通过防弹陶瓷孔的加工实验,对烧结金刚石钻头的磨损状况进行研究。分析钻头唇面的磨损变相及打滑现象,指出内外径金刚石承受的切削载荷差异是造成钻头唇面磨损变相的主要原因;打滑现象则是由于出露的金刚石磨损过快,胎体的磨损不能与之... 通过防弹陶瓷孔的加工实验,对烧结金刚石钻头的磨损状况进行研究。分析钻头唇面的磨损变相及打滑现象,指出内外径金刚石承受的切削载荷差异是造成钻头唇面磨损变相的主要原因;打滑现象则是由于出露的金刚石磨损过快,胎体的磨损不能与之匹配造成的。根据磨损状况,提出改变金刚石品级、浓度分布、水口总宽度等改善磨损变相的措施以及采用弱包镶、改善胎体耐磨性、优化唇面和水口形状、控制冷却液流量等防止打滑的措施。该研究对优化防弹陶瓷加工工具设计,提高防弹陶瓷的加工效率和加工质量具有一定的参考价值。 展开更多
关键词 防弹陶瓷 烧结金刚石钻头 磨损变相 打滑
在线阅读 下载PDF
Effect of applied load on transition behavior of wear mechanism in Cu-15Ni-8Sn alloy under oil lubrication 被引量:6
2
作者 张世忠 甘雪萍 +3 位作者 成金娟 姜业欣 李周 周科朝 《Journal of Central South University》 SCIE EI CAS CSCD 2017年第8期1754-1761,共8页
Tribological behavior of Cu-15Ni-8Sn(mass fraction, %) alloy against GCr15 ring under various loads was investigated on a ring-on-block tester in oil lubrication. The results showed that the wear rate increased slowly... Tribological behavior of Cu-15Ni-8Sn(mass fraction, %) alloy against GCr15 ring under various loads was investigated on a ring-on-block tester in oil lubrication. The results showed that the wear rate increased slowly from 1.7×10^(-7) to 9.8× 10^(-7) mm^3/mm under the load lower than 300 N, and then increased dramatically to the climax of 216×10^(-7) mm^3/mm under the load over 300 N, which indicated the transition of wear mechanism with the increase of applied load. The wear mechanism mainly was plastic deformation and abrasive wear under the load less than 300 N. As the applied load was more than 300 N, the wear mechanism of Cu-15Ni-8Sn alloy primarily was delamination wear. Besides, the transition can also be confirmed from the different morphologies of worn surface, subsurface and wear debris. It is distinctly indicated that the appearance of flaky debris at the applied load over 300 N may be a critical point for the change of wear mechanism. 展开更多