CaGdAlO 4∶Yb^(3+)/Er^(3+)/Mn^(4+)荧光粉上转换发光及其双探针温度传感研究
1
作者 李玉强 杨健 +2 位作者 王帅 周恒为 刘玉学 《化工新型材料》 北大核心 2025年第2期187-192,共6页
过渡金属离子上转换发光是拓展稀土离子光谱范围的有效途径之一。使用高温固相法合成了Yb^(3+)/Er^(3+)/Mn^(4+)掺杂的CaGdAlO_(4)纯相荧光粉,在980nm激光激发下,CaGdAlO_(4)∶Yb_(0.1),Er_(0.01),Mn_(0.003)荧光粉的上转换发光性能最... 过渡金属离子上转换发光是拓展稀土离子光谱范围的有效途径之一。使用高温固相法合成了Yb^(3+)/Er^(3+)/Mn^(4+)掺杂的CaGdAlO_(4)纯相荧光粉,在980nm激光激发下,CaGdAlO_(4)∶Yb_(0.1),Er_(0.01),Mn_(0.003)荧光粉的上转换发光性能最优。室温发射谱图中,位于528、550、663和710nm处的发射峰分别归属于Er^(3+)的^(2)H_(11/2)→^(4)I_(15/2)、^(4)S_(3/2)→^(4)I_(15/2)、^(4)F_(9/2)→^(4)I_(15/2)和Mn^(4+)的^(2)E→^(4)A_(2)能级跃迁,均是双光子过程。300~573K变温实验表明,基于单一发光中心Er^(3+)荧光强度比FIR_(528/550)参数,相对灵敏度S_(R-528/550)从0.95×10^(-2)K^(-1)(300K)单调减小到0.27×10^(-2)K^(-1)(573K);基于Mn^(4+)-Er^(3+)双发光中心荧光强度比FIR_(710/663)参数,相对灵敏度S_(R-710/663)从0.37×10^(-2)K^(-1)(300K)先增大到2.08×10^(-2)K^(-1)(418K),随后减小为1.35×10^(-2)K^(-1)(573K)。当温度为420K时,S_(R-710/663)相比于S_(R-528/550)增大了近4倍。结果表明,CaGdAlO_(4)∶Yb 0.1,Er 0.01,Mn 0.003荧光粉在双探针光学温度传感领域具有潜在的应用价值。 展开更多
关键词 荧光粉 上转换 Mn^(4+) 荧光强度比 温度传感
在线阅读 下载PDF
Ca_(2)MgTeO_(6)∶Bi^(3+),Mn^(4+)材料的发光性能和温度探测 被引量:1
2
作者 祝冰心 朱肖 +5 位作者 王磊 时秋峰 郭海洁 乔建伟 崔彩娥 黄平 《发光学报》 EI CAS CSCD 北大核心 2024年第4期579-590,共12页
通过高温固相法成功制备了一系列Ca_(2)MgTeO_(6)∶Bi^(3+),Mn^(4+)荧光粉,对其微观结构、形貌、发光特性和温敏特性进行了表征。Ca_(2)MgTeO_(6)∶Bi^(3+),Mn^(4+)荧光粉具有不同温度敏感性的双发射中心,分别来自于Bi^(3+)离子^(3)P_(1... 通过高温固相法成功制备了一系列Ca_(2)MgTeO_(6)∶Bi^(3+),Mn^(4+)荧光粉,对其微观结构、形貌、发光特性和温敏特性进行了表征。Ca_(2)MgTeO_(6)∶Bi^(3+),Mn^(4+)荧光粉具有不同温度敏感性的双发射中心,分别来自于Bi^(3+)离子^(3)P_(1)→^(1)S_(0)跃迁和Mn^(4+)离子的^(2)E_(g)→^(4)A_(2g)跃迁。由于Bi^(3+)、Mn^(4+)离子的发光强度随温度变化的规律不同,利用该特性进行测温研究,在200~500 K范围内,该荧光粉的最大绝对灵敏度和相对灵敏度分别达到0.027 K^(-1)和1.83%·K^(-1),并且观察到荧光粉的发光颜色由橙黄色逐渐变为紫红色。实验结果表明,Ca_(2)MgTeO_(6)∶Bi^(3+),Mn^(4+)荧光粉作为光学测温材料在温度探测方面有一定的潜力。 展开更多
关键词 光学测温 荧光强度比 Bi^(3+) Mn^(4+) 温敏特性
在线阅读 下载PDF
主发射波长大于631 nm的Mn^(4+)激活氟化物荧光粉
3
作者 董效良 张明欣 +1 位作者 张丽莹 姬海鹏 《发光学报》 EI CAS CSCD 北大核心 2024年第10期1613-1621,共9页
利用比目前商用Mn^(4+)激活氟化物红粉主发射波长更长的红粉封装所得白光LED为背光源的液晶显示可以实现更广的显色色域。本文对已报道的主发射波长较长(632~637 nm)的Mn^(4+)激活氟化物红粉进行总结,并对其发射波长如何受被取代离子价... 利用比目前商用Mn^(4+)激活氟化物红粉主发射波长更长的红粉封装所得白光LED为背光源的液晶显示可以实现更广的显色色域。本文对已报道的主发射波长较长(632~637 nm)的Mn^(4+)激活氟化物红粉进行总结,并对其发射波长如何受被取代离子价态与半径、所形成八面体畸变程度、邻位阳离子的极化力等因素的影响进行了讨论。 展开更多
关键词 Mn^(4+) 红光荧光粉 氟化物 长发射波长
在线阅读 下载PDF
Al_(2)O_(3)表面包覆增强K_(2)SiF_(6)∶Mn^(4+)荧光粉发光性能和湿热稳定性
4
作者 段凌岳 路万兵 +4 位作者 王智逾 赵金鑫 王大伟 刘海旭 于威 《发光学报》 EI CAS CSCD 北大核心 2024年第3期443-449,共7页
研究了粉末原子层沉积技术(ALD)在白光LED用K_(2)SiF_(6)∶Mn^(4+)(KSFM)红色荧光粉包覆和表面改性中的应用,以及对其结构特性、发光性能和湿热环境中稳定性的影响。结果表明,采用ALD技术以三甲基铝作为前驱体、臭氧作为氧化剂,可以在K... 研究了粉末原子层沉积技术(ALD)在白光LED用K_(2)SiF_(6)∶Mn^(4+)(KSFM)红色荧光粉包覆和表面改性中的应用,以及对其结构特性、发光性能和湿热环境中稳定性的影响。结果表明,采用ALD技术以三甲基铝作为前驱体、臭氧作为氧化剂,可以在KSFM表面形成氧化铝包覆层。X射线衍射、表面形貌分析表明,ALD处理过程不会影响KSFM荧光粉的晶相和形貌特征。发光光谱分析表明,由于氧化铝钝化特性还会增强KSFM荧光粉的发光强度,并且不改变其发光波长。相较于未经包覆的KSFM荧光粉,包覆层可以显著改善KSFM粉末的湿热环境稳定性,ALD包覆后样品的相对发光强度在85%湿度/85℃环境中老化处理24 h后仍能保持初始值的84%。 展开更多
关键词 K_(2)SiF_(6)∶Mn^(4+) 红色荧光粉 表面改性 原子层沉积 湿热稳定性
在线阅读 下载PDF
K_(2)TiF_(6)∶Mn^(4+)窄带红色荧光粉的制备及其光学性能研究
5
作者 王晓 赵豫洁 李全安 《化工新型材料》 北大核心 2025年第1期131-135,143,共6页
在共沉淀和阳离子交换法的基础上,采用无氢氟酸液相法制备了K_2TiF_6∶Mn^(4+)窄带红色荧光粉,研究了氟化铵与硫酸(NH_(4)F+H_(2)SO_(4))用量以及Mn^(4+)掺杂量对样品结构形貌和发光性能的影响,将K_2TiF_6∶Mn^(4+)与商用Y_3Al_5O_(12)... 在共沉淀和阳离子交换法的基础上,采用无氢氟酸液相法制备了K_2TiF_6∶Mn^(4+)窄带红色荧光粉,研究了氟化铵与硫酸(NH_(4)F+H_(2)SO_(4))用量以及Mn^(4+)掺杂量对样品结构形貌和发光性能的影响,将K_2TiF_6∶Mn^(4+)与商用Y_3Al_5O_(12)∶Ce^(3+)荧光粉及氮化铟镓(InGaN)蓝光芯片组合封装出白光发光二极管(WLED)器件。结果表明,制备的K_2TiF_6∶Mn^(4+)红色荧光粉在~360nm和~465nm附近对紫外光和蓝光具有强烈的吸收,在600~650nm范围呈现出尖锐的发射峰。荧光粉的发光强度随着NH_(4)F+H_(2)SO_(4)用量的增加先增强后降低,当Mn^(4+)掺杂量为10%(摩尔分数,下同)时样品表现出浓度猝灭效应。在NH_(4)F和H_(2)SO_(4)用量均为60mmol,Mn^(4+)掺杂量为8%条件下,制备的荧光粉量子效率达到67%,用其封装的WLED器件显色指数为79.4,流明效率为80.62lm/W。 展开更多
关键词 Mn^(4+)掺杂 氟化物 红色荧光粉 白光发光二极管
在线阅读 下载PDF
Mn^(2+)掺杂对YAG∶Ce^(3+)荧光陶瓷发光性能的影响
6
作者 喻彬 孙炳恒 +7 位作者 付秀梅 周世斌 郝好莹 沈方樑 范金太 姜本学 张龙 孙军 《发光学报》 EI CAS CSCD 北大核心 2024年第5期762-771,共10页
过渡族金属Mn^(2+)掺杂的石榴石荧光陶瓷被认为是实现高显色激光照明的候选材料。然而,由于Mn^(2+)在不同配位环境下离子半径的多样性,Mn^(2+)掺杂石榴石陶瓷体系设计方案尚不明确。本文采用真空烧结技术制备得到不同浓度Mn^(2+)掺杂的... 过渡族金属Mn^(2+)掺杂的石榴石荧光陶瓷被认为是实现高显色激光照明的候选材料。然而,由于Mn^(2+)在不同配位环境下离子半径的多样性,Mn^(2+)掺杂石榴石陶瓷体系设计方案尚不明确。本文采用真空烧结技术制备得到不同浓度Mn^(2+)掺杂的YAG∶Ce^(3+)荧光陶瓷,并将Mn^(2+)分别设计进入八面体(OC)和十二面体(DO)格位。通过表征样品物相和显微结构、光致发光、荧光寿命、量子效率等,并通过LD激光器激发对荧光陶瓷的发光性能进行研究。实验结果表明,在添加电荷与体积补偿剂SiO_(2)的前提下,相比Mn^(2+)进入十二面体格位,Mn^(2+)进入八面体后石榴石的晶体结构更加稳定。因此,当Mn^(2+)的浓度控制在0.5%^(6)%(at)范围内,OC系列样品的量子效率高于DO系列样品。此外,OC系列样品的PL谱中位于588 nm和725 nm处的发射峰分别对应于Mn^(2+)占据八面体和十二面体格位的^(4)T_(1)→^(6)A_(1)电子跃迁,而DO系列样品中位于572 nm处的发射峰则源于Mn^(2+)占据扭曲的十二面体格位产生的电子跃迁。得益于Ce^(3+)→Mn^(2+)间高效的能量传递,将浓度为6%(at)的Mn^(2+)设计进入YAG∶Ce^(3+)中八面体格位制得荧光陶瓷,封装得到的激光白光光源的显色指数为70.8,相对色温为5117 K。本文对于Mn^(2+)掺杂的石榴石发光材料的开发研究是有力补充,也为提升YAG∶Ce^(3+)荧光陶瓷光谱中的红光成分,进而提高医疗、显示等领域的激光光源的显色性能提供借鉴。 展开更多
关键词 荧光陶瓷 Ce^(3+)掺杂 Mn^(2+)掺杂 格位
在线阅读 下载PDF
Mn^(2+)掺杂Cs_(3)Cu_(2)I_(5)微晶的温和、快速溶液法合成
7
作者 严鑫鑫 胡扬香 +2 位作者 万凝 庞起 陈旖勃 《发光学报》 EI CAS CSCD 北大核心 2024年第3期375-382,共8页
在铜基金属卤化物Cs_(3)Cu_(2)I_(5)中掺杂Mn^(2+)是拓宽发光范围的重要途径,但是已报道的掺杂方法大多需要高温、惰性气氛、较长时间和专用设备等。本工作将CsI固体粉末直接投加至CuI和MnCl_(2)的氢碘酸溶液中,在较低温度(60℃)、空气... 在铜基金属卤化物Cs_(3)Cu_(2)I_(5)中掺杂Mn^(2+)是拓宽发光范围的重要途径,但是已报道的掺杂方法大多需要高温、惰性气氛、较长时间和专用设备等。本工作将CsI固体粉末直接投加至CuI和MnCl_(2)的氢碘酸溶液中,在较低温度(60℃)、空气条件下快速(3 min)合成Mn^(2+)掺杂Cs_(3)Cu_(2)I_(5)微晶,并测试了其结构和发光性能。通过系列对比实验,提出一种由反应物溶解度控制的“缓释生长-掺杂”机制,证实CsI固体粉末在高浓度氢碘酸中的缓慢溶解能够降低Cs_(3)Cu_(2)I_(5)晶体的生长速率,为Mn^(2+)的低温、可控掺杂提供有利的动力学条件。该方法为全无机金属卤化物体系的掺杂发光和掺杂动力学研究提供了新的思路。 展开更多
关键词 Mn^(2+)掺杂 缓释生长-掺杂 Cs_(3)Cu_(2)I_(5)
在线阅读 下载PDF
葡萄糖-BrO_3^--Mn^(2+)-H_2SO_4-丙酮体系的振荡反应 被引量:15
8
作者 李和兴 刘敏 +2 位作者 王寿祥 许海涵 傅楚瑾 《物理化学学报》 SCIE CAS CSCD 北大核心 1990年第5期609-612,共4页
本文首次报道葡萄糖(以Glu表示)-丙酮(Act)-Mn^(2+)-BrO_3^--H_2SO_4体系的化学振荡反应,这种由糖类及丙酮作混和底物的均相B-Z振荡反应至今尚未见报道。实验部分1.试剂及药品:实验中各物质均采用分析纯,溶液在去离子水中配制。2.实验... 本文首次报道葡萄糖(以Glu表示)-丙酮(Act)-Mn^(2+)-BrO_3^--H_2SO_4体系的化学振荡反应,这种由糖类及丙酮作混和底物的均相B-Z振荡反应至今尚未见报道。实验部分1.试剂及药品:实验中各物质均采用分析纯,溶液在去离子水中配制。2.实验仪器及方法:实验在恒温30°±0.2℃下进行,以溴离子选择性电极和PXS-215型离子活度计测量电势(E)随时间(t)的变化来反映log[Br^-]的变化,以Hg|Hg_2SO_4|K_2SO_4为参比电极,振荡现象可通过XWT-台式自动平衡电位记录仪记录的E~t曲线观察,同时也可采用HP-8451A型紫外可见分光光度计,测定特定波长下吸光率的变化反映读物质浓度的变化,实验时溶液均匀搅拌。 展开更多
关键词 振荡反应 GLU BrO3^- MN^2+ 硫酸
在线阅读 下载PDF
红色长余辉材料Mg_2SiO_4∶Dy^(3+),Mn^(2+)的制备及发光特性 被引量:14
9
作者 林林 尹民 +2 位作者 施朝淑 张慰萍 徐美 《发光学报》 EI CAS CSCD 北大核心 2006年第3期331-336,共6页
用高温固相法制备了长余辉发光材料Mg2SiO4∶Dy3+,Mn2+,对这种材料的红色长余辉性质进行了研究。对以不同掺杂浓度单掺杂Mn2+、单掺杂Dy3+以及双掺杂Dy3+,Mn2+的Mg2SiO4体系,通过在紫外激发下的发射光谱及其激发光谱的研究,确认了在双... 用高温固相法制备了长余辉发光材料Mg2SiO4∶Dy3+,Mn2+,对这种材料的红色长余辉性质进行了研究。对以不同掺杂浓度单掺杂Mn2+、单掺杂Dy3+以及双掺杂Dy3+,Mn2+的Mg2SiO4体系,通过在紫外激发下的发射光谱及其激发光谱的研究,确认了在双掺杂体系中,峰值为660 nm的发光带对应着Mn2+的4T1(4G)→6A1(6S)跃迁,Mn2+为主要发光中心。Mn2+的660 nm发射的激发谱分布很宽,样品在近紫外和可见光区都有良好的吸收,长波边可达600 nm,是这种材料的一个显著优点。还研究了双掺杂体系中Dy3+对Mn2+的660 nm发光带的敏化作用。另外,通过对单掺杂、双掺杂体系热释光曲线的比较,揭示了双掺杂体系中Dy3+的陷阱作用。 展开更多
关键词 Mg2SiO4 DY^3+ MN^2+ 长余辉荧光粉 能量传递
在线阅读 下载PDF
Mn^(2+)、Ce^(3+)共掺杂Zn_2SiO_4材料的溶胶-凝胶法制备及光学性能研究 被引量:4
10
作者 徐光青 郑治祥 汤文明 《合肥工业大学学报(自然科学版)》 CAS CSCD 北大核心 2006年第4期427-430,共4页
采用溶胶-凝胶、化学掺杂方法制备了Mn2+、Ce3+离子掺杂Zn2SiO4材料;用X射线衍射仪、透射电子显微镜、吸收光谱仪以及荧光光谱仪对其结构、形貌和光致发光性能进行测试分析;结果表明,900℃热处理基本形成Zn2SiO4晶体,一次颗粒尺寸大约为... 采用溶胶-凝胶、化学掺杂方法制备了Mn2+、Ce3+离子掺杂Zn2SiO4材料;用X射线衍射仪、透射电子显微镜、吸收光谱仪以及荧光光谱仪对其结构、形貌和光致发光性能进行测试分析;结果表明,900℃热处理基本形成Zn2SiO4晶体,一次颗粒尺寸大约为200 nm左右;在空气中1 100℃和H2气氛中900℃热处理后,样品中存在2个发光峰:Mn2+产生的522 nm强绿光发射,Ce3+离子产生的398 nm弱紫光发射。 展开更多
关键词 光致发光 Ce^3+Mn^2+离子掺杂 溶胶-凝胶技术
在线阅读 下载PDF
Synthesis and Luminescence Improvement of CaAlSiN_(3) Phosphors Doped with Eu^(2+) and Mn^(2+) for White LEDs
11
作者 WEI Dong SU Wenxia 《发光学报》 EI CAS CSCD 北大核心 2024年第10期1656-1666,共11页
Eu^(2+) and Mn^(2+) co-activated CaAlSiN_(3) red phosphors were produced using the solid-state reaction tech⁃nique in a N2 environment.Excitation spectra,emission spectra,and diffuse reflection spectra were used to st... Eu^(2+) and Mn^(2+) co-activated CaAlSiN_(3) red phosphors were produced using the solid-state reaction tech⁃nique in a N2 environment.Excitation spectra,emission spectra,and diffuse reflection spectra were used to study the luminescence characteristics,energy gap,and thermal stability in detail.CaAlSiN_(3)∶Eu^(2+) exhibits an extended emission band when stimulated with 450 nm blue light,which is caused by the 4f65d to 4f7 transition of Eu^(2+).Similar⁃ly,CaAlSiN_(3)∶Mn^(2+) displays a wide emission band centered at 628 nm,which results from Mn^(2+)’s transition from 4T1(4G) to 6A1(6S).When the ions of Mn^(2+)were combined into CaAlSiN_(3)∶Eu^(2+),the photoluminescence intensity of Eu^(2+ )was greatly boosted because there was energy transfer and co-emission between Mn^(2+) and Eu^(2+).Beyond that,CaAlSiN_(3)∶Eu^(2+),Mn^(2+) emerges with splendid thermostability and high quantum efficiency,the quenching temperature surpasses 300℃,and the internal quantum efficiency is determined to be around 84.9%.The white LED was pack⁃aged with a combination of CaAlSiN_(3)∶Eu^(2+),Mn^(2+),LuAG∶Ce3+ and a blue chip.At a warm white-light corresponding color temperature(3009 K) with CIE coordinates(0.4223,0.3748),the color rendering index Ra has reached 93.2.CaAlSiN_(3)∶Eu^(2+),Mn^(2+) would have great application potential as a red-emitting phosphor for white LEDs. 展开更多
关键词 energy transfer silicon nitrides CaAlSiN_(3)∶Eu^(2+) Mn^(2+) red phosphor
在线阅读 下载PDF
植物生长LED用Sr_(2)MgAl_(22)O_(36)∶Mn^(4+)荧光玻璃的制备与发光性质 被引量:3
12
作者 杨茂林 郑俊丽 +2 位作者 余丽萍 廉世勋 周文理 《发光学报》 EI CAS CSCD 北大核心 2021年第5期717-723,共7页
采用两步烧结法低温制备了Sr_(2)MgAl_(22)O_(36)∶Mn^(4+)-(SiO_(2)-Al ^(2)O_(3)-ZnO-BaO)荧光玻璃(SMA∶Mn^(4+)-PiG)。通过X射线衍射、扫描电镜、光致激发和发射光谱、荧光衰减曲线等手段对其物相、成分与发光性能进行了研究。实验... 采用两步烧结法低温制备了Sr_(2)MgAl_(22)O_(36)∶Mn^(4+)-(SiO_(2)-Al ^(2)O_(3)-ZnO-BaO)荧光玻璃(SMA∶Mn^(4+)-PiG)。通过X射线衍射、扫描电镜、光致激发和发射光谱、荧光衰减曲线等手段对其物相、成分与发光性能进行了研究。实验结果表明,形成PiG后,SMA∶Mn^(4+)荧光粉的物相和元素组成保持不变。不同SAM∶Mn^(4+)含量的PiG样品在328 nm光激发下,在661 nm处均显示强的发射带,归属于荧光粉中Mn^(4+)的2E→4A 2跃迁,发光光谱与植物光敏色素的红区吸收光谱匹配良好。随着荧光粉含量的增加,SAM∶Mn^(4+)-PiG的发光强度逐渐增大。15%SMA∶Mn^(4+)-PiG样品的内、外量子效率分别为26%和20%,低于SMA∶Mn^(4+)荧光粉的59%和40%。相比于SMA∶Mn^(4+)荧光粉,荧光玻璃的吸收效率和热稳定性略有提高。通过与高功率紫外芯片封装,SMA∶Mn^(4+)-PiG红光LED器件在100 mA驱动电流下展现了最高的电致发光强度。 展开更多
关键词 荧光玻璃 植物生长 Mn^(4+) 发光二极管
在线阅读 下载PDF
小尺寸Mn^(4+) 掺杂氟化物制备方法的研究进展
13
作者 罗沛兰 罗志怀 +3 位作者 周志军 陈哲 何雪龙 张文华 《南昌工程学院学报》 CAS 2024年第1期102-106,共5页
Mn^(4+)掺杂氟化物荧光材料展现出众多优势,包括无毒、蓝光激发、超窄发射谱带、高发光效率、符合Rec.2020标准的发射波长、无重吸收以及优良的热稳定性。这些特点使其成为下一代Mini/Micro-LED显示技术的理想红光介质材料。然而,要应用... Mn^(4+)掺杂氟化物荧光材料展现出众多优势,包括无毒、蓝光激发、超窄发射谱带、高发光效率、符合Rec.2020标准的发射波长、无重吸收以及优良的热稳定性。这些特点使其成为下一代Mini/Micro-LED显示技术的理想红光介质材料。然而,要应用于Mini/Micro-LED,需要小尺寸的氟化物。因此,本文从制备方法入手,深入探讨了国内外小尺寸Mn^(4+)掺杂氟化物的研究现状。在此基础上,总结并提出当前小尺寸Mn^(4+)掺杂氟化物面临的关键问题,旨在为研发高效优质的小尺寸Mn^(4+)掺杂氟化物提供参考。 展开更多
关键词 Mn^(4+) Micro-LED 红色荧光粉 氟化物
在线阅读 下载PDF
基于单元共取代策略调控Mn^(4+)/Pb^(2+)掺杂LaAlO_(3)荧光材料的晶格环境与发光性能研究进展
14
作者 卢思瑜 李思远 朱琦 《发光学报》 EI CAS CSCD 北大核心 2023年第12期2188-2201,共14页
LaAlO_(3)属于典型的畸变钙钛矿结构,具有较低的声子能量、较宽的带隙和优异的结构稳定性,是一种优良的发光基质。Mn^(4+)和Pb^(2+)的发光性能与其所处的微观配位环境密切相关,可以通过调控晶格环境优化其发光性能。本文综述了调控Mn4+... LaAlO_(3)属于典型的畸变钙钛矿结构,具有较低的声子能量、较宽的带隙和优异的结构稳定性,是一种优良的发光基质。Mn^(4+)和Pb^(2+)的发光性能与其所处的微观配位环境密切相关,可以通过调控晶格环境优化其发光性能。本文综述了调控Mn4+的零声子线(Zero‐phonon line,ZPL)发射和Pb^(2+)的发光性能研究进展,系统探讨了单元共取代对晶体结构和Mn^(4+)、Pb^(2+)的发光性能的影响,详尽分析了激活离子的晶格环境与发光性能之间的构效关系。 展开更多
关键词 LaAlO_(3) Mn^(4+) Pb^(2+) 单元共取代
在线阅读 下载PDF
Mn^(4+)掺杂氟化物红色发光粒子的表面钝化和白色发光二极管应用 被引量:1
15
作者 杨晨 叶梦琳 周文理 《发光学报》 EI CAS CSCD 北大核心 2024年第2期299-307,共9页
Mn^(4+)掺杂的氟化物红色荧光粉的耐湿性差,严重影响了白色发光二极管(WLEDs)的光色稳定性。本工作基于绿矾溶液的还原性,将K_(2)SiF_(6)∶Mn^(4+)颗粒表面的Mn^(4+)还原成可溶的低价态Mn^(2+),实现了氟化物粒子的表面钝化及高耐湿性。... Mn^(4+)掺杂的氟化物红色荧光粉的耐湿性差,严重影响了白色发光二极管(WLEDs)的光色稳定性。本工作基于绿矾溶液的还原性,将K_(2)SiF_(6)∶Mn^(4+)颗粒表面的Mn^(4+)还原成可溶的低价态Mn^(2+),实现了氟化物粒子的表面钝化及高耐湿性。在水浸360 h后,表面钝化的K_(2)SiF_(6)∶Mn^(4+)粒子的发光强度仍保持初始强度的95%,而未处理的K_(2)SiF_(6):Mn^(4+)颗粒发光强度迅速降为初始值的46%。此外,采用绿矾溶液对表面已水解的氟化物荧光粉进行简单的浸泡,可使其完全恢复原来的发光强度。电感耦合等离子体-原子发射光谱、X射线光电子谱、元素能谱等表征结果显示,经绿矾溶液处理的K_(2)SiF_(6):Mn^(4+)粒子表面的Mn^(4+)浓度显著减小,证实了惰性壳层K_(2)SiF_(6)的形成,揭示了氟化物粒子耐湿性显著提升的原因。此外,经高温(85℃)高湿(85%)的条件老化1 000 h后,WLEDs器件中表面钝化的K_(2)SiF_(6)∶Mn^(4+)粒子仍保持着100%的红色发光强度,明显高于未钝化的氟化物的59%,进一步证实了绿矾溶液钝化的K_(2)SiF_(6)∶Mn^(4+)红色荧光粉具有非常优异的环境稳定性。 展开更多
关键词 Mn^(4+)掺杂 红色荧光粉 耐湿性 绿矾溶液 表面钝化
在线阅读 下载PDF
Mn^(3+)/Mn^(2+)间接电氧化法分解辉钼矿 被引量:7
16
作者 符剑刚 钟宏 +1 位作者 黄永平 卜向明 《中南大学学报(自然科学版)》 EI CAS CSCD 北大核心 2004年第5期797-801,共5页
采用Mn3+/Mn2+间接电氧化法湿法分解辉钼矿。在强酸介质中,媒介Mn3+/Mn2+氧化能力很强,能将MoS2氧化分解为MoO3和硫酸,且锰离子可以循环利用。探讨了Mn3+/Mn2+间接电氧化法的工艺条件,结果表明:在H2SO4浓度为7mol/L,MnSO4浓度为0.5mol/L... 采用Mn3+/Mn2+间接电氧化法湿法分解辉钼矿。在强酸介质中,媒介Mn3+/Mn2+氧化能力很强,能将MoS2氧化分解为MoO3和硫酸,且锰离子可以循环利用。探讨了Mn3+/Mn2+间接电氧化法的工艺条件,结果表明:在H2SO4浓度为7mol/L,MnSO4浓度为0.5mol/L,电解电量为20A·h·g-1,电极间距15mm,阳极电流密度为800A·m-2,矿浆液固比为40,温度为55℃的条件下,钼的浸出率为88.5%。此外,对氧化浸出过程采用了超声波外场强化,Mo浸出率可以提高到92.3%。 展开更多
关键词 间接电氧化 辉钼矿 Mn^3+/Mn^2+ 超声波 浸出
在线阅读 下载PDF
Tb^(3+),Mn^(2+)作为激活剂的PDP绿色荧光粉的研究 被引量:5
17
作者 陶怡 李岚 +3 位作者 王达健 张晓松 张纳 李光旻 《液晶与显示》 CAS CSCD 北大核心 2005年第4期296-301,共6页
分别介绍了以Mn2+和Tb3+作为激活中心的PDP用硅酸盐体系、铝酸盐体系、硼酸盐体系和磷酸盐等体系绿色荧光粉的研究现状。在以Mn2+作为发光中心的绿粉中,目前研究主要集中在通过调整Mn2+的离子浓度、添加其他杂质,探索使用新的基质材料,... 分别介绍了以Mn2+和Tb3+作为激活中心的PDP用硅酸盐体系、铝酸盐体系、硼酸盐体系和磷酸盐等体系绿色荧光粉的研究现状。在以Mn2+作为发光中心的绿粉中,目前研究主要集中在通过调整Mn2+的离子浓度、添加其他杂质,探索使用新的基质材料,或是使用不同的合成技术等方法来改进其余辉时间过长、易时效劣化以及形貌上的不足。在以Tb3+作为激活中心的绿粉中,为了获取在真空紫外激发条件下高的发光效率,则主要围绕寻找在VUV区域内有强吸收的基质和能够有效进行能量传递的稀土敏化剂,以及利用量子剪裁效应来使得荧光粉发光量子效率大于1等方面进行。 展开更多
关键词 PDP TB^3+ MN^2+ 荧光粉 能量传递 量子剪裁
在线阅读 下载PDF
(Ba,Mg,Sr)O·nAl_2O_3∶Mn^(2+)的合成及发光性质研究 被引量:3
18
作者 沈雷军 张忠义 +4 位作者 韩莉 周永勃 刘翠兰 陶冶 巨新 《发光学报》 EI CAS CSCD 北大核心 2003年第2期189-193,共5页
用高温固相反应合成了Ba0 04Mg0 16Sr0 8O·nAl2O3∶Mn2+0 07(n=4 1,4 2…4 9)和Ba0 1Mg0 1Sr0 8O·nAl2O3∶Mn2+0 07(n=4 1,4 2…4 9)铝酸盐体系发光材料。X射线衍射呈单相,说明生成了完全互溶的连续固溶体。经检测发现Mg2+,S... 用高温固相反应合成了Ba0 04Mg0 16Sr0 8O·nAl2O3∶Mn2+0 07(n=4 1,4 2…4 9)和Ba0 1Mg0 1Sr0 8O·nAl2O3∶Mn2+0 07(n=4 1,4 2…4 9)铝酸盐体系发光材料。X射线衍射呈单相,说明生成了完全互溶的连续固溶体。经检测发现Mg2+,Sr2+的引入有效地优化了发光基质,使Mn2+在真空紫外激发下的发射明显增强。在Ba0 04Mg0 16Sr0 8O·nAl2O3∶Mn2+0 07体系中,在一定范围内改变Al3+含量(n值)可适当调整激发光谱峰位;适当调整Al3+和Mn2+的含量比可以改变体系的发光强度,以满足等离子平板显示(PDP)技术的需求。 展开更多
关键词 高温固相反应 (Ba Mg Sr)O·nAl2O3:Mn^2+ 合成 发光性质 铝酸盐体系发光材料
在线阅读 下载PDF
红外光谱法研究胡敏酸与Fe^3+、Al^3+、Mn^2+金属离子配位机理 被引量:4
19
作者 王强 魏世强 黄玉明 《土壤学报》 CAS CSCD 北大核心 2008年第2期366-369,共4页
关键词 胡敏酸 Fe^3+、Al^3+、Mn^2+金属离子 红外光谱 反应机理
在线阅读 下载PDF
以衣康酸-BrO_3^--Mn^(2+)为体系的化学振荡研究 被引量:3
20
作者 卢峰 许海涵 《物理化学学报》 SCIE CAS CSCD 北大核心 1989年第3期310-315,共6页
本文研究了BrO_3^--Br^--H^+-Mn^(2+)-衣康酸体系的振荡行为,利用电位法及分光光度计对体系做了一系列测定,根据FKN机理,提出了本体系可能的反应进程,同时测定了各种反应条件对振荡的诱导期及周期影响,并根据机理分析把诱导期分成两个部... 本文研究了BrO_3^--Br^--H^+-Mn^(2+)-衣康酸体系的振荡行为,利用电位法及分光光度计对体系做了一系列测定,根据FKN机理,提出了本体系可能的反应进程,同时测定了各种反应条件对振荡的诱导期及周期影响,并根据机理分析把诱导期分成两个部分,得到1/τ_(i1),1/τ_(i2),1/τ_p对各种反应物起始浓度的关系式。还发观葡萄糖能促进振荡进行。 展开更多
关键词 衣康酸 BrO3 MN^2+ 振荡反应
在线阅读 下载PDF