不同固化压力下制备碳纤维增强铝层板的拉伸性能 被引量:1
1
作者 林磊 欧阳求保 +2 位作者 黄宇 诸静 虞红 《机械工程材料》 CAS CSCD 北大核心 2016年第12期53-56,共4页
以市售碳纤维增强环氧树脂预浸料和铝板为原料,以E-51环氧树脂为胶黏剂,分别在0.1,0.3,0.6MPa压力下于180℃固化2h制备了碳纤维增强铝层板(CRALL),研究了固化压力和铝板表面处理状态对其拉伸性能的影响。结果表明:随着固化压力的降低,CR... 以市售碳纤维增强环氧树脂预浸料和铝板为原料,以E-51环氧树脂为胶黏剂,分别在0.1,0.3,0.6MPa压力下于180℃固化2h制备了碳纤维增强铝层板(CRALL),研究了固化压力和铝板表面处理状态对其拉伸性能的影响。结果表明:随着固化压力的降低,CRALL的抗拉强度下降,失效方式由直接断裂转变为分层脱粘失效。在固化压力为0.6MPa、铝板经表面处理条件下制备的CRALL中,碳纤维增强层之间没有出现明显的分层现象,铝板与碳纤维增强层的界面结合良好;其抗拉强度为1 010MPa,弹性模量为77GPa,均接近理论值;拉伸时试样直接断裂,仅有较少的分层脱粘现象;而用未表面处理铝板制备的CRALL的抗拉强度比用表面处理铝板的下降了39%。 展开更多
关键词 碳纤维增强铝层板 固化压力 拉伸性能 显微组织 预浸料
在线阅读 下载PDF
Corrosion damage evolution and mechanical properties of carbon fiber reinforced aluminum laminate 被引量:4
2
作者 WU Xin-tong ZHAN Li-hua +3 位作者 HUANG Ming-hui ZHAO Xing WANG Xun ZHAO Guo-qing 《Journal of Central South University》 SCIE EI CAS CSCD 2021年第3期657-668,共12页
Fiber metal laminates(FMLs),a kind of lightweight material with excellent comprehensive performance,have been successfully applied in aerospace.FMLs reinforced with carbon fiber have better mechanical properties than ... Fiber metal laminates(FMLs),a kind of lightweight material with excellent comprehensive performance,have been successfully applied in aerospace.FMLs reinforced with carbon fiber have better mechanical properties than those with glass or aramid fiber.However,carbon fiber binding metal may lead to galvanic corrosion which limits its application.In this paper,electrochemical methods,optical microscope and scanning electron microscope were used to analyze the corrosion evolution of carbon fiber reinforced aluminum laminate(CARALL)in corrosive environment and explore anti-corrosion ways to protect CARALL.The results show that the connection between carbon fiber and aluminum alloy changes electric potential,causing galvanic corrosion.The galvanic corrosion will obviously accelerate CARALL corroded in solution,leading to a 72.1%decrease in interlaminar shear strength,and the crevice corrosion has a greater impact on CARALL resulting in delamination.The reduction of interlaminar shear strength has a similar linear relationship with the corrosion time.In addition,the adhesive layers between carbon fiber and aluminum alloy cannot protect CARALL,while side edge protection can effectively slow down corrosion rate.Therefore,the exposed edges should be coated with anti-corrosion painting.CARALL has the potential to be used for aerospace components. 展开更多
关键词 carbon fiber reinforced aluminum laminate galvanic corrosion ELECTROCHEMISTRY interlaminar shear strength aluminum alloy