Fabrication of RDX Based Composites via Water Flotation and Monometallic Polydopamine Coatings
1
作者 LI Xiao QIN Liang +5 位作者 XU Jian-xin ZHANG Lu-yao SHEN Jin-jie LAN Guan-chao WANG Jian-long CHEN Li-zhen 《火炸药学报》 北大核心 2025年第8期763-769,I0004,共8页
To enhance the overall performance of cyclotrimethylenetrinitramine(RDX),a modification strategy for RDX via in situ coordination with monometallic polydopamine(PDA)coatings(PDA-Fe,PDA-Cu,and PDA-Pb)was developed.The ... To enhance the overall performance of cyclotrimethylenetrinitramine(RDX),a modification strategy for RDX via in situ coordination with monometallic polydopamine(PDA)coatings(PDA-Fe,PDA-Cu,and PDA-Pb)was developed.The thermal properties of pristine RDX and its modified variants(RDX@PDA-Fe,RDX@PDA-Cu,RDX@PDA-Pb)were characterized using differential scanning calorimetry(DSC)and accelerating rate calorimetry(ARC).The impact sensitivity of these materials was evaluated via the characteristic drop-height method.The results demonstrate that PDA-metal metal coatings—formed through coordination between PDA and single metal ions(Fe^(3+),Cu^(2+),or Pb^(2+))—significantly enhance RDX′s thermal stability while attenuating its mechanical sensitivity.These coatings act as energy-absorbing barriers against external stimuli,effectively mitigating RDX′s sensitivity.Furthermore,they elevate RDX′s thermal stability by increasing its decomposition onset temperature and accelerating its decomposition kinetics.The monometallic coatings also catalyze RDX′s thermal decomposition and combustion,with Cu and Pb exhibiting particularly distinct catalytic effects. 展开更多
关键词 physical chemistry RDX situ coordination compositeS catalytic mechanic
在线阅读 下载PDF
Evolution of the volume expansion of SiO/C composite electrodes in lithium-ion batteries during aging cycles
2
作者 Haosong Yang Kai Sun +2 位作者 Xueyan Li Peng Tan Lili Gong 《中国科学技术大学学报》 北大核心 2025年第2期27-33,26,I0001,共9页
As a negative electrode material for lithium-ion batteries,silicon monoxide(SiO)suffers from dramatic volume changes during cycling,causing excessive stress within the electrode and resulting in electrode deformation ... As a negative electrode material for lithium-ion batteries,silicon monoxide(SiO)suffers from dramatic volume changes during cycling,causing excessive stress within the electrode and resulting in electrode deformation and fragmentation.This ultimately leads to a decrease in cell capacity.The trends of volume expansion and capacity change of the SiO/graphite(SiO/C)composite electrode during cycling were investigated via in situ expansion monitoring.First,a series of expansion test schemes were designed,and the linear relationship between negative electrode expansion and cell capacity degradation was quantitatively analyzed.Then,the effects of different initial pressures on the long-term cycling performance of the cell were evaluated.Finally,the mechanism of their effects was analyzed by scanning electron microscope.The results show that after 50 cycles,the cell capacity decreases from 2.556 mAh to 1.689 mAh,with a capacity retention ratio(CRR)of only 66.08%.A linear relationship between the capacity retention ratio and thickness expansion was found.Electrochemical measurements and scanning electron microscope images demonstrate that intense stress inhibits the lithiation of the negative electrode and that the electrode is more susceptible to irreversible damage during cycling.Overall,these results reveal the relationship between the cycling performance of SiO and the internal pressure of the electrode from a macroscopic point of view,which provides some reference for the application of SiO/C composite electrodes in lithium-ion batteries. 展开更多
关键词 lithium-ion batteries in situ expansion measurement initial stress cycle life SiO/C composite electrode
在线阅读 下载PDF
Preparation of defect free ceramic/Ti composite membranes by surface modification and in situ oxidation 被引量:1
3
作者 ZHANG Dong-qiang YANG Ping +2 位作者 WU Jian-yang ZHAO Jing CHEN Yan-an 《Journal of Central South University》 SCIE EI CAS CSCD 2019年第12期3295-3304,共10页
Al2O3 ceramic powder was applied to modify the large pores defects on the surface of the porous metal Ti support,in situ oxidation method was a convenient method to prepare defect free ceramic/Ti composite membranes o... Al2O3 ceramic powder was applied to modify the large pores defects on the surface of the porous metal Ti support,in situ oxidation method was a convenient method to prepare defect free ceramic/Ti composite membranes on this basis.In situ oxidation conditions experimental results show that the best condition for preparing the TiO2-Al2O3/Ti composite membrane is under 800°C for 2 h,and the microstructure and pore sizes of the TiO2-Al2O3/Ti composite membranes are affected obviously.The thickness and composition of the TiO2/Ti composite membranes are determined by SEM and XRD completely.The pore size distribution of the composite membrane is measured by bubble pressure method,the most probable aperture is about 3.12μm,while the average pore size of defect free TiO2-Al2O3/Ti is about 3.23μm.After ultrasonic treatment,the slight weight change of membranes reveals no observable change,which indicates that TiO2-Al2O3/Ti composite membranes maintain a good stability. 展开更多
关键词 porous Ti CERAMIC TiO2 layer in situ oxidation composite membrane surface modification
在线阅读 下载PDF
Reactive Processing and Mechanical Properties of Al/SiC_P Composite 被引量:4
4
作者 CHEN Kang-hua GE Jian-guo +1 位作者 LIU Hong-wei LIU Yun-zhong 《Journal of Central South University》 SCIE EI CAS 2000年第1期1-3,共3页
The reactive process for Al/SiC P composite was studied. SiC particles were in situ coated by the exothermal reaction of SiC Ti powder compact in Al melt bath, and easily incorporated into Al melt. The detailed study ... The reactive process for Al/SiC P composite was studied. SiC particles were in situ coated by the exothermal reaction of SiC Ti powder compact in Al melt bath, and easily incorporated into Al melt. The detailed study was carried out to understand the microstructures of the reacted SiC particles. During the reaction and consequent mixing, the successive processes include in situ coating on the reacted SiC particles, coat dissolution and SiC P splitting. The tensile mechanical properties of 6013Al/SiC P composite processed by the present technology showed that the reacted SiC P considerably reinforced the 6013 matrix. 展开更多
关键词 Al/SiC_P composite REACTIVE processing in situ coating MECHANICAL properties
在线阅读 下载PDF
Influence of B4C particle size on microstructure and damping capacities of(B_(4)C+Ti)/Mg composites 被引量:5
5
作者 YAO Yan-tao CHEN Li-qing WANG Wen-guang 《Journal of Central South University》 SCIE EI CAS CSCD 2021年第3期648-656,共9页
To study the influence of B4C particle size on the microstructure and damping capacities of(B_(4)C+Ti)/Mg composites,in situ reactive infiltration technique was utilized to prepare Mg-matrix composites.The microstruct... To study the influence of B4C particle size on the microstructure and damping capacities of(B_(4)C+Ti)/Mg composites,in situ reactive infiltration technique was utilized to prepare Mg-matrix composites.The microstructure,produced phases and damping capacities of the composites prepared with different particle size of B4C were characterized and analyzed.The results show that the reaction between B4C and Ti tends to be more complete when finer B_(4)C particle was used to prepare the composites.But the microstructure of the as-prepared composites is more homogenous when B4C and Ti have similar particle size.The strain-dependent damping capacities of(B_(4)C+Ti)/Mg composites improve gradually with the increase of strain amplitude,and composites prepared with coarser B4C particles tend to have higher damping capacities.The temperature-dependent damping capacities improve with increasing the measuring temperatures,and the kind of damping capacities of the composites prepared with 5mm B4C are inferior to those of coarser particles.The dominant damping mechanism for the strain-damping capacity is dislocation damping and plastic zone damping,while that for the temperature-damping capacity is interface damping or grain boundary damping. 展开更多
关键词 Mg-matrix composites in situ reactive infiltration particle size MICROSTRUCTURE damping capacity mechanism
在线阅读 下载PDF
Bearing capacity and mechanical behavior of CFG pile composite foundation
6
作者 陈秋南 赵明华 +1 位作者 周国华 张主华 《Journal of Central South University》 SCIE EI CAS 2008年第S2期45-49,共5页
CFG pile (i.e., pile constructed by granular materials of cement, fly-ash and gravel) composite foundation is applied in subsoil treatment widely and successfully. In order to have a further study of this kind of subs... CFG pile (i.e., pile constructed by granular materials of cement, fly-ash and gravel) composite foundation is applied in subsoil treatment widely and successfully. In order to have a further study of this kind of subsoil treatment technology, the influencing factors and calculation methods of the vertical bearing capacity of single CFG pile and the CFG pile composite foundation were discussed respectively. And based on the obtained solutions, effects by the cushion and measurements to reduce negative friction area were analyzed. Moreover, the developing law of settlement and bearing capacity eigenvalue controlled by the material strength with the increase of load were given for the CFG composite foundation. The in-situ static load test was tested for CFG pile. The results of test show that the maximum test load or half of the ultimate load is used from all the points of test, the average bearing capacity eigenvalue of single pile is 390 kN, and slightly greater than the design value of bearing capacity. The bearing capacity eigenvalues of composite foundation for 3 piles are greater than 300 kPa, and the mechanical properties of CFG pile composite foundation are almost identical in the case of the same load and cushion thickness. The pile-soil stress ratio and the load-sharing ratio can be adjusted through setting up cushion thickness. 展开更多
关键词 CFG PILE composite FOUNDATION properties of BEARING capacity in-situ static load PILE-SOIL stress ratio
在线阅读 下载PDF
Synthesis and characterization of alumina-matrix oxide/oxide composites
7
作者 Makoto EZUMI Daisuke NOMOTO Takahiro AKAO Tetsuhiko ONDA Zhong-Chun CHEN 《材料与冶金学报》 CAS 2010年第4期290-295,共6页
在线阅读 下载PDF
TiC-TiB_(2)/Al-xSi-4.5Cu复合材料的制备与性能
8
作者 梁艳峰 刘逍恂 +1 位作者 夏峰 郭巧琴 《热加工工艺》 北大核心 2025年第9期92-97,共6页
根据TiB_(2)与TiC原位粒子的形成温区,设计粒子的原位反应路径,在铸造Al-xSi-4.5Cu(x=7,2,18,wt%)合金熔体内成功制备TiB_(2)与TiC双相粒子。借助OM、SEM、EDS等方法观察所制备的复合材料微观组织,并测试其维氏硬度,探究基体合金中Si含... 根据TiB_(2)与TiC原位粒子的形成温区,设计粒子的原位反应路径,在铸造Al-xSi-4.5Cu(x=7,2,18,wt%)合金熔体内成功制备TiB_(2)与TiC双相粒子。借助OM、SEM、EDS等方法观察所制备的复合材料微观组织,并测试其维氏硬度,探究基体合金中Si含量对原位TiB_(2)与TiC粒子分布及复合材料硬度的影响。结果表明:3种Si含量的复合材料均可以通过原位自生法获得微纳米尺度的TiB_(2)与TiC双相粒子,但随着Si含量增加,原位粒子在Si相附近团聚加剧;当Si含量为12wt%时,复合材料硬度达到极值,为173.56 HV;当Si含量增加到18wt%时,TiC粒子发生失稳分解,导致了复合材料硬度下降。 展开更多
关键词 AL-SI-CU合金 AL基复合材料 TIC TiB_(2) 原位自生法
在线阅读 下载PDF
原位自生TiB_(w)/Ti网状复合材料的热变形行为
9
作者 贾建波 穆利双 +2 位作者 赵留洋 刘宝宝 徐岩 《中国有色金属学报》 北大核心 2025年第8期2772-2787,共16页
通过热压缩等温实验对放电等离子烧结原位自生TiB_(w)/Ti复合材料在变形温度650~800℃、应变速率0.01~5 s^(-1)条件下的热变形行为进行了研究,并建立了复合材料的本构方程,获得了Zener-Hollomon参数对微观组织演变的影响规律。结果表明:... 通过热压缩等温实验对放电等离子烧结原位自生TiB_(w)/Ti复合材料在变形温度650~800℃、应变速率0.01~5 s^(-1)条件下的热变形行为进行了研究,并建立了复合材料的本构方程,获得了Zener-Hollomon参数对微观组织演变的影响规律。结果表明:TiB_(w)/Ti复合材料的峰值应力随温度降低和应变速率升高而升高。不同ln Z值对应不同的组织形貌特征,当ln Z为高值(≥42.50)时,局部塑性流动区是主要的微观组织特征,动态再结晶程度低,再结晶晶粒平均尺寸小于1.40μm。当ln Z为中值(34.29~38.50)时,动态再结晶显著,再结晶晶粒平均尺寸为1.53~2.91μm,且随ln Z值减小,增强颗粒长径比增大,偏聚现象改善,位错密度降低,再结晶程度提高。当ln Z为低值(≤32.48)时,再结晶晶粒明显粗化,平均晶粒尺寸大于3.18μm。 展开更多
关键词 TiB_(w)/Ti复合材料 原位自生 热变形行为 ZENER-HOLLOMON参数 微观组织
在线阅读 下载PDF
原位合成(TiC+Al_(3)Ti)增强铝基复合材料组织及性能研究
10
作者 庄伟彬 曹庆 +3 位作者 覃龙健 孙川淼 金忠贵 刘敬福 《功能材料》 北大核心 2025年第7期7140-7145,共6页
采用原位合成方法,制备了1%、3%、5%(质量分数)(TiC+Al_(3)Ti)/6061铝基复合材料,研究了双相增强体含量对复合材料组织及性能的影响。在复合材料中,TiC颗粒分布于晶界处,而Al_(3)Ti相呈短棒状、分布于晶粒内部。复合材料的晶粒尺寸随着(... 采用原位合成方法,制备了1%、3%、5%(质量分数)(TiC+Al_(3)Ti)/6061铝基复合材料,研究了双相增强体含量对复合材料组织及性能的影响。在复合材料中,TiC颗粒分布于晶界处,而Al_(3)Ti相呈短棒状、分布于晶粒内部。复合材料的晶粒尺寸随着(TiC+Al_(3)Ti)含量的增加而逐渐减小,当(TiC+Al_(3)Ti)含量为5%(质量分数)时,晶粒细化效果最为显著,此时复合材料平均晶粒尺寸为43.02μm。随着(TiC+Al_(3)Ti)含量的增加,铸态复合材料布氏硬度、抗拉强度、屈服强度以及最大抗压载荷逐渐增加,5%(质量分数)(TiC+Al_(3)Ti)/6061复合材料的各项力学性能最高,其值分别为104.57 HB、322.19 MPa、186.27 MPa、457.13 MPa。 展开更多
关键词 铝基复合材料 原位合成 (TiC+Al_(3)Ti) 显微组织 力学性能
在线阅读 下载PDF
原位纳米ZrB_(2)颗粒与稀土Sc协同增强7N01铝合金的微观组织与拉伸性能
11
作者 怯喜周 陈锐崐 +1 位作者 彭艳杰 赵玉涛 《热加工工艺》 北大核心 2025年第9期108-112,共5页
在7N01铝合金中同时引入原位纳米ZrB_(2)颗粒和稀土元素Sc,通过原位纳米颗粒和稀土元素的协同作用来提高材料的强塑性。研究表明,向铝合金中单独引入原位纳米ZrB_(2)颗粒的含量超过3wt%后,其团聚现象较严重,不利于复合材料性能的提高。... 在7N01铝合金中同时引入原位纳米ZrB_(2)颗粒和稀土元素Sc,通过原位纳米颗粒和稀土元素的协同作用来提高材料的强塑性。研究表明,向铝合金中单独引入原位纳米ZrB_(2)颗粒的含量超过3wt%后,其团聚现象较严重,不利于复合材料性能的提高。在此基础上引入稀土Sc后,原位ZrB_(2)纳米颗粒的团聚现象得到显著改善。同时,Sc的加入还可有效改善粗大的含铁析出相,细化基体晶粒;原位纳米ZrB_(2)颗粒和稀土Sc的协同引入使复合材料的强度和塑性较7N01基体的性能大幅提高,当ZrB_(2)和Sc的引入量分别为3wt%和0.2wt%时,复合材料的屈服强度、抗拉强度和伸长率匹配最优,分别为447 MPa、481 MPa和9.6%,相比7N01铝合金基体的性能分别提高16.1%、11.3%和29.7%。 展开更多
关键词 7N01基复合材料 原位纳米ZrB_(2)颗粒 稀土Sc 微观组织 拉伸性能
在线阅读 下载PDF
硫酸镁/硅胶复合蜂窝胚体的制备及其除湿特性研究
12
作者 张向京 张美瑶 +2 位作者 郑金海 徐晓阳 任鹏 《无机盐工业》 北大核心 2025年第8期58-64,共7页
为了开发高性能除湿转轮,通过创新材料设计和工艺优化的方式,采用原位生长技术在圆柱形蜂窝载体上沉积硅胶基质,以硫酸镁(MgSO4)作为吸湿盐进行改性,成功制备了MgSO4/硅胶复合蜂窝胚体。采用单因素实验法,系统探究了增强载体机械强度的... 为了开发高性能除湿转轮,通过创新材料设计和工艺优化的方式,采用原位生长技术在圆柱形蜂窝载体上沉积硅胶基质,以硫酸镁(MgSO4)作为吸湿盐进行改性,成功制备了MgSO4/硅胶复合蜂窝胚体。采用单因素实验法,系统探究了增强载体机械强度的预处理条件和复合除湿材料的制备条件,确定了最优的预处理浆液配方为硅酸钠、聚乙烯醇(PVA)、铝溶胶的混合溶液(固体质量比1∶1∶1)。采用单因素实验法,确定了最佳负载工艺条件是硅酸钠质量分数为30%、分3次浸渍、酸化温度为90℃、酸质量分数为20%。胚体吸附测试结果表明,随着相对湿度从30%提升至80%,样品的吸附量从162 mg/g提升至251 mg/g,相对提高了54.93%,是单一硅胶的2~3倍。随着温度由15℃升高到35℃,样品的吸附平衡时间由835 s缩短至435 s,但吸附量由256 mg/g减少至133 mg/g。风速提高加快吸附速率,对平衡吸附量影响不大。循环吸脱附实验表明,材料具有优异的循环稳定性和再创性能。 展开更多
关键词 转轮除湿 复合除湿材料 原位生长技术 除湿特性
在线阅读 下载PDF
Al/Ni-WC复合涂层高温抗氧化性能与扩散分析
13
作者 李德元 孙继博 +2 位作者 李光全 张楠楠 祝成 《沈阳工业大学学报》 北大核心 2025年第2期197-204,共8页
【目的】碳钢因其较差的抗氧化性能,在高温工况下的使用受到了严格限制。Ni-Al金属间化合物由于具有较高的熔点和较好的高温抗氧化性能,在实际工业领域应用众多。针对含有Ni-Al金属间化合物的涂层,研究其高温抗氧化涂层的进一步应用,提... 【目的】碳钢因其较差的抗氧化性能,在高温工况下的使用受到了严格限制。Ni-Al金属间化合物由于具有较高的熔点和较好的高温抗氧化性能,在实际工业领域应用众多。针对含有Ni-Al金属间化合物的涂层,研究其高温抗氧化涂层的进一步应用,提高碳钢的高温使用寿命,拟在碳钢表面制备Ni-Al反应改性涂层。【方法】采用超音速火焰喷涂在碳钢基体上制备Ni-WC涂层,随后在其上利用电弧喷涂制备Al涂层,在800℃不同时间扩散处理下使得涂层内的Ni-Al发生反应,以得到金属间化合物并增强其高温抗氧化性能。通过记录氧化增重曲线测试涂层的高温抗氧化性能。【结果】在高温氧化过程中Al/Ni-WC复合涂层在Al/Ni界面处原位生成了富铝的Ni-Al金属间化合物。Al/Ni-WC涂层经800℃扩散处理过程中,首先形成富Al的NiAl 3,且其表面Al原子与大气中的氧原子反应形成了Al_(2)O_(3)。随着反应时间的延长,在Al/Ni界面形成的NiAl 3相转变为抗高温氧化能力更优异的Ni_(2)Al_(3)相,两种Ni-Al金属间化合物本身具有高熔点和高温抗氧化性能,且在Al/Ni-WC复合涂层表面形成的Al_(2)O_(3)减缓了氧原子的扩散过程。Al/Ni-WC复合涂层试件的扩散层厚度随着扩散处理时间的延长呈现类似线性增长趋势。经800℃扩散处理后,Al/Ni-WC涂层中NiAl 3层的增厚速率较快,且在加热10 h后原位反应生成了更厚的Ni_(2)Al_(3)层。经800℃扩散处理20 h后,经过原位反应得到了比NiAl 3层稍厚一些的Ni_(2)Al_(3)层。由于Ni_(2)Al_(3)层熔点更高且更稳定,因而经过800℃扩散处理后的Al/Ni-WC涂层具有更好的高温抗氧化能力。经900℃/50 h扩散处理后的Al/Ni-WC涂层经循环氧化后存在陶瓷相Al_(2)O_(3)、WC和NiAl相,在陶瓷相和NiAl相的共同作用下呈现较好的高温抗氧化性能。测得不同扩散时间下Al/Ni-WC涂层的扩散层厚度,得到了Ni和Al之间的扩散关系式,其扩散反应动力指数为0.79045,复合涂层对碳钢基体的保护作用明显提高。【结论】在氧化过程中形成的Ni-Al金属间化合物、Al_(2)O_(3)膜与涂层中原有WC相的共同作用下碳钢基体的高温抗氧化性能得到了明显提升。通过氧化增重实验可知,在Ni层中增加陶瓷相以后,金属-陶瓷复合涂层的高温抗氧化能力明显优于碳钢基体,因而对碳钢基体的保护效果更好。 展开更多
关键词 电弧喷涂 超音速火焰喷涂 碳钢 原位生成 Al/Ni-WC复合涂层 Al/Ni界面 高温抗氧化性能 Ni-Al金属间化合物
在线阅读 下载PDF
冷喷涂Ti-Al复合材料的搅拌摩擦加工改性研究 被引量:1
14
作者 刘杨 徐雅欣 李文亚 《表面技术》 北大核心 2025年第3期210-219,共10页
目的解决冷喷涂直接沉积钛铝金属间化合物时因金属颗粒硬脆而出现的沉积率极低或无法沉积等问题,针对增材制造钛铝合金的需求,采用冷喷涂和搅拌摩擦加工相结合的方法原位制备钛铝金属间化合物。方法采用纯铝板为冷喷涂基板,经冷喷涂沉积... 目的解决冷喷涂直接沉积钛铝金属间化合物时因金属颗粒硬脆而出现的沉积率极低或无法沉积等问题,针对增材制造钛铝合金的需求,采用冷喷涂和搅拌摩擦加工相结合的方法原位制备钛铝金属间化合物。方法采用纯铝板为冷喷涂基板,经冷喷涂沉积纯Ti、Al后得到预沉积体,对已沉积的Ti-Al复合材料进行不同参数的搅拌摩擦加工后制备出试样,并采用光镜、扫描电镜、X射线衍射、硬度测试对比研究不同处理状态复合材料的组织和性能。结果喷涂态沉积体并未形成Ti-Al金属间化合物。经FSP处理后,沉积体中形成了含有细小晶粒的Ti和Ti-Al金属间化合物复合组织。由XRD结果可知,FSP制备的金属间化合物为TiAl3,且复合材料中存在未反应的原始Ti颗粒。冷喷涂沉积体经热处理因Kirkendall效应会产生较大孔隙,但经FSP处理后组织致密,无明显孔隙,硬度显著提高到256HV,复合材料的组织得到细化。结论通过高压冷喷涂技术和搅拌摩擦加工原位制备了组织均匀且致密、内部结合良好的钛铝金属间化合物,并使用优化后的搅拌摩擦工艺参数完成了良好的钛铝金属间化合物的增材制造,达到试验预期要求。 展开更多
关键词 原位生成 TIAL复合材料 冷喷涂 搅拌摩擦加工 微观组织 力学性能
在线阅读 下载PDF
原位自生TiB_(2)陶瓷颗粒增强铝基复合材料及其在航天领域的应用
15
作者 刘钧 陈哲 +4 位作者 陈东 李险峰 吴一 夏存娟 王浩伟 《载人航天》 北大核心 2025年第2期241-247,共7页
原位自生TiB_(2)陶瓷颗粒增强铝基复合材料兼具高模量、高强塑性、高抗疲劳与良好的加工成形性能,作为结构材料应用于航天飞行器,有助于实现相关构件的轻量化设计,且仅通过常规铝合金加工方法与设备,即可实现铝基复合材料构件的规模化... 原位自生TiB_(2)陶瓷颗粒增强铝基复合材料兼具高模量、高强塑性、高抗疲劳与良好的加工成形性能,作为结构材料应用于航天飞行器,有助于实现相关构件的轻量化设计,且仅通过常规铝合金加工方法与设备,即可实现铝基复合材料构件的规模化制造。对比分析了原位自生TiB_(2)陶瓷颗粒增强铝基复合材料与铝合金、传统铝基复合材料的优缺点,介绍了铸造、变形和增材制造三大系列原位自生铝基复合材料的组织性能与研究现状,以及相关系列铝基复合材料在航天领域的典型应用情况,并展望了原位自生TiB_(2)陶瓷颗粒增强铝基复合材料的发展方向。 展开更多
关键词 金属基复合材料 陶瓷颗粒 原位自生 铸造成形 塑性加工 增材制造
在线阅读 下载PDF
CsPbBr_(3)@MOF复合材料的制备及稳定性分析
16
作者 杨宇轩 杨晓华 +3 位作者 陈健壮 沈建华 张建鹏 杨晓玲 《功能材料》 北大核心 2025年第7期7008-7014,共7页
钙钛矿材料因具备结构可调、光电特性优异、制备成本较低等优点,在光电探测领域获得广泛关注。针对钙钛矿量子点目前存在的环境稳定性差的关键问题,采用固相模板法在金属有机框架材料MOF-5(Zn)孔隙内实现了钙钛矿量子点的原位合成,成功... 钙钛矿材料因具备结构可调、光电特性优异、制备成本较低等优点,在光电探测领域获得广泛关注。针对钙钛矿量子点目前存在的环境稳定性差的关键问题,采用固相模板法在金属有机框架材料MOF-5(Zn)孔隙内实现了钙钛矿量子点的原位合成,成功制备出具有优异稳定性的CsPbBr_(3)@MOF复合材料。通过透射电镜和X射线衍射表征证实了CsPbBr_(3)量子点成功合成并填充在MOF孔隙中。利用X射线光电子能谱分析了CsPbBr_(3)@MOF的化学组成和表面结构。同时,采用紫外-可见分光光度计、荧光分光光度计和瞬态荧光光谱研究了CsPbBr_(3)@MOF的光学性能。基于荧光光谱强度的变化趋势,证实了复合材料CsPbBr_(3)@MOF的水、光和热稳定性相较于CsPbBr_(3),获得显著提升。该研究为提高钙钛矿量子点的稳定性并拓展其应用提供了新思路及解决方案。 展开更多
关键词 固相模板法 原位合成 钙钛矿量子点 复合材料 稳定性
在线阅读 下载PDF
硼砂助熔剂诱导莫来石晶须增强硅酸铝纤维/SiO_(2)气凝胶复合材料的制备与性能研究
17
作者 马晓亮 汪桂根 +4 位作者 张孟予 赵宝军 钟业盛 史丽萍 赫晓东 《陶瓷学报》 北大核心 2025年第4期786-795,共10页
为改善陶瓷纤维增强气凝胶材料力学性能不足、容易脆裂的问题,在硅酸铝纤维表面引入原位生长的莫来石晶须,以硅酸铝纤维/莫来石晶须作为增强体,将SiO_(2)湿凝胶引入增强体中,通过常压干燥法获得硅酸铝纤维/莫来石晶须增强SiO_(2)气凝胶... 为改善陶瓷纤维增强气凝胶材料力学性能不足、容易脆裂的问题,在硅酸铝纤维表面引入原位生长的莫来石晶须,以硅酸铝纤维/莫来石晶须作为增强体,将SiO_(2)湿凝胶引入增强体中,通过常压干燥法获得硅酸铝纤维/莫来石晶须增强SiO_(2)气凝胶复合材料。该复合材料最大压缩形变可达60%,在60%压缩形变下,材料抗压强度可达1.745 MPa,约为硅酸铝纤维增强SiO_(2)气凝胶材料抗压强度(0.518 MPa)的3.4倍,该复合材料还具有密度低(0.24 g·cm^(-3))、热导率低(0.038 W·m^(-1)·K^(-1))、比表面积高(106.21 m^(2)·g^(-1))等优点。 展开更多
关键词 莫来石晶须 原位生长 气凝胶复合材料 力学性能 热物理性能
在线阅读 下载PDF
基于原位自动铺放成形工艺的丢层结构轨迹规划方法
18
作者 胡诗睿 李彦锐 +3 位作者 廖文强 陈志坤 黄志高 周华民 《精密成形工程》 北大核心 2025年第8期194-202,共9页
目的针对复合材料丢层结构的特点,对自动铺放工艺的轨迹规划进行研究。方法首先基于CATIA平台对复合材料丢层结构进行了详细的结构建模与设计,分析了丢层区域的几何特征及其对铺层轨迹生成的影响。针对丢层铺层面的形状复杂性,提出了一... 目的针对复合材料丢层结构的特点,对自动铺放工艺的轨迹规划进行研究。方法首先基于CATIA平台对复合材料丢层结构进行了详细的结构建模与设计,分析了丢层区域的几何特征及其对铺层轨迹生成的影响。针对丢层铺层面的形状复杂性,提出了一种结合铺层面填充、轨迹生成与轨迹投影的综合轨迹规划方法。该方法通过铺层填充策略,确保了轨迹在复杂区域内的覆盖完整性,最后采用几何投影对丢层区域进行路径划分。在实验部分,利用搭建的自动铺放平台对典型丢层结构样件进行了铺放验证。结果采用所提出的方法能够高效生成适应丢层结构特征的铺放轨迹,在不考虑非工艺因素的情况下,轨迹精度和铺放质量均达到较高水平。结论为实际工程中处理类似丢层复杂结构的轨迹规划提供了理论和技术支持。 展开更多
关键词 复合材料 丢层结构 轨迹规划 自动铺放 原位成形
在线阅读 下载PDF
Cu-Fe-Cr原位复合材料的纤维相结构 被引量:5
19
作者 孙世清 郭志猛 殷声 《中国有色金属学报》 EI CAS CSCD 北大核心 2003年第3期658-661,共4页
通过感应熔炼和冷拔变形制备了Cu 16Fe 2Cr原位复合材料 ,将铜基体选择腐蚀后提取出了纤维 ,采用SEM和TEM观察分析了纤维相结构。在较低的应变量 (η =1.6 7)时 ,纤维不均匀 ,随着变形量的增大 (η =5 .42 ) ,纤维外形变得均匀。在 η =... 通过感应熔炼和冷拔变形制备了Cu 16Fe 2Cr原位复合材料 ,将铜基体选择腐蚀后提取出了纤维 ,采用SEM和TEM观察分析了纤维相结构。在较低的应变量 (η =1.6 7)时 ,纤维不均匀 ,随着变形量的增大 (η =5 .42 ) ,纤维外形变得均匀。在 η =5 .42时 ,一个显著的特点是单根Fe Cr纤维分为一些由晶界隔开的平行亚单元 (宽度约为 10 0nm) ,通过亚单元共同的 [110 ]衍射获得了晶粒之间的相对取向 ,相邻晶粒的取向角在 3°~ 15°之间。 展开更多
关键词 cu-fe-cr原位复合材料 选择腐蚀 Fe-Cr纤维 亚单元 织构
在线阅读 下载PDF
Cu-Fe-Cr-Ni原位复合材料的结构与性能 被引量:1
20
作者 孟永强 孙世清 +1 位作者 毛磊 刘宗茂 《河北科技大学学报》 CAS 2006年第4期297-301,共5页
通过感应熔炼、浇铸、热轧和冷拔制备了Cu-Fe-Cr-Ni原位复合材料,采用XRD,SEM和TEM研究了Ni元素和拉拔变形量对其显微结构的影响。用拉伸实验测试了材料的强度,用标准四探针方法测量了材料的电阻。在Cu-Fe-Cr-Ni合金铸锭中,bcc结构的第... 通过感应熔炼、浇铸、热轧和冷拔制备了Cu-Fe-Cr-Ni原位复合材料,采用XRD,SEM和TEM研究了Ni元素和拉拔变形量对其显微结构的影响。用拉伸实验测试了材料的强度,用标准四探针方法测量了材料的电阻。在Cu-Fe-Cr-Ni合金铸锭中,bcc结构的第2相为近球形颗粒形态,经过后续的变形加工,颗粒演变成了近圆形横截面的纤维。对Cu-Fe-Cr-Ni原位复合材料只进行了1次550℃中间退火,就可以获得较高的拉拔变形量(η=5.32),表明Ni的加入可以改善原位复合材料的塑性。随着拉拔变形量的增大,Cu-Fe-Cr-Ni原位复合材料的强度增加,电导率下降。 展开更多
关键词 原位复合材料 Ni元素 塑性 强度 电导率