以硝酸铈和尿素为原料,1,3,5苯三甲酸为配体,采用简单的静电自组装法合成了铈金属有机框架(Ce-BTC)和石墨相氮化碳(g-C_(3)N_(4))的复合材料(Ce-BTC/g-C_(3)N_(4)),用于二氧化碳还原制一氧化碳的研究,并探索Ce-BTC的复合对g-C_(3)N_(4)...以硝酸铈和尿素为原料,1,3,5苯三甲酸为配体,采用简单的静电自组装法合成了铈金属有机框架(Ce-BTC)和石墨相氮化碳(g-C_(3)N_(4))的复合材料(Ce-BTC/g-C_(3)N_(4)),用于二氧化碳还原制一氧化碳的研究,并探索Ce-BTC的复合对g-C_(3)N_(4)性能的影响机制。利用X射线衍射、红外光谱、扫描电子显微镜、紫外-可见光吸收光谱、荧光光谱、阻抗、光电流测试和CO_(2)还原性能测试对复合材料的结构、形貌、光电学性能及催化性能进行研究。结果表明Ce-BTC与g-C_(3)N_(4)的复合可能使得g-C_(3)N_(4)层间距发生改变,在细化晶体颗粒的同时提高样品比表面积,使复合样品获得更高的可见光捕获能力且载流子的分离效率更高;在仅加入1 mL H2O作为质子提供源的前提下,Ce-BTC/g-C_(3)N_(4)-3拥有最优光催化性能。CO产率为19.02μmol/(h·g),是g-C_(3)N_(4)的2.25倍,循环测试后催化性能基本保持稳定。展开更多
Atom economy of the process of rare earth separation by using fluoride was discussed in this paper.We compared the atomic economic characters between the processes of vitriolic composite salt and fluoride,then stated ...Atom economy of the process of rare earth separation by using fluoride was discussed in this paper.We compared the atomic economic characters between the processes of vitriolic composite salt and fluoride,then stated that changing present rare earth producing process by green chemistry and technology transformation was the best way to make our rare earth manufacture prosperous.展开更多
文摘以硝酸铈和尿素为原料,1,3,5苯三甲酸为配体,采用简单的静电自组装法合成了铈金属有机框架(Ce-BTC)和石墨相氮化碳(g-C_(3)N_(4))的复合材料(Ce-BTC/g-C_(3)N_(4)),用于二氧化碳还原制一氧化碳的研究,并探索Ce-BTC的复合对g-C_(3)N_(4)性能的影响机制。利用X射线衍射、红外光谱、扫描电子显微镜、紫外-可见光吸收光谱、荧光光谱、阻抗、光电流测试和CO_(2)还原性能测试对复合材料的结构、形貌、光电学性能及催化性能进行研究。结果表明Ce-BTC与g-C_(3)N_(4)的复合可能使得g-C_(3)N_(4)层间距发生改变,在细化晶体颗粒的同时提高样品比表面积,使复合样品获得更高的可见光捕获能力且载流子的分离效率更高;在仅加入1 mL H2O作为质子提供源的前提下,Ce-BTC/g-C_(3)N_(4)-3拥有最优光催化性能。CO产率为19.02μmol/(h·g),是g-C_(3)N_(4)的2.25倍,循环测试后催化性能基本保持稳定。
文摘Atom economy of the process of rare earth separation by using fluoride was discussed in this paper.We compared the atomic economic characters between the processes of vitriolic composite salt and fluoride,then stated that changing present rare earth producing process by green chemistry and technology transformation was the best way to make our rare earth manufacture prosperous.