纳米SiO_(2) 钢纤维 PVA纤维 正交试验 力学性能
在线阅读 下载PDF
内嵌式光纤布拉格光栅传感器智能钢绞线有效预应力监测技术的工程应用 被引量:1
17
作者 贾俊峰 侯智献 +3 位作者 杜瑞民 王蕾 白石 李小龙 《济南大学学报(自然科学版)》 北大核心 2025年第2期228-237,244,共11页
为了解决实际工程中预应力混凝土结构体内有效预应力无法监测的问题,根据光纤布拉格光栅传感器在结构健康监测中具有精度高、实时性强等优点,探讨内嵌式光纤布拉格光栅传感器智能钢绞线有效预应力监测技术的工程应用;通过对该智能钢绞... 为了解决实际工程中预应力混凝土结构体内有效预应力无法监测的问题,根据光纤布拉格光栅传感器在结构健康监测中具有精度高、实时性强等优点,探讨内嵌式光纤布拉格光栅传感器智能钢绞线有效预应力监测技术的工程应用;通过对该智能钢绞线开展拉伸试验,检验智能钢绞线的拉伸强度、线性度等参数;以云南省某高速公路预应力混凝土T梁桥示范工程为例,同时监测预应力混凝土T梁桥正、负弯矩区智能钢绞线张拉过程中智能钢绞线内的有效预应力,得到正弯矩区混凝土弹性压缩、智能钢绞线与孔道间摩擦、锚具变形和智能钢绞线内缩造成的预应力损失,并与千斤顶张拉应力及预应力损失的规范理论计算值对比。结果表明:该智能钢绞线力学性能和线性度良好,并且应变灵敏度系数即每微应变波长的变化值为1.22~1.26 pm,与应变灵敏度系数的理论值1.21 pm相差较小;相对于千斤顶张拉应力及有效预应力的规范理论计算值,预应力混凝土T梁桥正、负弯矩区智能钢绞线张拉过程中各测点处光纤布拉格光栅传感器监测应力的最大误差不超过3.86%,并且与预应力损失的规范理论计算值相比,该智能钢绞线在各测点处的预应力损失监测值误差较小;该智能钢绞线表现出良好的可靠性和稳定性,能满足实际工程需求。 展开更多
关键词 结构健康监测 有效预应力 智能钢绞线 光纤布拉格光栅传感器 工程应用
在线阅读 下载PDF
钢渣-钢纤维水泥基复合材料的自感知性能
18
作者 周中一 洪雅妮 +1 位作者 庞新龙 王涛 《北京工业大学学报》 北大核心 2025年第9期1092-1101,共10页
为了研究钢渣对硅砂的替代率、钢渣粒径和钢纤维掺量对该复合材料力学性能和自感知性能的影响,进行了不同配合比的水泥基自感知复合材料力学性能和自感知性能试验,结果表明:钢渣粒径对自感知复合材料抗压强度的影响显著;极化效应会引起... 为了研究钢渣对硅砂的替代率、钢渣粒径和钢纤维掺量对该复合材料力学性能和自感知性能的影响,进行了不同配合比的水泥基自感知复合材料力学性能和自感知性能试验,结果表明:钢渣粒径对自感知复合材料抗压强度的影响显著;极化效应会引起试件电阻大幅增加进而干扰压阻效应测试中电阻的测量,通电一定时间后极化效应趋于稳定,电阻不再增加;增加钢纤维含量可缩短极化稳定时间,针对钢渣、钢纤维自感知复合材料,建议预极化处理时间为20 min以减小极化效应的不利影响;增加钢纤维掺量可提高复合材料应力感知灵敏度,应力传感灵敏度最高为1.36×10-3MPa-1。 展开更多
关键词 钢渣 钢纤维 水泥基复合材料 自感知 压阻效应 应力灵敏度
在线阅读 下载PDF
带缝钢-聚丙烯混杂纤维混凝土碳化试验研究 被引量:1
19
作者 吴海林 李岳松 +2 位作者 周超月 张玉 何卫平 《混凝土》 北大核心 2025年第5期22-26,共5页
为了探讨钢-聚丙烯混杂纤维混凝土在裂缝状态下的碳化规律,设计并开展带缝钢-聚丙烯混杂纤维混凝土的碳化试验,研究了不同裂缝性状和纤维掺量对混凝土碳化深度的影响。结果显示,裂缝宽度和深度均显著影响混凝土的碳化深度,裂缝处碳化深... 为了探讨钢-聚丙烯混杂纤维混凝土在裂缝状态下的碳化规律,设计并开展带缝钢-聚丙烯混杂纤维混凝土的碳化试验,研究了不同裂缝性状和纤维掺量对混凝土碳化深度的影响。结果显示,裂缝宽度和深度均显著影响混凝土的碳化深度,裂缝处碳化深度随裂缝宽度和深度的增加而增大。掺入混杂纤维可减小同等条件下混凝土的碳化深度,混杂纤维混凝土在钢纤维体积掺量1.5%、聚丙烯纤维掺量0.06%时,碳化深度最小,相较于素混凝土、单掺钢纤维和单掺聚丙烯纤维混凝土,最大碳化深度分别降低了47.5%、5.9%、42.9%。开裂后,混杂纤维混凝土裂缝处碳化深度增加,但仍低于同种状态下素混凝土和单掺纤维混凝土。研究证实,适量掺入钢纤维和聚丙烯纤维能有效提高混凝土在开裂状态下的抗碳化性能。 展开更多
关键词 钢-聚丙烯混杂纤维混凝土 裂缝 碳化试验 碳化深度
在线阅读 下载PDF
纤维对3D打印UHPC流变性能和力学性能的影响
20
作者 赵宇 王哲 朱伶俐 《硅酸盐通报》 北大核心 2025年第8期2823-2838,共16页
超高性能混凝土(ultra-high performance concrete,UHPC)具有超高的强度及出色的耐久性能,然而,UHPC的低水胶比及掺加纤维等因素,使得其流动性能欠佳,进而影响3D打印超高性能混凝土(3D printing of ultra-high performance concrete,3DP... 超高性能混凝土(ultra-high performance concrete,UHPC)具有超高的强度及出色的耐久性能,然而,UHPC的低水胶比及掺加纤维等因素,使得其流动性能欠佳,进而影响3D打印超高性能混凝土(3D printing of ultra-high performance concrete,3DP-UHPC)在打印过程中的可挤出性能和可建造性能。为了制备适用于高温环境下的3DP-UHPC,本文探究了不同长度、掺量的钢纤维和不同掺量的聚丙烯纤维对3DP-UHPC流变性能、早期力学性能、硬化后力学性能的影响,为后续高温测试提供前期理论依据。结果表明,钢纤维长度是影响可挤出性能的关键因素,钢纤维和聚丙烯纤维的掺量是影响可建造性能的关键因素。随着聚丙烯纤维掺量的增加,湿坯强度逐渐降低,和静态屈服应力发展趋势相同。3D打印工艺约束了钢纤维沿打印方向的定向排列,使打印试块抗折强度较传统浇筑试块提升较高,且孔隙分布呈现差异化特征。 展开更多
关键词 3D打印超高性能混凝土 钢纤维 流变性能 湿坯强度 硬化后力学性能 三维孔隙分析
在线阅读 下载PDF
上一页 1 2 90 下一页 到第
使用帮助 返回顶部