铜合金表面等离子堆焊NiCrSiB系自熔合金的组织和性能 被引量:1
1
作者 刘欢 朱圣华 李运昌 《林业机械与木工设备》 2016年第7期35-37,共3页
采用等离子堆焊技术,在一种铜合金基体上制备NiCrSiB系自熔合金粉末的堆焊层。使用扫描电子显微镜、X-射线衍射仪、显微硬度计等测试仪器,研究NiCrSiB系自熔合金粉末堆焊层的组织结构和显微硬度。结果表明:基体和堆焊层实现了冶金熔合;... 采用等离子堆焊技术,在一种铜合金基体上制备NiCrSiB系自熔合金粉末的堆焊层。使用扫描电子显微镜、X-射线衍射仪、显微硬度计等测试仪器,研究NiCrSiB系自熔合金粉末堆焊层的组织结构和显微硬度。结果表明:基体和堆焊层实现了冶金熔合;堆焊层由γ-Ni相固溶体和γ'、-Ni相固溶体组成,同时有Fe Ni_3、Al B_2、Cr B、Cr Ni等化合物相的析出。 展开更多
关键词 铜合金 等离子堆焊 Ni-Cr-Si-B系自熔合金 组合和性能
在线阅读 下载PDF
Microstructure characteristics and effect of grain orientation on magnetic properties of Fe_(63)Co_(32)Gd_5 alloy ribbons
2
作者 姚文静 王楠 LEE Je-hyun 《Journal of Central South University》 SCIE EI CAS CSCD 2015年第6期2014-2019,共6页
By using the melt spinning techniques, the Fe63Co32Gd5 alloy ribbons with 15-50 m in thickness and 3-7 mm in width were prepared at the wheel speeds of 15, 20, 25 and 35 m/s. The rapid solidification microstructures w... By using the melt spinning techniques, the Fe63Co32Gd5 alloy ribbons with 15-50 m in thickness and 3-7 mm in width were prepared at the wheel speeds of 15, 20, 25 and 35 m/s. The rapid solidification microstructures were characterized by three layers, the middle layer of which reaches 80% thickness and forms the column grain of(Fe,Co) solid with Gd solution. Grain refinement takes place with the increase of the wheel speed. And after 0.5 h heat treatment at 823 K, the ribbon thickness becomes larger and the middle layer of column grain is very orderly perpendicular to the ribbon plane. The coercivity of quenched and annealed Fe63Co32Gd5 ribbons both have the inflection point at the wheel speed of 20 m/s, and the tendency is declining. The heat treatment processing makes the coercivity become lower by improving the order of(Fe,Co)17Gd2 compound. The saturation magnetization of quenched ribbons increases with the enhancement of wheel speed, whereas that of annealed ones decreases firstly and then increases. The minimum coercivity is 5.30×103 A/m and the maximum saturation magnetization is 163.62 A·m2/kg, which is obtained in the conditions of the wheel speed of 35 m/s and 0.5 h heat treatment at the temperature of 823 K. 展开更多
关键词 Fe-Co-Gd alloy ribbon rapid solidification phase composition magnetic properties
在线阅读 下载PDF