To develop suitable grouting materials for water conveyance tunnels in cold regions,firstly,this study investigated the performance evolution of ferrite-rich sulfoaluminate-based composite cement(FSAC grouting materia...To develop suitable grouting materials for water conveyance tunnels in cold regions,firstly,this study investigated the performance evolution of ferrite-rich sulfoaluminate-based composite cement(FSAC grouting material)at 20 and 3℃.The results show that low temperature only delays the strength development of FSAC grouting material within the first 3 d.Then,the effect of four typical early strength synergists on the early properties of FSAC grouting material was evaluated to optimize the early(£1 d)strength at 3℃.The most effective synergist,Ca(HCOO)_(2),which enhances the low-temperature early strength without compromising fluidity was selected based on strength and fluidity tests.Its micro-mechanism was analyzed by XRD,TG,and SEM methods.The results reveal that the most suitable dosage range is 0.3 wt%−0.5 wt%.Proper addition of Ca(HCOO)_(2)changed the crystal morphology of the hydration products,decreased the pore size and formed more compact hydration products by interlocking and overlapping.However,excessive addition of Ca(HCOO)_(2)inhibited the hydration reaction,resulting in a simple and loose structure of the hydration products.The research results have reference value for controlling surrounding rock deformation and preventing water and mud inrushes during the excavation in cold region tunnels.展开更多
A series of researches were carried out for the soil samples in the Pearl River Delta under the action of consolidation loads,such as the quantitative analyses of the pore scale,shape and size distributions of micro-s...A series of researches were carried out for the soil samples in the Pearl River Delta under the action of consolidation loads,such as the quantitative analyses of the pore scale,shape and size distributions of micro-structure units,with an environmental scanning electron microscope (ESEM),a mercury intrusion analyzer and a mineral diffractometer. The experimental results show that the consolidation pressures remarkably change the pore sizes and distribution characteristics of the silt,thus changing its compressibility and permeability. This can be proved by the fact that,in the earlier stage with a consolidation pressure of p<200 kPa,the pore sizes are greater and the compressibility and permeability coefficients are larger. However,they rapidly decrease with the increase in consolidation pressure. And in the later stage with a consolidation pressure of p>200 kPa,the pore sizes are smaller and the compressibility and permeability coefficients are less. Therefore,the empirical formulas of compression coefficient and permeability coefficient vs consolidation load and average pore diameter are deduced.展开更多
基金Projcet(52279119)supported by the National Natural Science Foundation of ChinaProject(XZ202201ZY0021G)supported by the Science and Technology Planning Project of Xizang Autonomous Region,China+1 种基金Project(2019QZKK0904)supported by the Second Xizang Plateau Scientific Expedition and Research Program of ChinaProject(51922104)supported by the National Natural Science Foundation for Distinguished Young Scholars of China。
文摘To develop suitable grouting materials for water conveyance tunnels in cold regions,firstly,this study investigated the performance evolution of ferrite-rich sulfoaluminate-based composite cement(FSAC grouting material)at 20 and 3℃.The results show that low temperature only delays the strength development of FSAC grouting material within the first 3 d.Then,the effect of four typical early strength synergists on the early properties of FSAC grouting material was evaluated to optimize the early(£1 d)strength at 3℃.The most effective synergist,Ca(HCOO)_(2),which enhances the low-temperature early strength without compromising fluidity was selected based on strength and fluidity tests.Its micro-mechanism was analyzed by XRD,TG,and SEM methods.The results reveal that the most suitable dosage range is 0.3 wt%−0.5 wt%.Proper addition of Ca(HCOO)_(2)changed the crystal morphology of the hydration products,decreased the pore size and formed more compact hydration products by interlocking and overlapping.However,excessive addition of Ca(HCOO)_(2)inhibited the hydration reaction,resulting in a simple and loose structure of the hydration products.The research results have reference value for controlling surrounding rock deformation and preventing water and mud inrushes during the excavation in cold region tunnels.
基金Project(2008ZA11) supported by State Key Laboratory of Subtropical Building Science in South China University of Technology, ChinaProject(20080430815) supported by China Postdoctoral Science Foundation
文摘A series of researches were carried out for the soil samples in the Pearl River Delta under the action of consolidation loads,such as the quantitative analyses of the pore scale,shape and size distributions of micro-structure units,with an environmental scanning electron microscope (ESEM),a mercury intrusion analyzer and a mineral diffractometer. The experimental results show that the consolidation pressures remarkably change the pore sizes and distribution characteristics of the silt,thus changing its compressibility and permeability. This can be proved by the fact that,in the earlier stage with a consolidation pressure of p<200 kPa,the pore sizes are greater and the compressibility and permeability coefficients are larger. However,they rapidly decrease with the increase in consolidation pressure. And in the later stage with a consolidation pressure of p>200 kPa,the pore sizes are smaller and the compressibility and permeability coefficients are less. Therefore,the empirical formulas of compression coefficient and permeability coefficient vs consolidation load and average pore diameter are deduced.