送粉激光熔覆层的逐层剥削磨损性能试验
1
作者 张庆茂 刘喜明 +1 位作者 陈莉 关振中 《机械工程材料》 CAS CSCD 北大核心 2000年第4期8-10,14,共4页
利用电子显微镜、X射线衍射、能谱分析 ,显微硬度和快速磨损试验 ,对送粉激光熔覆层逐层剥削 ,进行组织和磨损性能的跟踪观测 ,分析了熔覆层组织特征和碳化物的分布规律 ,熔覆层强度和硬度的提高是组织细化、碳化物强化的结果。为确定... 利用电子显微镜、X射线衍射、能谱分析 ,显微硬度和快速磨损试验 ,对送粉激光熔覆层逐层剥削 ,进行组织和磨损性能的跟踪观测 ,分析了熔覆层组织特征和碳化物的分布规律 ,熔覆层强度和硬度的提高是组织细化、碳化物强化的结果。为确定激光熔覆层的加工余量提供了依据。 展开更多
关键词 磨损性能试验 逐层剥削 送粉激光熔覆层
在线阅读 下载PDF
Friction properties of groove texture on Cr12MoV surface 被引量:6
2
作者 王敬 周杰 +1 位作者 朱姗姗 张建生 《Journal of Central South University》 SCIE EI CAS CSCD 2017年第2期303-310,共8页
To analyze the influence of surface texture on friction properties of Crl2MoV', ordinary grinder and spinning technology were adopted to obtain the grooved surface morphology of samples, and then the impact of spindl... To analyze the influence of surface texture on friction properties of Crl2MoV', ordinary grinder and spinning technology were adopted to obtain the grooved surface morphology of samples, and then the impact of spindle speed and feed in z-direction on surface morphology in the process of spinning was studied. In addition, the corresponding friction coefficient of sample was obtained through friction and wear tests. The results show that the peak clipping and the valley filling were conducted on the grinding surface, which could improve the surface roughness effectively and make the grinding trench-type wear scar more uniform. Both the area ratio of groove and groove spacing increased initially and then decreased with the increase of the spindle speed or the feed in z-direction. As a kind of micro-process, the groove could influence the friction coefficient of sample surface, whose distribution was beneficial to the reduction of friction coefficient. Compared with the surface obtained through ordinary grinding, grooved surface morphology through spinning technology was more conductive to reduce the friction coefficient, which could be reduced by 25%. When the friction coefficient of sample was reduced to the minimum, the texture of groove corresponded had an optimal area ratio and an optimal groove spacing, 37.5% and 27.5 μm, respectively. 展开更多
关键词 groove texture SPINNING friction coefficient area ratio groove spacing
在线阅读 下载PDF