DP780冷轧热镀锌钢板点焊接头的高速拉伸性能 被引量:1
1
作者 王威 张永强 +2 位作者 徐兴智 尚永辉 李珊珊 《机械工程材料》 CSCD 北大核心 2017年第10期74-76,81,共4页
利用拉伸试验设备对1.2mm厚DP780冷轧热镀锌钢板点焊接头分别进行了准静态拉伸和高速拉伸试验,分析了点焊接头的高速拉伸特性,并与母材的进行了对比。结果表明:在准静态拉伸和高速拉伸时,点焊接头试样分别在一侧母材和过渡弧处发生断裂... 利用拉伸试验设备对1.2mm厚DP780冷轧热镀锌钢板点焊接头分别进行了准静态拉伸和高速拉伸试验,分析了点焊接头的高速拉伸特性,并与母材的进行了对比。结果表明:在准静态拉伸和高速拉伸时,点焊接头试样分别在一侧母材和过渡弧处发生断裂;准静态拉伸时的最大拉伸力为9.90kN,随着应变速率的增大,最大拉伸力逐渐增大,在应变速率为500s^(-1)时达到11.50kN;当应变为0.20~0.25时,点焊接头发生断裂失效,而此时仍处于母材的安全有效区间内。 展开更多
关键词 应变速率 dp780冷轧 点焊接头 拉伸性能
在线阅读 下载PDF
Effect of laser power on microstructure and mechanical properties of laser heat conduction lap welded joint between AZ31B magnesium alloy and DP780 galvanized steel 被引量:3
2
作者 GAO Ju-ming WANG Dan +2 位作者 ZHUANG Dong-dong ZHAO Xin-yi LEI Yu-cheng 《Journal of Central South University》 SCIE EI CAS CSCD 2022年第10期3463-3475,共13页
In this work, laser heat conduction lap welding(LHCLW) of AZ31B magnesium alloy sheet and DP780galvanized steel sheet was carried out by the defocused laser beam. The effects of laser power on the microstructure and m... In this work, laser heat conduction lap welding(LHCLW) of AZ31B magnesium alloy sheet and DP780galvanized steel sheet was carried out by the defocused laser beam. The effects of laser power on the microstructure and mechanical properties of the joint were studied. The pros and cons of the joint were identified and evaluated by measuring the tensile shear strength, microhardness and microstructure observation. The formation mechanism of various phases at the Mg/steel interface was analyzed. The results indicated that the galvanized layer could promote the metallurgical bonding between magnesium alloy and steel by improving the diffusion ability of molten magnesium alloy at the steel interface and reacting with Mg, so as to enhance the strength of the joint. A continuous dense layered eutectic structure(α-Mg+MgZn) was formed at the interface of the joint, while MgZn_(2)and MgZn phase was formed at the weld edge zone and heat affective zone(HAZ), whereas no reaction layer was generated between the uncoated steel and magnesium alloy. A sound joint could be obtained at 2.5 kW, and the corresponding tensile shear strength reached the maximum value of 42.9 N/mm. The strength was slightly reduced at 2.6 kW due to the existence of microcracks in the eutectic reaction layer. 展开更多
关键词 AZ31B magnesium alloy dp780 galvanized steel laser heat conduction lap welding laser power microstructure mechanical properties
在线阅读 下载PDF