Study on the Zirconolite Solidification of Simulated Np/Pu Radioactive Incineration Ash
1
作者 WEN Mingfen WANG Jianchen 《矿物学报》 CAS CSCD 北大核心 2013年第S1期108-108,共1页
High level waste is nuclear energy generated during the application process ,which is the greatest and the most difficult to management the waste. Proper treatment and disposal of it has already become a worldwide pro... High level waste is nuclear energy generated during the application process ,which is the greatest and the most difficult to management the waste. Proper treatment and disposal of it has already become a worldwide problem, and has become one of the key factors of restricting nuclear energy for sustainable development. Zirconolite (CaZrTi2O7) is one of the most stable mineral on the Earth and actinide major parasitic phase, therefore, it is widely used to solidify actinides separated from high level radioactive waste. In this paper, the zirconolite solid solution was synthesized by high temperature solid-stated method using a particular composition of simulated Np/Pu radioactive incineration ash (SRIA). The phase composition has been investigated by X-ray diffraction (XRD), the calcined temperature gained according to thermogravimetry scanning calorimeter (TG-DSC) analysis. Anti-leaching performance has also been researched with MCC-1 method. Results show that CaZrTi2O7 can load 40% SRIA, the accumulated leaching fraction of Ca is only about 10-4 cm in 28 days at 90 ℃, the concentrations of Zr , Ti and other noble metal ions were all less than detectability of ICP-MS, the leaching rate , normalization leaching rate, and accumulated leaching fraction of all Zr , Ti and other noble ions were 10-8 cm/d, 10-8 g/cm2·d and 10-7 cm, the results indicate that the zirconolite solidification has excellent chemical durability. 展开更多
关键词 ZIRCONOLITE SOLIDIFICATION simulated np/pu radioactive incineration ash leaching performance
在线阅读 下载PDF
碱矿渣复合水泥固化模拟放射性焚烧灰 被引量:11
2
作者 李长成 赵颜红 +1 位作者 潘社奇 崔琪 《原子能科学技术》 EI CAS CSCD 北大核心 2010年第4期400-407,共8页
用偏高岭土、沸石及聚合物乳胶粉改性的碱矿渣复合水泥进行了模拟放射性焚烧灰固化处置研究。结果表明:模拟放射性焚烧灰包容量为40%时,水泥固化体性能满足国标GB14569.1—93要求。Cs+的第42d浸出率(GB7023—86,25℃)最低为1.32×10... 用偏高岭土、沸石及聚合物乳胶粉改性的碱矿渣复合水泥进行了模拟放射性焚烧灰固化处置研究。结果表明:模拟放射性焚烧灰包容量为40%时,水泥固化体性能满足国标GB14569.1—93要求。Cs+的第42d浸出率(GB7023—86,25℃)最低为1.32×10-4cm/d,累积浸出分数仅为0.041cm。28d抗压强度最低为45.6MPa,且后期强度增长依然较高。碱矿渣复合水泥凝结迅速,克服了焚烧灰中某些成分对水化造成的不利影响。偏高岭土、沸石之间存在协同效应,显著提高固化体的抗压强度,同时改善对核素离子的固化能力。乳胶粉在固化体内形成三维网状结构,改善固化体韧性及抗冲击性,引入的微小气泡优化孔结构、提高耐久性,但导致抗压强度下降,掺量以5%为宜。 展开更多
关键词 碱矿渣复合水泥 模拟放射性焚烧灰 固化 乳胶粉 偏高岭土
在线阅读 下载PDF