基于WSR-DEMATEL模型的硫化矿石自燃灾害事故影响因素分析 被引量:4
1
作者 毛亚军 阳富强 《安全与环境工程》 CAS CSCD 北大核心 2023年第3期1-6,12,共7页
为了更加系统全面地了解硫化矿石自燃灾害事故影响因素,首先基于WSR(物理-事理-人理)系统分析方法找出可能引起硫化矿石自燃灾害事故的影响因素,从而构建硫化矿石自燃灾害事故影响因素指标体系,然后运用矩阵决策实验室分析法(DEMATEL)... 为了更加系统全面地了解硫化矿石自燃灾害事故影响因素,首先基于WSR(物理-事理-人理)系统分析方法找出可能引起硫化矿石自燃灾害事故的影响因素,从而构建硫化矿石自燃灾害事故影响因素指标体系,然后运用矩阵决策实验室分析法(DEMATEL)研究影响因素之间的相互影响关系,计算不同影响因素的中心度和原因度,确定关键影响因素。结果表明:通过综合考虑中心度和原因度,识别出引起硫化矿石自燃灾害事故的关键影响因素为温度、pH值、蓄热条件、矿石成分及含量、初始铁离子浓度、地质条件和氧气浓度。该研究可为有效提高金属矿山企业安全管理水平提供理论参考。 展开更多
关键词 矿山安全管理 硫化矿石自燃 影响因素 WSR DEMATEL
在线阅读 下载PDF
Nonlinear characteristics of induced spontaneous combustion process of sulfide ores 被引量:2
2
作者 潘伟 吴超 +2 位作者 李孜军 石英 杨月平 《Journal of Central South University》 SCIE EI CAS CSCD 2016年第12期3284-3292,共9页
To investigate the relationship between nonlinear parameters and spontaneous combustion tendency of sulfide ores, nine different sulfide ore samples were taken from a pyrite mine in China, and induced spontaneous comb... To investigate the relationship between nonlinear parameters and spontaneous combustion tendency of sulfide ores, nine different sulfide ore samples were taken from a pyrite mine in China, and induced spontaneous combustion experiment was carried out in the laboratory. Different stages of the induced spontaneous combustion process were studied by integrating wavelet technology and nonlinear dynamics theory. The results show that ignition points of all the ore samples are above 330 ℃, indicating that sulfide ores of the pyrite mine are difficult to combust spontaneously under normal mining conditions. Spontaneous combustion process includes three stages: incubation stage, development stage and approaching stage. The average temperature rising rate of the three stages are 1.0 ~C/min, 2.0 ~C/min and 4.2 ~C/min, respectively. During the spontaneous combustion process, mean values of approximate entropy and correlation dimension increase at first, and then decrease in the following stage. The mean value of the maximum Lyapunov exponent increases with the passage of reaction time. In a whole, correlation among the three nonlinear parameters firstly weakens, then enhances, and the best correlation period is at approaching stage. As ignition point increases, the maximum Lyapunov exponent of approaching stage decreases. Therefore, combustible tendency of sulfide ores could be qualitatively evaluated based on the maximum Lyapunov exponent of this stage. 展开更多
关键词 sulfide ores induced spontaneous combustion nonlinear parameters ignition point maximum Lyapunov exponent
在线阅读 下载PDF
Locating method of fire source for spontaneous combustion of sulfide ores 被引量:8
3
作者 刘辉 吴超 石英 《Journal of Central South University》 SCIE EI CAS 2011年第4期1034-1040,共7页
in order to achieve a more efficient way to accurately detect the position of the fire source of spontaneous combustion underground mine, a simple fire source locating method, based on infrared scanning system which c... in order to achieve a more efficient way to accurately detect the position of the fire source of spontaneous combustion underground mine, a simple fire source locating method, based on infrared scanning system which can determine the point where the highest temperature on the surface of igniting ores occurs, was proposed. First, the differential equations that describe heat flow in ore body were presented and the relationship between the surface temperature distribution and the depth and intensity of inner fire source was established with a relatively simple heat transfer model. With the solution of equation, the expression of the relationship between the surface temperature distribution and the inner fire source was deduced and the mathematical-physical model of heat transfer process was set up. Then, with the model, visualization of fire source on the basis of MATLAB simulation platform was realized. The results show that: 1) within 10 m, when the detecting depth is less than 2 m, the temperature perturbation on ores surface can change rapidly, and then slowly; after 4 m, in contrast, it changes very little, and is even close to zero at 10 m; 2) When it is close to self-ignition duration and the detective depths are 2, 5 and 10 m, respectively, the maximum temperature differences are correspondingly 0.5, 0.04 and 0.005 ℃ in the scope of 1 m×1 m; under the same condition, the maximum temperature differences are 1.391, 0.136 and 0.018 ℃, respectively, in the scope of 2 m×2 m. Therefore, this system can be used to measure the temperature differences on the surface of ore body and determine the highest temperature point directly. Also, it is possible to determine the depth of fire source and its intensity by locating method of fire source indirectly. 展开更多
关键词 sulfide ores spontaneous combustion location of fire source DETECTION
在线阅读 下载PDF
Spontaneous combustion tendency of fresh and pre-oxidized sulfide ores 被引量:2
4
作者 阳富强 吴超 李孜军 《Journal of Central South University》 SCIE EI CAS 2014年第2期715-719,共5页
Three representative sulfide ore samples were collected from typical metal mines,and their corresponding pre-oxidized products were obtained under nature environment.The thermal behaviors of each sample at heating rat... Three representative sulfide ore samples were collected from typical metal mines,and their corresponding pre-oxidized products were obtained under nature environment.The thermal behaviors of each sample at heating rates of 5,10,15 and 20 °C/min in air flow from ambient temperature to 800 °C were studied by simultaneous thermal analysis and the TG/DSC curves before and after the pre-oxidation were compared.By the peak temperature of DTG curves,the whole reaction process for each sample was divided into different stages,and the apparent activation energies were calculated by the Ozawa-Flynn-Wall method.The results show that the reaction process of each sample after pre-oxidation is more complex,with quicker reaction rates,fewer heat production quantities,and higher or lower ignition-points.The apparent activation energies decrease from 364.017-474.228 kJ/mol to 244.523- 333.161 kJ/mol.Therefore,sulfide ores are more susceptible to spontaneous combustion after the pre-oxidation. 展开更多
关键词 sulfide ores spontaneous combustion tendency apparent activation energy PRE-OXIDATION
在线阅读 下载PDF