A pre-reduction sintering process with flue gas recirculation(PSP_(fsg)-FGR)was developed to mitigate alkalis harm to the blast furnace and reduce the flue gas emission in the whole ironmaking process.The results indi...A pre-reduction sintering process with flue gas recirculation(PSP_(fsg)-FGR)was developed to mitigate alkalis harm to the blast furnace and reduce the flue gas emission in the whole ironmaking process.The results indicated that the pre-reduction sintering process(PSP)can effectively remove 58.02%of K and 30.68%of Na from raw mixtures and improve yield and tumbler index to 74.40%and 68.69%,respectively.Moreover,PSP was conducive to reducing NO_(x) and SO_(2)emissions and simultaneously increasing CO content in flue gas.Circulating CO-containing flue gas to sintering bed effectively recycled CO and further improved K and Na removal ratio to 74.11%and 32.92%,respectively.Microstructural analysis revealed that the pre-reduced sinter mainly consisted of magnetite,wustite and a small quantity of metallic iron,and very few silicate glass phase was also formed.This process can simultaneously realize alkali metal elements removal as well as flue gas emission reduction from the integrated ironmaking process.展开更多
It is of great significance for cleaner production to substitute bio-energy for fossil fuels in iron ore sintering. However, with the replacement ratio increasing, the consistency of heat front and flame front is brok...It is of great significance for cleaner production to substitute bio-energy for fossil fuels in iron ore sintering. However, with the replacement ratio increasing, the consistency of heat front and flame front is broken, and the thermal utilizing efficiency of fuel is reduced, which results in the decrease of yield and tumble index of sinter. Circulating flue gas to sintering bed as biochar replacing 40% coke, CO in flue gas can be reused so as to increase the thermal utilizing efficiency of fuels, and the consistency of two fronts is recovered for the circulating flue gas containing certain CO2, H2 O and lower O2, which contributes to increasing the maximum temperature, extending the high temperature duration time of sintering bed, and results in improving the output and quality of sinter. In the condition of circulating 40% flue gas, the sintering with biomass fuels is strengthened, and the sintering indexes with biomass fuel replacing 40% coke breeze are comparative to those of using coke breeze completely.展开更多
基金Project(52274290)supported by the National Natural Science Foundation of ChinaProject(72088101)supported by the Basic Science Center Project for National Natural Science Foundation of China。
文摘A pre-reduction sintering process with flue gas recirculation(PSP_(fsg)-FGR)was developed to mitigate alkalis harm to the blast furnace and reduce the flue gas emission in the whole ironmaking process.The results indicated that the pre-reduction sintering process(PSP)can effectively remove 58.02%of K and 30.68%of Na from raw mixtures and improve yield and tumbler index to 74.40%and 68.69%,respectively.Moreover,PSP was conducive to reducing NO_(x) and SO_(2)emissions and simultaneously increasing CO content in flue gas.Circulating CO-containing flue gas to sintering bed effectively recycled CO and further improved K and Na removal ratio to 74.11%and 32.92%,respectively.Microstructural analysis revealed that the pre-reduced sinter mainly consisted of magnetite,wustite and a small quantity of metallic iron,and very few silicate glass phase was also formed.This process can simultaneously realize alkali metal elements removal as well as flue gas emission reduction from the integrated ironmaking process.
基金Projects(51174253,51304245) supported by National Natural Science Foundation of China
文摘It is of great significance for cleaner production to substitute bio-energy for fossil fuels in iron ore sintering. However, with the replacement ratio increasing, the consistency of heat front and flame front is broken, and the thermal utilizing efficiency of fuel is reduced, which results in the decrease of yield and tumble index of sinter. Circulating flue gas to sintering bed as biochar replacing 40% coke, CO in flue gas can be reused so as to increase the thermal utilizing efficiency of fuels, and the consistency of two fronts is recovered for the circulating flue gas containing certain CO2, H2 O and lower O2, which contributes to increasing the maximum temperature, extending the high temperature duration time of sintering bed, and results in improving the output and quality of sinter. In the condition of circulating 40% flue gas, the sintering with biomass fuels is strengthened, and the sintering indexes with biomass fuel replacing 40% coke breeze are comparative to those of using coke breeze completely.