ZnO thin films with varying Ta concentrations were fabricated through magnetron sputtering.The crystallinity and surface morphology of the ZnO films are significantly influenced by the incorporation of Ta,as evidenced...ZnO thin films with varying Ta concentrations were fabricated through magnetron sputtering.The crystallinity and surface morphology of the ZnO films are significantly influenced by the incorporation of Ta,as evidenced by the X-ray diffraction and scanning electron microscopy results.The lattice constants,as determined by X-ray diffraction,contradict the disparity in Ta and Zn ion radii,which is attributed to the impact of interstitial defects.This inconsistency introduces variations in carrier concentration in this experiment compared with prior studies.Subsequent exploration of the luminescent characteristics and emission mechanism of defect levels in Ta-doped ZnO films was conducted through photoluminescence.Furthermore,the factors influencing the bandgap are discussed.展开更多
In this article,the effect of using water/zinc oxide nanofluid as a working fluid on the performance of solar collector is investigated experimentally.The volumetric concentration of nanoparticles is 0.4%,and the part...In this article,the effect of using water/zinc oxide nanofluid as a working fluid on the performance of solar collector is investigated experimentally.The volumetric concentration of nanoparticles is 0.4%,and the particle size is 40 nm,and the mass flow rate of the fluid varies from 1 to 3 kg/min.For this experiment,a device has been prepared with appropriate measuring instruments whose energy source is solar radiation.The solar energy absorbed by the flat plate collector is absorbed by the nanofluid of water/zinc oxide.The nanofluid is pumped to the consumer,a heat exchanger,where it heats the water.The temperature,radiation level,flow rate,and pressure in different parts of the device were measured.The pressure drop and the heat transferred are the most important results of this experimental work.The ASHRAE standard is used to calculate efficiency.The results showed that the use of water/zinc oxide nanofluid increases the collector performance compared to water.For 1 kg/min of mass flow rate,the nanofluids have a 16% increase in efficiency compared to water.From the results,it can be concluded that the choice of optimum mass flow rate in both water and nanofluid cases increases efficiency.展开更多
The leaching kinetics of low grade zinc oxide ore in NH3-NH4Cl-H2O system was studied. The effects of ore particle size, reaction temperature and the sum concentration of ammonium ion and ammonia on the leaching effic...The leaching kinetics of low grade zinc oxide ore in NH3-NH4Cl-H2O system was studied. The effects of ore particle size, reaction temperature and the sum concentration of ammonium ion and ammonia on the leaching efficiency of zinc were examined. The leaching kinetics of low-grade zinc oxide ore in NH3-NH4Cl-H2O system follows the kinetic law of shrinking-core model. The results show that diffusion through the inert particle pores is the leaching kinetics rate controlling step. The calculated apparent activation energy of the process is about 7.057 kJ/mol. The leaching efficiency of zinc is 92.1% under the conditions of ore particle size of 69 μm, holding at 80 ℃ for 60 min, sum ammonia concentration of 7.5 mol/L, the molar ratio of ammonium to ammonia being 2-1, and the ratio (g/mL) of solid to liquid being 1-10.展开更多
Zinc extraction from crude zinc oxide(CZO)is beneficial to the full utilization of secondary resources and environmental protection.In this paper,a systematic investigation was carried out to study the leaching behavi...Zinc extraction from crude zinc oxide(CZO)is beneficial to the full utilization of secondary resources and environmental protection.In this paper,a systematic investigation was carried out to study the leaching behavior of CZO by using ammonia-ammonium carbonate solution.It was found that the maximum leaching rate of zinc from CZO dust was 95.7%under the conditions of[Zn]T:[NH 3]T:[CO_(3)^(2−)]=1:7.00:1.75,liquid to solid ratio 5:1,leaching temperature 30℃ and leaching time 60 min.Compared with pure zinc oxide(PZO)leaching,the CZO leaching required longer time and more leaching agents,which is caused by the Cd^(2+),Pb^(2+) and other metal cationic impurities in CZO.The metal cationic impurities dissolved in the leaching solution and combined with ammonium to form complexes,consuming leaching agents and affecting zinc leaching.展开更多
ZnO-Bi2O3-based varistor ceramics doped with Yb2O3 in the range from 0 to 0.4% (molar fraction) were obtained by a solid reaction route. The X-ray diffractometry (XRD) and scanning electron microscopy (SEM) were...ZnO-Bi2O3-based varistor ceramics doped with Yb2O3 in the range from 0 to 0.4% (molar fraction) were obtained by a solid reaction route. The X-ray diffractometry (XRD) and scanning electron microscopy (SEM) were applied to characterize the phases and microstructure of the varistor ceramics, and a DC parameter instrument for varistor ceramics was applied to investigate their electrical properties and V-I characteristics. The XRD analysis of the samples shows that the ZnO phase, Bi2O3 phase, ZnTSbaOl2-type spinel phase and Zn2Bi3Sb3O14-type pyrochlore are present, and the Yb2O3 phases and Sb2O4 phases are found in varistor ceramics with increasing amounts of Yb2O3. The average size of ZnO grain firstly increases and then decreases with the increase of Yb2O3 content. The result also shows that the threshold voltage is between 656 V/nun and 1 232 V/mm, the nonlinear coefficient is in the range of 14.1-22.3, and the leakage current is between 0.60 μA and 19.6 μA. The 0.20% Yb2O3-added ZnO-Bi2O3-based varistor ceramics sintered at 900 ℃ have the best electrical characteristics.展开更多
Microstructure and electrical properties of La2 O3-doped ZnO-Bi2 O3 thin films prepared by sol–gel process have been investigated.X-ray diffraction shows that most diffraction peaks of ZnO are equal,and the crystals ...Microstructure and electrical properties of La2 O3-doped ZnO-Bi2 O3 thin films prepared by sol–gel process have been investigated.X-ray diffraction shows that most diffraction peaks of ZnO are equal,and the crystals of ZnO grow well.Scanning electron microscopy and atomic force microscopy results indicate that the samples have a good structure and lower surface roughness.The nonlinear V–I characteristics of the films show that La2 O3 develops the electrical properties largely and the best doped content is 0.3% lanthanum ion,with the leakage current of 0.25 mA,the threshold field of 150 V/mm and the nonlinear coefficient of 4.0 in detail.展开更多
基金supported by the National Natural Science Foundation of China(61774140).
文摘ZnO thin films with varying Ta concentrations were fabricated through magnetron sputtering.The crystallinity and surface morphology of the ZnO films are significantly influenced by the incorporation of Ta,as evidenced by the X-ray diffraction and scanning electron microscopy results.The lattice constants,as determined by X-ray diffraction,contradict the disparity in Ta and Zn ion radii,which is attributed to the impact of interstitial defects.This inconsistency introduces variations in carrier concentration in this experiment compared with prior studies.Subsequent exploration of the luminescent characteristics and emission mechanism of defect levels in Ta-doped ZnO films was conducted through photoluminescence.Furthermore,the factors influencing the bandgap are discussed.
文摘In this article,the effect of using water/zinc oxide nanofluid as a working fluid on the performance of solar collector is investigated experimentally.The volumetric concentration of nanoparticles is 0.4%,and the particle size is 40 nm,and the mass flow rate of the fluid varies from 1 to 3 kg/min.For this experiment,a device has been prepared with appropriate measuring instruments whose energy source is solar radiation.The solar energy absorbed by the flat plate collector is absorbed by the nanofluid of water/zinc oxide.The nanofluid is pumped to the consumer,a heat exchanger,where it heats the water.The temperature,radiation level,flow rate,and pressure in different parts of the device were measured.The pressure drop and the heat transferred are the most important results of this experimental work.The ASHRAE standard is used to calculate efficiency.The results showed that the use of water/zinc oxide nanofluid increases the collector performance compared to water.For 1 kg/min of mass flow rate,the nanofluids have a 16% increase in efficiency compared to water.From the results,it can be concluded that the choice of optimum mass flow rate in both water and nanofluid cases increases efficiency.
基金Project(2007CB613604) supported by the Major State Basic Research Development Program of ChinaProject(50674104) supported by the National Natural Science Foundation of ChinaProject(GJJ08279) supported by the Department of Education of Jiangxi Province
文摘The leaching kinetics of low grade zinc oxide ore in NH3-NH4Cl-H2O system was studied. The effects of ore particle size, reaction temperature and the sum concentration of ammonium ion and ammonia on the leaching efficiency of zinc were examined. The leaching kinetics of low-grade zinc oxide ore in NH3-NH4Cl-H2O system follows the kinetic law of shrinking-core model. The results show that diffusion through the inert particle pores is the leaching kinetics rate controlling step. The calculated apparent activation energy of the process is about 7.057 kJ/mol. The leaching efficiency of zinc is 92.1% under the conditions of ore particle size of 69 μm, holding at 80 ℃ for 60 min, sum ammonia concentration of 7.5 mol/L, the molar ratio of ammonium to ammonia being 2-1, and the ratio (g/mL) of solid to liquid being 1-10.
基金Project(2020YFC1909805)supported by the National Key Research and Development Program of ChinaProjects(51504293,51574284)supported by the National Natural Science Foundation of China+2 种基金Project(2018-GX-A7)supported by Qinghai Provincial Major Scientific and Technological Special Project of ChinaProject(2020SK2125)supported by the Key Research and Development Program of Hunan Province,ChinaProject(CSUZC202129)supported by Open Sharing Fund for the Large-scale Instruments and Equipments of Central South University,China。
文摘Zinc extraction from crude zinc oxide(CZO)is beneficial to the full utilization of secondary resources and environmental protection.In this paper,a systematic investigation was carried out to study the leaching behavior of CZO by using ammonia-ammonium carbonate solution.It was found that the maximum leaching rate of zinc from CZO dust was 95.7%under the conditions of[Zn]T:[NH 3]T:[CO_(3)^(2−)]=1:7.00:1.75,liquid to solid ratio 5:1,leaching temperature 30℃ and leaching time 60 min.Compared with pure zinc oxide(PZO)leaching,the CZO leaching required longer time and more leaching agents,which is caused by the Cd^(2+),Pb^(2+) and other metal cationic impurities in CZO.The metal cationic impurities dissolved in the leaching solution and combined with ammonium to form complexes,consuming leaching agents and affecting zinc leaching.
基金Project(BK2011243) supported by the Natural Science Foundation of Jiangsu Province,ChinaProject(2007DA10512711408) supported by the Visiting Scholarship of State Key Laboratory of Power Transmission Equipment & System Security and New Technology (Chongqing University),China+4 种基金Project(EIPE11204) supported by the State Key Laboratory of Electrical Insulation and Power Equipment,ChinaProject(KF201104) supported by the State Key Laboratory of New Ceramic and Fine Processing,ChinaProject(KFJJ201105) supported by the Opening Project of State Key Laboratory of Electronic Thin Films and Integrated Devices,ChinaProject(10KJD430002) supported by the Universities Natural Science Research Project of Jiangsu Province,ChinaProject(11JDG084) supported by the Research Foundation of Jiangsu University,China
文摘ZnO-Bi2O3-based varistor ceramics doped with Yb2O3 in the range from 0 to 0.4% (molar fraction) were obtained by a solid reaction route. The X-ray diffractometry (XRD) and scanning electron microscopy (SEM) were applied to characterize the phases and microstructure of the varistor ceramics, and a DC parameter instrument for varistor ceramics was applied to investigate their electrical properties and V-I characteristics. The XRD analysis of the samples shows that the ZnO phase, Bi2O3 phase, ZnTSbaOl2-type spinel phase and Zn2Bi3Sb3O14-type pyrochlore are present, and the Yb2O3 phases and Sb2O4 phases are found in varistor ceramics with increasing amounts of Yb2O3. The average size of ZnO grain firstly increases and then decreases with the increase of Yb2O3 content. The result also shows that the threshold voltage is between 656 V/nun and 1 232 V/mm, the nonlinear coefficient is in the range of 14.1-22.3, and the leakage current is between 0.60 μA and 19.6 μA. The 0.20% Yb2O3-added ZnO-Bi2O3-based varistor ceramics sintered at 900 ℃ have the best electrical characteristics.
基金Project(20123227120021)supported by the Specialized Research Fund for the Doctoral Program of Higher Education of ChinaProject(BK2012156)supported by the Natural Science Foundation of Jiangsu Province,China+3 种基金Project(KFJJ201105)supported by the Opening Project of State Key Laboratory of Electronic Thin Films and Integrated Devices,ChinaProject(CJ20125001)supported by the Application Program for Basic Research of Changzhou,ChinaProject(13KJB430006)supported by the Universities Natural Science Research project of Jiangsu Province,ChinaProject supported by the Industrial Center of Jiangsu University Undergraduate Practice-Innovation Training Program,China
文摘Microstructure and electrical properties of La2 O3-doped ZnO-Bi2 O3 thin films prepared by sol–gel process have been investigated.X-ray diffraction shows that most diffraction peaks of ZnO are equal,and the crystals of ZnO grow well.Scanning electron microscopy and atomic force microscopy results indicate that the samples have a good structure and lower surface roughness.The nonlinear V–I characteristics of the films show that La2 O3 develops the electrical properties largely and the best doped content is 0.3% lanthanum ion,with the leakage current of 0.25 mA,the threshold field of 150 V/mm and the nonlinear coefficient of 4.0 in detail.