Titanium alloy has the advantages of high strength,strong corrosion resistance,excellent high and low temperature mechanical properties,etc.,and is widely used in aerospace,shipbuilding,weapons and equipment,and other...Titanium alloy has the advantages of high strength,strong corrosion resistance,excellent high and low temperature mechanical properties,etc.,and is widely used in aerospace,shipbuilding,weapons and equipment,and other fields.In recent years,with the continuous increase in demand for medium-thick plate titanium alloys,corresponding welding technologies have also continued to develop.Therefore,this article reviews the research progress of deep penetration welding technology for medium-thick plate titanium alloys,mainly covering traditional arc welding,high-energy beam welding,and other welding technologies.Among many methods,narrow gap welding,hybrid welding,and external energy field assistance welding all contribute to improving the welding efficiency and quality of medium-thick plate titanium alloys.Finally,the development trend of deep penetration welding technology for mediumthick plate titanium alloys is prospected.展开更多
Metal matrix composites tiles based on Ti-6Al-4V(Ti64)alloy,reinforced with 10,20,and 40(vol%)of either TiC or TiB particles were made using press-and-sinter blended elemental powder metallurgy(BEPM)and then bonded to...Metal matrix composites tiles based on Ti-6Al-4V(Ti64)alloy,reinforced with 10,20,and 40(vol%)of either TiC or TiB particles were made using press-and-sinter blended elemental powder metallurgy(BEPM)and then bonded together into 3-layer laminated plates using hot isostatic pressing(HIP).The laminates were ballistically tested and demonstrated superior performance.The microstructure and properties of the laminates were analyzed to determine the effect of the BEPM and HIP processing on the ballistic properties of the layered plates.The effect of porosity in sintered composites on further diffusion bonding of the plates during HIP is analyzed to understand the bonding features at the interfaces between different adjacent layers in the laminate.Exceptional ballistic performance of fabricated structures was explained by a significant reduction in the residual porosity of the BEPM products by their additional processing using HIP,which provides an unprecedented increase in the hardness of the layered composites.It is argued that the combination of the used two technologies,BEPM and HIP is principally complimentary for the materials in question with the abilities to solve the essential problems of each used individually.展开更多
To develop an effective process for titanium powders production, a calciothermic reduction process of pigment titanium dioxide (w(TiO2)〉98%), based on the preform reduction process (PRP), was investigated by me...To develop an effective process for titanium powders production, a calciothermic reduction process of pigment titanium dioxide (w(TiO2)〉98%), based on the preform reduction process (PRP), was investigated by means of XRD, SEM and EDS. In this process, the mixture of TiO2 powder and CaC12 was pressed into pieces as feed preform and was reduced by calcium vapor. Titanium powders was recovered after leaching from the reduced preform with hydrochloric acid and deionized water. The results indicate when the mass ratio of CaC12 to TiO2 is about 1:4 and at a constant temperature of 1 273 K for 6 h in vacuum furnace, titanium powders with 99.55% purity by EDS analysis and irregular shape (8-15 μm in particle size) are obtained.展开更多
In order to produce low-cost titanium(Ti)with high productivity,fundamental studies on producing metallic Ti from titanium dioxide(TiO_(2))in the cold pressed pellets were conducted by metallothermic reduction with an...In order to produce low-cost titanium(Ti)with high productivity,fundamental studies on producing metallic Ti from titanium dioxide(TiO_(2))in the cold pressed pellets were conducted by metallothermic reduction with an indirect contact method.This paper focuses on discussing the mechanism of the reduction process and the relationships of RM(a revised reduction index)with reduction temperature,reduction time,and mole ratio of TiO_(2) to CaCl_(2)(nTiO_(2)/nCaCl_(2))in the pellets.The results show that metallic Ti was obtained from the reduction of TiO_(2) in the pellets by calcium(Ca)vapor;pellets were reduced homogenously and Ca vapor diffused into the porous pellets by Knudsen diffusion or the mixing diffusion of molecular diffusion and Knudsen diffusion at 1273 K;RM increased with the increases of temperature and reduction time and was 96.34%when T_(Redu)=1273 K,t_(Redu)=6 h,and nTiO_(2)/nCaCl_(2)=4;the reasonable nTiO_(2)/nCaCl_(2) value is 3−5 for the pellets with enough strength and high RM.展开更多
In this paper,the springback of TC4 titanium alloy under hot stamping condition was studied by means of experiment and numerical analysis.Firstly,an analytical model was established to predict the V-shaped springback ...In this paper,the springback of TC4 titanium alloy under hot stamping condition was studied by means of experiment and numerical analysis.Firstly,an analytical model was established to predict the V-shaped springback angleΔαunder the stretch-bending conditions.The model took into account of blank holder force,friction,property of the material,thickness of the sheet and the neutral layer shift.Then,the influence of several process parameters on springback was studied by experiment and finite element simulation using a V-shaped stamping tool.In the hot stamping tests,the titanium alloy sheet fractured seriously at room temperature.The titanium alloy has good formability when the initial temperature of the sheet is 750–900°C.However,the springback angle of formed parts is large and decreases with increasing temperature.The springback angleΔαdecreased by 50%from 0.5°to 0.25°,and the angleΔβdecreased by 46.7%from 1.5°to 0.8°when the initial temperature of sheet increased from 750°C to 900°C.The springback angle of titanium alloy sheet increases gradually with the increase of the punch radius,because of the increase of elastic recovery,the complex distribution of stress,the length of forming region and the decreasing degree of stress.Compared with the simulation results,the analytical model can better predict the springback angleΔα.展开更多
A yttrium-containing high-temperature titanium alloy(Ti-6Al-2.7Sn-4Zr-0.4Mo-0.45Si-0.1Y, mass fraction, %) has been additively manufactured using selective electron beam melting(SEBM). The resulting microstructure and...A yttrium-containing high-temperature titanium alloy(Ti-6Al-2.7Sn-4Zr-0.4Mo-0.45Si-0.1Y, mass fraction, %) has been additively manufactured using selective electron beam melting(SEBM). The resulting microstructure and textures were studied using scanning electron microscopy(SEM), transmission electron microscopy(TEM), X-ray diffraction(XRD) and electron backscattered diffraction(EBSD) and compared with the conventionally manufactured form. A notable distinct difference of microstructures is that additive manufacturing by SEBM enables homogeneous precipitation of fine Y2O3 dispersoids in the size range of 50-250 nm throughout the as-fabricated alloy, despite the presence of just trace levels of oxygen(7×10-4, mass fraction) and yttrium(10-3, mass fraction) in the alloy. In contrast, the conventionally manufactured alloy shows inhomogeneously distributed coarse Y2O3 precipitates, including cracked or debonded Y2O3 particles.展开更多
The expanding of material library of laser powder bed fusion(L-PBF)is of great significance to the development of material science.In this study,the biomedical Ti-13Nb-13Zr powder was mixed with the tantalum particles...The expanding of material library of laser powder bed fusion(L-PBF)is of great significance to the development of material science.In this study,the biomedical Ti-13Nb-13Zr powder was mixed with the tantalum particles(2 wt%−8 wt%)and fabricated by L-PBF.The microstructure consists of aβmatrix with partially unmelted pure tantalum distributed along the boundaries of molten pool owing to the Marangoni convention.Because the melting process of Ta absorbs lots of energy,the size of molten pool becomes smaller with the increase of Ta content.The fine microstructure exists in the center of melt pool while coarse microstructure is on the boundaries of melt pool because of the existence of heat-affected zone.The columnar-to-equiaxed transitions(CETs)happen in the zones near the unmelted Ta,and the low lattice mismatch induced by solid Ta phase is responsible for this phenomenon.The recrystallization texture is strengthened while the fiber texture is weakened when the tantalum content is increased.Due to the formation of refined martensiteα′grains during L-PBF,the compressive strengths of L-PBF-processed samples are higher than those fabricated by traditional processing technologies.The present research will provide an important reference for biomedical alloy design via L-PBF process in the future.展开更多
Anodic oxide films of titanium alloy Ti-10V-2Fe-3Al were sealed in calcium acetate solution. The morphology and composition of the sealed films were investigated using scanning electron microscopy (SEM), atomic force ...Anodic oxide films of titanium alloy Ti-10V-2Fe-3Al were sealed in calcium acetate solution. The morphology and composition of the sealed films were investigated using scanning electron microscopy (SEM), atomic force microscope (AFM) and energy dispersive spectroscopy (EDS). The results show that the sealing process makes the anodic oxide films more uniform. Elemental calcium is presented through the whole depth of the anodic oxide films. The roughness of the anodic oxide films is reduced after the sealing process. Electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization were used to study the corrosion behavior of the anodic oxide films. It is revealed that the sealing process improves the corrosion resistance of the anodic oxide film of titanium alloy Ti-10V-2Fe-3Al.展开更多
In the production process of titanium dioxide with sulfuric acid, the contamination of the titanium sulfate solution (the ilmenite leaching solution) in the Fe 3+ reduction stage by iron scraps is a practical problem ...In the production process of titanium dioxide with sulfuric acid, the contamination of the titanium sulfate solution (the ilmenite leaching solution) in the Fe 3+ reduction stage by iron scraps is a practical problem because it is difficult to guarantee the quality of the iron scraps. In this research, a new method, called the ion exchange membrane primary cell method, for reduction of Fe 3+ in the titanium sulfate solution has been advanced. The positive compartment of the primary cell consists of lead (copper) electrode and the titanium sulfate solution, and the negative compartment consists of iron electrode and acidic FeSO 4 solution. The anion ion exchange membrane is used as the diaphragm between two compartments. Fe 3+ in the titanium sulfate solution is reduced by the electric discharge of the primary cell. The effects of temperature, stirring strength of the solution and membrane area on the reduction rate have been investigated. The experimental result shows that the optimum current density can be higher than 100 A/m 2.展开更多
Titanium has found extensive use in various engineering applications due to its attractive physical,mechanical, and chemical characteristics. However, titanium has relatively low hardness for use as an armour material...Titanium has found extensive use in various engineering applications due to its attractive physical,mechanical, and chemical characteristics. However, titanium has relatively low hardness for use as an armour material. ZrB2 was incorporated to the Ti matrix to form a Ti-based binary composites. In this study, powder metallurgy techniques were employed to disperse the ceramic particulates throughout the matrix material then consolidated through spark plasma sintering. The composites were densified at1300 ℃, pressure of 50 MPa, and holding time of 5 min. The microstructure and phase analysis of the sintered composites was carried out using SEM and XRD, while the hardness was determined using Vickers' microhardness tester. The SEM and XRD results confirmed the presence of the TiB whiskers which renowned with the improving the hardness of titanium. The hardness of the composite with 10 wt% ZrB_2 showed the highest hardness compared to that obtained for the 5 and 15 wt% ZrB_2 composites which was 495 and 571 Hv respectively.展开更多
To determine mirror surface finishing conditions and efficient and economical superfinishing conditions for pure titanium and titanium alloys, an abrasive film is used when superfinishing is performed under varying co...To determine mirror surface finishing conditions and efficient and economical superfinishing conditions for pure titanium and titanium alloys, an abrasive film is used when superfinishing is performed under varying conditions. These conditions include the workpiece rotation speed, the oscillation speed, the contact pressure of the roller, the hardness of the roller, and the type of abrasive film. The superfinishing device is applied to polishing a thin and long cylindrical bar. A micro-finishing film and a lapping film were used as abrasive films. A1203 grains or SiC grains were used as abrasives. The surface roughness of a polished workpiece was measured using a stylus-type surface-roughness measuring instrument. As a result, the conditions to improve the polishing surface efficiently include high values for the workpiece rotation speed, oscillation speed and contact pressure. The roller hardness has no effect on the efficient polishing conditions. The mirror finish of a surface can be created using lapping film of 3 μm with Al2O3 grains after polishing to a steady surface roughness under the efficient polishing conditions.展开更多
Multilayer materials are widely used in military,automobile and aerospace industries.In this paper,the response of an explosion-welded Ti6Al4V/pure titanium with a flat interface to dynamic loading is investigated.An ...Multilayer materials are widely used in military,automobile and aerospace industries.In this paper,the response of an explosion-welded Ti6Al4V/pure titanium with a flat interface to dynamic loading is investigated.An SHPB apparatus is used.Then,the dynamic behaviour of a bimetal sample is explored with a DIC system coupled to the SHPB.Result indicates that in the bimetal sample pure titanium is deformed and failed before Ti6Al4V.The stress curve of the sample shows two different peaks in a striker velocity higher than the 18.3 m/s.When the incident wave encounters the interface of the Ti6Al4V/pure titanium sample,only a small fraction of the wave is reflected owing to similar impedance.Using the direct interpretation stress-strain curve is unreasonable in this case because of unhomogenised plastic deformation.The micro structure of the sample is investigated after loading.An adiabatic shear band is formed in the pure titanium side before failure,and the interface of the sample remains intact under different loading conditions.The FEM simulation result for the sample is in good agreement with experimental observations.展开更多
Ti/Fe clad plate had attracted extensive attention because of its important application. In order to reduce the titanium layer thickness, the explosive welding of TA1 titanium foil to Q235 steel plate was carried out....Ti/Fe clad plate had attracted extensive attention because of its important application. In order to reduce the titanium layer thickness, the explosive welding of TA1 titanium foil to Q235 steel plate was carried out. The interfacial bonding performance was analyzed by micromorphology analysis and mechanical property test, and the formation process of interfacial wave and molten block in the vortex was simulated by smoothed particle hydrodynamics(SPH) method. The results showed that salt as pressure transfer layer used in explosive welding could play a good buffer effect on the collision between flyer and base layers. Regular waveforms were formed on the bonding interface, and the titanium foil/steel clad plate exhibited good welding quality and bonding property. The crest of the observed interfacial wave moved 200 μm from the beginning to the final formation, and it was important of jet on the formation of interfacial waveform. The interface was mainly bonded in the form of molten layer, and the grains near the interface were streamlined. Molten block containing intermetallic compounds and metal oxides appeared in the vortex of wave crest.展开更多
The high-temperature acoustic absorption performance of porous titanium fiber material was investigated in terms of sample thickness, porosity, temperature, air-cavity thickness and double-layer structure arrangement....The high-temperature acoustic absorption performance of porous titanium fiber material was investigated in terms of sample thickness, porosity, temperature, air-cavity thickness and double-layer structure arrangement. The effects on absorption coefficient were systematically assessed. The results show that the sound absorption performance is improved by increasing the sample porosity and/or thickness, and/or increasing the air-cavity thickness. Meanwhile, increasing the temperature gives better acoustic absorption performance in the low frequency range but also lowers the performance in the high frequency range, while double-layer structure enables better acoustic absorption performance.展开更多
Titanium minerals are of interest because they constitute the most important source of titanium,a strategic metal in modem industry.However, knowledge on their structure,composition,and properties of nanodisperse stru...Titanium minerals are of interest because they constitute the most important source of titanium,a strategic metal in modem industry.However, knowledge on their structure,composition,and properties of nanodisperse structures has been limited. Several studies have shown that synthetic analogs of natural titanium oxides have structural features and physico-chemical properties distinctly different展开更多
基金financially supported by the Key Research and Development Program of Ningbo(Grant No.2023Z098)Natural Science Foundation of Inner Mongolia(Grant No.2023MS05040)+1 种基金Shenyang Collaborative Innovation Center Project for Multiple Energy Fields Composite Processing of Special Materials(Grant No.JG210027)Shenyang Key Technology Special Project of The Open Competition Mechanism to Select the Best Solution(Grant Nos.2022210101000827,2022-0-43-048).
文摘Titanium alloy has the advantages of high strength,strong corrosion resistance,excellent high and low temperature mechanical properties,etc.,and is widely used in aerospace,shipbuilding,weapons and equipment,and other fields.In recent years,with the continuous increase in demand for medium-thick plate titanium alloys,corresponding welding technologies have also continued to develop.Therefore,this article reviews the research progress of deep penetration welding technology for medium-thick plate titanium alloys,mainly covering traditional arc welding,high-energy beam welding,and other welding technologies.Among many methods,narrow gap welding,hybrid welding,and external energy field assistance welding all contribute to improving the welding efficiency and quality of medium-thick plate titanium alloys.Finally,the development trend of deep penetration welding technology for mediumthick plate titanium alloys is prospected.
基金funding from the NATO Agency Science for Peace and Security (#G5787)Ballistic investigations were co-financed by Military University of Technology in Warsaw under research project UGB 829/2023/WATSeparate works made in G.V.Kurdyumov Institute for Metal Physics of N.A.S.of Ukraine were partially financially supported by N.A.S.of Ukraine within the frames of project#III09-18。
文摘Metal matrix composites tiles based on Ti-6Al-4V(Ti64)alloy,reinforced with 10,20,and 40(vol%)of either TiC or TiB particles were made using press-and-sinter blended elemental powder metallurgy(BEPM)and then bonded together into 3-layer laminated plates using hot isostatic pressing(HIP).The laminates were ballistically tested and demonstrated superior performance.The microstructure and properties of the laminates were analyzed to determine the effect of the BEPM and HIP processing on the ballistic properties of the layered plates.The effect of porosity in sintered composites on further diffusion bonding of the plates during HIP is analyzed to understand the bonding features at the interfaces between different adjacent layers in the laminate.Exceptional ballistic performance of fabricated structures was explained by a significant reduction in the residual porosity of the BEPM products by their additional processing using HIP,which provides an unprecedented increase in the hardness of the layered composites.It is argued that the combination of the used two technologies,BEPM and HIP is principally complimentary for the materials in question with the abilities to solve the essential problems of each used individually.
基金Project(51004058) supported by the National Natural Science Foundation of ChinaProject(2011FB039) supported by the Natural Science Foundation of Yunnan Province,China
文摘To develop an effective process for titanium powders production, a calciothermic reduction process of pigment titanium dioxide (w(TiO2)〉98%), based on the preform reduction process (PRP), was investigated by means of XRD, SEM and EDS. In this process, the mixture of TiO2 powder and CaC12 was pressed into pieces as feed preform and was reduced by calcium vapor. Titanium powders was recovered after leaching from the reduced preform with hydrochloric acid and deionized water. The results indicate when the mass ratio of CaC12 to TiO2 is about 1:4 and at a constant temperature of 1 273 K for 6 h in vacuum furnace, titanium powders with 99.55% purity by EDS analysis and irregular shape (8-15 μm in particle size) are obtained.
基金Projects(51774071,50804007,51974073)supported by the National Natural Science Foundation of China。
文摘In order to produce low-cost titanium(Ti)with high productivity,fundamental studies on producing metallic Ti from titanium dioxide(TiO_(2))in the cold pressed pellets were conducted by metallothermic reduction with an indirect contact method.This paper focuses on discussing the mechanism of the reduction process and the relationships of RM(a revised reduction index)with reduction temperature,reduction time,and mole ratio of TiO_(2) to CaCl_(2)(nTiO_(2)/nCaCl_(2))in the pellets.The results show that metallic Ti was obtained from the reduction of TiO_(2) in the pellets by calcium(Ca)vapor;pellets were reduced homogenously and Ca vapor diffused into the porous pellets by Knudsen diffusion or the mixing diffusion of molecular diffusion and Knudsen diffusion at 1273 K;RM increased with the increases of temperature and reduction time and was 96.34%when T_(Redu)=1273 K,t_(Redu)=6 h,and nTiO_(2)/nCaCl_(2)=4;the reasonable nTiO_(2)/nCaCl_(2) value is 3−5 for the pellets with enough strength and high RM.
基金Projects(U1564202,51705018)supported by the National Natural Science Foundation of ChinaProject supported by the Beijing Laboratory of Modern Transportation Metal Materials and Processing Technology and the Beijing Key Laboratory of Metal Forming Lightweight,China。
文摘In this paper,the springback of TC4 titanium alloy under hot stamping condition was studied by means of experiment and numerical analysis.Firstly,an analytical model was established to predict the V-shaped springback angleΔαunder the stretch-bending conditions.The model took into account of blank holder force,friction,property of the material,thickness of the sheet and the neutral layer shift.Then,the influence of several process parameters on springback was studied by experiment and finite element simulation using a V-shaped stamping tool.In the hot stamping tests,the titanium alloy sheet fractured seriously at room temperature.The titanium alloy has good formability when the initial temperature of the sheet is 750–900°C.However,the springback angle of formed parts is large and decreases with increasing temperature.The springback angleΔαdecreased by 50%from 0.5°to 0.25°,and the angleΔβdecreased by 46.7%from 1.5°to 0.8°when the initial temperature of sheet increased from 750°C to 900°C.The springback angle of titanium alloy sheet increases gradually with the increase of the punch radius,because of the increase of elastic recovery,the complex distribution of stress,the length of forming region and the decreasing degree of stress.Compared with the simulation results,the analytical model can better predict the springback angleΔα.
基金Projects(2014KTZB01-02-03,2014KTZB01-02-04)supported by Shaanxi Science and Technology Coordination and Innovation Program,ChinaProject(DP120101672)supported by Australian Research Council(ARC)Discovery Grant,ARC Centre of Excellence for Design in Light Metals,Australia
文摘A yttrium-containing high-temperature titanium alloy(Ti-6Al-2.7Sn-4Zr-0.4Mo-0.45Si-0.1Y, mass fraction, %) has been additively manufactured using selective electron beam melting(SEBM). The resulting microstructure and textures were studied using scanning electron microscopy(SEM), transmission electron microscopy(TEM), X-ray diffraction(XRD) and electron backscattered diffraction(EBSD) and compared with the conventionally manufactured form. A notable distinct difference of microstructures is that additive manufacturing by SEBM enables homogeneous precipitation of fine Y2O3 dispersoids in the size range of 50-250 nm throughout the as-fabricated alloy, despite the presence of just trace levels of oxygen(7×10-4, mass fraction) and yttrium(10-3, mass fraction) in the alloy. In contrast, the conventionally manufactured alloy shows inhomogeneously distributed coarse Y2O3 precipitates, including cracked or debonded Y2O3 particles.
基金Projects(51975061,51775055)supported by the National Natural Science Foundation of ChinaProject(2020JJ5599)supported by the Natural Science Foundation of Hunan Province,ChinaProjects(19C0032,19B033)supported by the Research Foundation of Education Bureau of Hunan Province,China。
文摘The expanding of material library of laser powder bed fusion(L-PBF)is of great significance to the development of material science.In this study,the biomedical Ti-13Nb-13Zr powder was mixed with the tantalum particles(2 wt%−8 wt%)and fabricated by L-PBF.The microstructure consists of aβmatrix with partially unmelted pure tantalum distributed along the boundaries of molten pool owing to the Marangoni convention.Because the melting process of Ta absorbs lots of energy,the size of molten pool becomes smaller with the increase of Ta content.The fine microstructure exists in the center of melt pool while coarse microstructure is on the boundaries of melt pool because of the existence of heat-affected zone.The columnar-to-equiaxed transitions(CETs)happen in the zones near the unmelted Ta,and the low lattice mismatch induced by solid Ta phase is responsible for this phenomenon.The recrystallization texture is strengthened while the fiber texture is weakened when the tantalum content is increased.Due to the formation of refined martensiteα′grains during L-PBF,the compressive strengths of L-PBF-processed samples are higher than those fabricated by traditional processing technologies.The present research will provide an important reference for biomedical alloy design via L-PBF process in the future.
基金Project(51171011)supported by the National Natural Science Foundation of China
文摘Anodic oxide films of titanium alloy Ti-10V-2Fe-3Al were sealed in calcium acetate solution. The morphology and composition of the sealed films were investigated using scanning electron microscopy (SEM), atomic force microscope (AFM) and energy dispersive spectroscopy (EDS). The results show that the sealing process makes the anodic oxide films more uniform. Elemental calcium is presented through the whole depth of the anodic oxide films. The roughness of the anodic oxide films is reduced after the sealing process. Electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization were used to study the corrosion behavior of the anodic oxide films. It is revealed that the sealing process improves the corrosion resistance of the anodic oxide film of titanium alloy Ti-10V-2Fe-3Al.
文摘In the production process of titanium dioxide with sulfuric acid, the contamination of the titanium sulfate solution (the ilmenite leaching solution) in the Fe 3+ reduction stage by iron scraps is a practical problem because it is difficult to guarantee the quality of the iron scraps. In this research, a new method, called the ion exchange membrane primary cell method, for reduction of Fe 3+ in the titanium sulfate solution has been advanced. The positive compartment of the primary cell consists of lead (copper) electrode and the titanium sulfate solution, and the negative compartment consists of iron electrode and acidic FeSO 4 solution. The anion ion exchange membrane is used as the diaphragm between two compartments. Fe 3+ in the titanium sulfate solution is reduced by the electric discharge of the primary cell. The effects of temperature, stirring strength of the solution and membrane area on the reduction rate have been investigated. The experimental result shows that the optimum current density can be higher than 100 A/m 2.
基金supported financially by the National Research Foundationthe support from the the Tshwane University of Technology, Pretoria, South Africa which helped to accomplish this work
文摘Titanium has found extensive use in various engineering applications due to its attractive physical,mechanical, and chemical characteristics. However, titanium has relatively low hardness for use as an armour material. ZrB2 was incorporated to the Ti matrix to form a Ti-based binary composites. In this study, powder metallurgy techniques were employed to disperse the ceramic particulates throughout the matrix material then consolidated through spark plasma sintering. The composites were densified at1300 ℃, pressure of 50 MPa, and holding time of 5 min. The microstructure and phase analysis of the sintered composites was carried out using SEM and XRD, while the hardness was determined using Vickers' microhardness tester. The SEM and XRD results confirmed the presence of the TiB whiskers which renowned with the improving the hardness of titanium. The hardness of the composite with 10 wt% ZrB_2 showed the highest hardness compared to that obtained for the 5 and 15 wt% ZrB_2 composites which was 495 and 571 Hv respectively.
基金work supported by the Second Stage of Brain Korea 21 Projects of Korea
文摘To determine mirror surface finishing conditions and efficient and economical superfinishing conditions for pure titanium and titanium alloys, an abrasive film is used when superfinishing is performed under varying conditions. These conditions include the workpiece rotation speed, the oscillation speed, the contact pressure of the roller, the hardness of the roller, and the type of abrasive film. The superfinishing device is applied to polishing a thin and long cylindrical bar. A micro-finishing film and a lapping film were used as abrasive films. A1203 grains or SiC grains were used as abrasives. The surface roughness of a polished workpiece was measured using a stylus-type surface-roughness measuring instrument. As a result, the conditions to improve the polishing surface efficiently include high values for the workpiece rotation speed, oscillation speed and contact pressure. The roller hardness has no effect on the efficient polishing conditions. The mirror finish of a surface can be created using lapping film of 3 μm with Al2O3 grains after polishing to a steady surface roughness under the efficient polishing conditions.
基金financially supported by National Natural Science Foundation of China with Grant No.11472054by the opening project of State Key Laboratory of Explosion Science and Technology(Beijing Institute of Technology) with Grant No. QNKT17-01
文摘Multilayer materials are widely used in military,automobile and aerospace industries.In this paper,the response of an explosion-welded Ti6Al4V/pure titanium with a flat interface to dynamic loading is investigated.An SHPB apparatus is used.Then,the dynamic behaviour of a bimetal sample is explored with a DIC system coupled to the SHPB.Result indicates that in the bimetal sample pure titanium is deformed and failed before Ti6Al4V.The stress curve of the sample shows two different peaks in a striker velocity higher than the 18.3 m/s.When the incident wave encounters the interface of the Ti6Al4V/pure titanium sample,only a small fraction of the wave is reflected owing to similar impedance.Using the direct interpretation stress-strain curve is unreasonable in this case because of unhomogenised plastic deformation.The micro structure of the sample is investigated after loading.An adiabatic shear band is formed in the pure titanium side before failure,and the interface of the sample remains intact under different loading conditions.The FEM simulation result for the sample is in good agreement with experimental observations.
文摘Ti/Fe clad plate had attracted extensive attention because of its important application. In order to reduce the titanium layer thickness, the explosive welding of TA1 titanium foil to Q235 steel plate was carried out. The interfacial bonding performance was analyzed by micromorphology analysis and mechanical property test, and the formation process of interfacial wave and molten block in the vortex was simulated by smoothed particle hydrodynamics(SPH) method. The results showed that salt as pressure transfer layer used in explosive welding could play a good buffer effect on the collision between flyer and base layers. Regular waveforms were formed on the bonding interface, and the titanium foil/steel clad plate exhibited good welding quality and bonding property. The crest of the observed interfacial wave moved 200 μm from the beginning to the final formation, and it was important of jet on the formation of interfacial waveform. The interface was mainly bonded in the form of molten layer, and the grains near the interface were streamlined. Molten block containing intermetallic compounds and metal oxides appeared in the vortex of wave crest.
基金Projects(51671152,51304153)supported by the National Natural Science Foundation of China
文摘The high-temperature acoustic absorption performance of porous titanium fiber material was investigated in terms of sample thickness, porosity, temperature, air-cavity thickness and double-layer structure arrangement. The effects on absorption coefficient were systematically assessed. The results show that the sound absorption performance is improved by increasing the sample porosity and/or thickness, and/or increasing the air-cavity thickness. Meanwhile, increasing the temperature gives better acoustic absorption performance in the low frequency range but also lowers the performance in the high frequency range, while double-layer structure enables better acoustic absorption performance.
文摘Titanium minerals are of interest because they constitute the most important source of titanium,a strategic metal in modem industry.However, knowledge on their structure,composition,and properties of nanodisperse structures has been limited. Several studies have shown that synthetic analogs of natural titanium oxides have structural features and physico-chemical properties distinctly different