This paper studies the friction stir spot welding of AA2024-T3/AA7075-T6 Al alloys in the ambient and underwater environments by clarifying the nugget features,microstructure,fracture and mechanical properties of the ...This paper studies the friction stir spot welding of AA2024-T3/AA7075-T6 Al alloys in the ambient and underwater environments by clarifying the nugget features,microstructure,fracture and mechanical properties of the joints.The results show that the water-cooling medium exhibits a significant heat absorption capacity in the AA2024-T3/AA7075-T6 welded joint.Nugget features such as stir zone width,circular imprints,average grain sizes,and angular inter-material hooking are reduced by the watercooling effect in the joints.Narrower whitish(intercalated structures)bands are formed in the underwater joints while Mg2Si and Al2CuMg precipitates are formed in the ambient and the underwater welded joints respectively.An increase in tool rotational speed(600e1400 rpm)and plunge depth(0.1 e0.5 mm)increases the tensile-shear force of the welded AA2024-T3/AA7075-T6 joints in both the ambient and underwater environments.The maximum tensile-shear forces of 5900 N and 6700 N were obtained in the ambient and the underwater welds respectively.展开更多
The microstructure and mechanical properties of dissimilar pinless friction stir spot welded joint of2A12aluminum alloy and TC4titanium alloy were evaluated.The results show that the joint of Al/Ti dissimilar alloys c...The microstructure and mechanical properties of dissimilar pinless friction stir spot welded joint of2A12aluminum alloy and TC4titanium alloy were evaluated.The results show that the joint of Al/Ti dissimilar alloys can be successfully attained through pinless friction stir spot welding(FSSW).The joint can be divided into three zones(SZ,TMAZ and HAZ).The microstructure of joint in Al alloy side changes significantly but it basically has no change in Ti alloy side.At the same rotation speed,the maximum load of welded joints gradually rises with the increase in dwell time.At the same dwell time,the maximum load of the welded joint increases with the increase of the rotational speed.In addition,optimal parameters were obtained in this work,and they are rotation speed of1500r/min,plunge speed of30mm/min,plunge depth of0.3mm and dwell time of15s.The fracture mode of welded joints is interfacial shear fracture.The microhardness of the joint on the Al side distributes in a typical“W”type and is symmetry along the weld center,but the distribution of the microhardness on the Ti side has no obvious change.展开更多
The role of oxides in the formation of hole defects in friction stir welded joint of 2519-T87 aluminum alloy has been investigated by using optical microscope, scanning electron microscope, electron backscatter diffra...The role of oxides in the formation of hole defects in friction stir welded joint of 2519-T87 aluminum alloy has been investigated by using optical microscope, scanning electron microscope, electron backscatter diffraction and electron probe microanalyzer to examine the distribution of oxides and the features of hole defects, and using ABAQUS 3D thermo-mechanical coupling finite element model based on arbitrary Lagrangian-Eulerian method to simulate the material flow behavior. Oxides exist at the edge of tunnel hole and in the micropores in the joint. Based on distribution of oxygen and material flow behavior, it is believed that the oxides on the surface of the alloy tend to flow down into the bulk along the flow direction of plastic material during friction stir welding, aggregate in the weak region of material flow at the intersection of the shoulder affected zone and the stir pin-tip affected zone, and consequently prevent the material from contacting and diffusing. Due to the insufficient material flow and therefore the small plastic deformation,the pressure is not high enough to compress the accumulated oxides, resulting in hole defects.展开更多
基金Scientific Research Fund of Hunan Provincial Education Department(No.15C1240)Innovation platform open fund Project(No.16K080).
文摘This paper studies the friction stir spot welding of AA2024-T3/AA7075-T6 Al alloys in the ambient and underwater environments by clarifying the nugget features,microstructure,fracture and mechanical properties of the joints.The results show that the water-cooling medium exhibits a significant heat absorption capacity in the AA2024-T3/AA7075-T6 welded joint.Nugget features such as stir zone width,circular imprints,average grain sizes,and angular inter-material hooking are reduced by the watercooling effect in the joints.Narrower whitish(intercalated structures)bands are formed in the underwater joints while Mg2Si and Al2CuMg precipitates are formed in the ambient and the underwater welded joints respectively.An increase in tool rotational speed(600e1400 rpm)and plunge depth(0.1 e0.5 mm)increases the tensile-shear force of the welded AA2024-T3/AA7075-T6 joints in both the ambient and underwater environments.The maximum tensile-shear forces of 5900 N and 6700 N were obtained in the ambient and the underwater welds respectively.
基金Projects(51405389,51675435)supported by the National Natural Science Foundation of ChinaProject(3102017ZY005)supported by the Fundamental Research Funds for the Central Universities,China+3 种基金Project(SAST2016043)supported by the Fund of SAST,ChinaProject(20161125002)supported by the Aeronautical Science Foundation of ChinaProject(B08040)supported by the 111 Project,ChinaProjects(2016YFB0701203,2016YFB1100104)supported by the National Key Research and Development Program of China
文摘The microstructure and mechanical properties of dissimilar pinless friction stir spot welded joint of2A12aluminum alloy and TC4titanium alloy were evaluated.The results show that the joint of Al/Ti dissimilar alloys can be successfully attained through pinless friction stir spot welding(FSSW).The joint can be divided into three zones(SZ,TMAZ and HAZ).The microstructure of joint in Al alloy side changes significantly but it basically has no change in Ti alloy side.At the same rotation speed,the maximum load of welded joints gradually rises with the increase in dwell time.At the same dwell time,the maximum load of the welded joint increases with the increase of the rotational speed.In addition,optimal parameters were obtained in this work,and they are rotation speed of1500r/min,plunge speed of30mm/min,plunge depth of0.3mm and dwell time of15s.The fracture mode of welded joints is interfacial shear fracture.The microhardness of the joint on the Al side distributes in a typical“W”type and is symmetry along the weld center,but the distribution of the microhardness on the Ti side has no obvious change.
文摘The role of oxides in the formation of hole defects in friction stir welded joint of 2519-T87 aluminum alloy has been investigated by using optical microscope, scanning electron microscope, electron backscatter diffraction and electron probe microanalyzer to examine the distribution of oxides and the features of hole defects, and using ABAQUS 3D thermo-mechanical coupling finite element model based on arbitrary Lagrangian-Eulerian method to simulate the material flow behavior. Oxides exist at the edge of tunnel hole and in the micropores in the joint. Based on distribution of oxygen and material flow behavior, it is believed that the oxides on the surface of the alloy tend to flow down into the bulk along the flow direction of plastic material during friction stir welding, aggregate in the weak region of material flow at the intersection of the shoulder affected zone and the stir pin-tip affected zone, and consequently prevent the material from contacting and diffusing. Due to the insufficient material flow and therefore the small plastic deformation,the pressure is not high enough to compress the accumulated oxides, resulting in hole defects.