Adding polypropylene(PP)fibers and coarse aggregates has become a popular way to enhance the strength and stability of the cemented tailings backfilling(CTB)body.It is essential to explore the influence of tailings-ag...Adding polypropylene(PP)fibers and coarse aggregates has become a popular way to enhance the strength and stability of the cemented tailings backfilling(CTB)body.It is essential to explore the influence of tailings-aggregate ratio and fiber content on the mechanical properties of CTB samples.The comprehensive tests of the unconfined compressive strength(UCS),slump and microstructure were designed,and the regression models were established to characterize the effect of the strength,ductility and fluidity.The results indicate that the tailings-aggregate ratio of 5:5 and PP fiber content of 0.5 kg/m^(3) are the optimum point considering the UCS,cracking strain,peak strain and post-peak ductility.The tailings-aggregate ratio is consistent with the unary quadratic to the UCS and a linear model with a negative slope to the slump.Microstructural analysis indicates that PP fiber tends to bridge the cracks and rod-mill sand to serve as the skeleton of the paste matrix,which can enhance the compactness and improve the ductility of the CTB.The results presented here are of great significance to the understanding and application of coarse aggregates and fibers to improve the mechanical properties of CTB.展开更多
Through adding different additional water use,the compressive strength,splitting tensile strength and fluidity of recycled concrete of three aggregate combination forms were studied by experiment respectively.The expe...Through adding different additional water use,the compressive strength,splitting tensile strength and fluidity of recycled concrete of three aggregate combination forms were studied by experiment respectively.The experimental results show that with the increase of adding additional water use,the compressive strength and splitting tensile strength of recycled coarse aggregate concrete decrease,but that of recycled fine aggregate concrete and recycled all aggregate concrete increase firstly then decrease.When additional water use is added more 15% or 20% than that of basic ordinary concrete,the recycled coarse aggregate concrete and fine one can get pretty good fluidity.When it is added more 30%,the recycled all aggregate concrete has fluidity that is just satisfied.展开更多
The high-flowing sand-concrete (HFSC) containing natural sands as aggregate was carried out. The high fluidity and stability of HFSC can be achieved by tailoring the mix design parameters, such as fine to coarse san...The high-flowing sand-concrete (HFSC) containing natural sands as aggregate was carried out. The high fluidity and stability of HFSC can be achieved by tailoring the mix design parameters, such as fine to coarse sand ratio, dosage of additions, water to binder ratio and dosage of admixtures. Mini-cone slump test, v-fl.mnel time test and viscosity model parameters were used to characterize the behaviour of HFSC in fresh state. The mechanical compressive strength in 28 d was also determined. A factorial design approach was used to establish models highlighting the effect of each mix-parameter on measured properties of HFSC. The derived models are valid for mixtures made with 0 to 0.3 of dune sand to total sand ratio, 82 to 418 kg/m3 of marble powder, 0.42 to 0.46 of water/binder ratio and 1.3% to 1.9% of superplasticizer high water-reducer. The results show that the derived models constitute very efficient means for understanding the influence of key mix-parameters on HFSC properties and are useful in selecting the optimum mix proportions, by simulating their impact on fluidity, stability and compressive strength.展开更多
Gum arabic, an inexpensive dispersant widely used in the food industry, has great potential for application in building materials. In order to find out the dispersion effect of gum arabic and the factors influencing t...Gum arabic, an inexpensive dispersant widely used in the food industry, has great potential for application in building materials. In order to find out the dispersion effect of gum arabic and the factors influencing the holding capacity of gum arabic in cement during hydration, rheological properties of cement paste with added gum arabic were assessed in this paper. The results show that 0.10wt%-0.60wt% of gum arabic positively affects dispersion, lower dosages have negligible effect. High speed mixing is required to maintain the dispersion stability of gum arabic in cement paste. The optimum dosage of gum arabic to achieve best disperse-holding capacity of cement paste was 0.3wt%, and the minimum water-cement ratio needed to obtain a dispersion effect was 0.28.展开更多
In the present paper,the fundamental research on the properties of boron-rich slag melting separated from boron-bearing iron concentrate was performed.The melting and fluidity of B2O3–MgO–SiO2–FeO slag system,cryst...In the present paper,the fundamental research on the properties of boron-rich slag melting separated from boron-bearing iron concentrate was performed.The melting and fluidity of B2O3–MgO–SiO2–FeO slag system,crystallization of separated boron-rich slag and factors on the extraction efficiency of boron-rich slag were systematically investigated.B2O3 content would heavily affect the melting and fluidity property of boron-rich slag.Generally,FeO could improve the melting and fluidity property of boron-rich slag.Boron-containing crystalline phase mainly precipitated in temperature range from 1200°C to 1100°C.Higher smelting temperature and B2O3 reduction ratio were negative for the extraction of boron.The cooling rate of 10–20°C/min was better for the crystallization of boron-containing crystalline phase.Based on the obtained experimental results,the optimum operating parameters for the development of pyrometallurgical boron and iron separation process and further boron-rich slag cooling process were proposed.展开更多
基金Project(51722401)supported by the National Science Foundation for Excellent Young Scholars of ChinaProject(51334001)supported by the Key Program of National Natural Science Foundation of ChinaProject(FRF-TP-18-003C1)supported by the Fundamental Research Funds for the Central Universities,China。
文摘Adding polypropylene(PP)fibers and coarse aggregates has become a popular way to enhance the strength and stability of the cemented tailings backfilling(CTB)body.It is essential to explore the influence of tailings-aggregate ratio and fiber content on the mechanical properties of CTB samples.The comprehensive tests of the unconfined compressive strength(UCS),slump and microstructure were designed,and the regression models were established to characterize the effect of the strength,ductility and fluidity.The results indicate that the tailings-aggregate ratio of 5:5 and PP fiber content of 0.5 kg/m^(3) are the optimum point considering the UCS,cracking strain,peak strain and post-peak ductility.The tailings-aggregate ratio is consistent with the unary quadratic to the UCS and a linear model with a negative slope to the slump.Microstructural analysis indicates that PP fiber tends to bridge the cracks and rod-mill sand to serve as the skeleton of the paste matrix,which can enhance the compactness and improve the ductility of the CTB.The results presented here are of great significance to the understanding and application of coarse aggregates and fibers to improve the mechanical properties of CTB.
基金Project(Xiangjianke(2007)No.425) supported by Scientific Research Fund of Hunan Provincial Construction DepartmentProject supported by the Youth Framework Teacher Fund of Xiangtan University(2006)
文摘Through adding different additional water use,the compressive strength,splitting tensile strength and fluidity of recycled concrete of three aggregate combination forms were studied by experiment respectively.The experimental results show that with the increase of adding additional water use,the compressive strength and splitting tensile strength of recycled coarse aggregate concrete decrease,but that of recycled fine aggregate concrete and recycled all aggregate concrete increase firstly then decrease.When additional water use is added more 15% or 20% than that of basic ordinary concrete,the recycled coarse aggregate concrete and fine one can get pretty good fluidity.When it is added more 30%,the recycled all aggregate concrete has fluidity that is just satisfied.
文摘The high-flowing sand-concrete (HFSC) containing natural sands as aggregate was carried out. The high fluidity and stability of HFSC can be achieved by tailoring the mix design parameters, such as fine to coarse sand ratio, dosage of additions, water to binder ratio and dosage of admixtures. Mini-cone slump test, v-fl.mnel time test and viscosity model parameters were used to characterize the behaviour of HFSC in fresh state. The mechanical compressive strength in 28 d was also determined. A factorial design approach was used to establish models highlighting the effect of each mix-parameter on measured properties of HFSC. The derived models are valid for mixtures made with 0 to 0.3 of dune sand to total sand ratio, 82 to 418 kg/m3 of marble powder, 0.42 to 0.46 of water/binder ratio and 1.3% to 1.9% of superplasticizer high water-reducer. The results show that the derived models constitute very efficient means for understanding the influence of key mix-parameters on HFSC properties and are useful in selecting the optimum mix proportions, by simulating their impact on fluidity, stability and compressive strength.
文摘Gum arabic, an inexpensive dispersant widely used in the food industry, has great potential for application in building materials. In order to find out the dispersion effect of gum arabic and the factors influencing the holding capacity of gum arabic in cement during hydration, rheological properties of cement paste with added gum arabic were assessed in this paper. The results show that 0.10wt%-0.60wt% of gum arabic positively affects dispersion, lower dosages have negligible effect. High speed mixing is required to maintain the dispersion stability of gum arabic in cement paste. The optimum dosage of gum arabic to achieve best disperse-holding capacity of cement paste was 0.3wt%, and the minimum water-cement ratio needed to obtain a dispersion effect was 0.28.
基金Project(FRF-TP-16-019A1)supported by the Fundamental Research Funds for the Central Universities,ChinaProject(51274033)supported by the National Natural Science Foundation of China
文摘In the present paper,the fundamental research on the properties of boron-rich slag melting separated from boron-bearing iron concentrate was performed.The melting and fluidity of B2O3–MgO–SiO2–FeO slag system,crystallization of separated boron-rich slag and factors on the extraction efficiency of boron-rich slag were systematically investigated.B2O3 content would heavily affect the melting and fluidity property of boron-rich slag.Generally,FeO could improve the melting and fluidity property of boron-rich slag.Boron-containing crystalline phase mainly precipitated in temperature range from 1200°C to 1100°C.Higher smelting temperature and B2O3 reduction ratio were negative for the extraction of boron.The cooling rate of 10–20°C/min was better for the crystallization of boron-containing crystalline phase.Based on the obtained experimental results,the optimum operating parameters for the development of pyrometallurgical boron and iron separation process and further boron-rich slag cooling process were proposed.