轿车前轮毂轴承疲劳寿命强化试验研究 被引量:6
1
作者 李兴林 王成焘 +1 位作者 张燕辽 阮建国 《轴承》 北大核心 2000年第4期37-41,共5页
利用上海大众、上海汇众汽车公司提供的国内外轮毂轴承样品 ,进行恒定载荷寿命台架试验 ,首次对国内外五个轴承公司生产的桑塔纳轿车前轮毂双列圆锥滚子轴承 81 1 4 0 762 5A(JRM3 93 9 JRM3 968XD)共 50套用完全强化试验方法进行额定... 利用上海大众、上海汇众汽车公司提供的国内外轮毂轴承样品 ,进行恒定载荷寿命台架试验 ,首次对国内外五个轴承公司生产的桑塔纳轿车前轮毂双列圆锥滚子轴承 81 1 4 0 762 5A(JRM3 93 9 JRM3 968XD)共 50套用完全强化试验方法进行额定动载荷承载能力寿命试验对比分析 ,试验结果符合Lundberg Palmgren的寿命理论 ,并用德国大众的评价标准PVW 2 0 0 6对试验样品作出了正确评价。附图 2幅 ,表 3个 ,参考文献 5篇。 展开更多
关键词 汽车 轮毂轴承 疲劳寿命强化 试验研究
在线阅读 下载PDF
Improvement of fretting fatigue lifetime at 500℃of GH 4169 dovetail component treated by nanosecond stacked femtosecond laser shock peening
2
作者 FANG Xiu-yang WANG Zheng +4 位作者 GONG Jian-en WANG Zhi-guo CHEN Tai-li NI Jing CAI Zhen-bing 《Journal of Central South University》 2025年第7期2364-2382,共19页
The effects of nanosecond laser shock peening without coating(LSPwC)and nanosecond stacked femtosecond laser shock peening compound strengthening(LSP-CS)on the surface integrity and fretting fatigue lifetime at 500℃o... The effects of nanosecond laser shock peening without coating(LSPwC)and nanosecond stacked femtosecond laser shock peening compound strengthening(LSP-CS)on the surface integrity and fretting fatigue lifetime at 500℃of GH 4169 dovetail component were investigated.The results show that LSP treatment does not significantly lead to changes in the grain size of GH 4169 alloy,but it introduces a large number of dislocations,resulting in the formation of a plastic deformation layer and residual compressive stress layer.The surface microhardness increased by 20.5%and 28.6%after being treated by LSPwC and LSP-CS,respectively.The surface residual compressive stresses were(-306.5±42.5)MPa and(-404.3±34.7)MPa,respectively;The depth of both the hardening layer and the residual compressive stress layer is 400μm,and along the cross-section with 0-100μm region after LSP-CS treatment has higher hardness and greater residual compressive stress.The fretting fatigue lifetime of the GH 4169 dovetail component at 500℃was increased by 346.8%and 494.9%,which is the result of the combined effects of the hardening layer and the residual stress layer.The LSP-CS treatment can effectively make up for the disadvantage of the LSPwC treatment,and further enhance the fretting fatigue lifetime of the GH 4169 dovetail component at high temperature. 展开更多
关键词 GH 4169 dovetail LSPwC LSP-CS fretting fatigue life high temperature