A newly isolated bacterium was screened out for its survival on medium with 6 000 mg/L kraft lignin as the sole carbon source and energy, and identified as Pandoraea sp. by 16S rRNA gene sequence analysis. The biodegr...A newly isolated bacterium was screened out for its survival on medium with 6 000 mg/L kraft lignin as the sole carbon source and energy, and identified as Pandoraea sp. by 16S rRNA gene sequence analysis. The biodegradation experiment was carried out in mineral salt medium, containing 5 000 mg/L kraft lignin as only carbon and energy at pH 8.0 and 30℃. Under these conditions, significant reduction in color and lignin content by the strain was observed after incubation for 5 d. The strain attains maximum reduction capability in color (44.6%) and lignin content (39.9%) within 5 d of incubation, and reduced chemical oxygen demand(COD) from initial concentration 7 399 to 3 980 mg/L at maximum reduction level of 46.2% on the 4th day. The total ion chromatograph (TIC) of compounds presented in the chloroform extract of control and bacterial treated samples shows the formation of several lignin-related aromatic compounds including some small molecular lignin fragments, indicating a strong destruction in the lignin structure.展开更多
Solid wastes derived from metallurgical industries pose a significant threat to environment. The utilization and disposal of these solid wastes are the major concern in the world. Semi-coke generated in coal-based dir...Solid wastes derived from metallurgical industries pose a significant threat to environment. The utilization and disposal of these solid wastes are the major concern in the world. Semi-coke generated in coal-based direct reduction process of iron ore is a by-product and its suitable utilization is not available so far. In order to handle it properly, the characteristics of this by-product were comprehensively investigated. A series of analysis methods were used to demonstrate its mineral compositions, petrography and physico-chemical properties. The results reveal that the semi-coke has poor washability. The fixed carbon content of semi-coke reaches 76.11% and the gross calorific value is 28.10 MJ/kg, both of which are similar to those of traditional sinter coke breeze. Also, semi-coke ash possesses lower content of SiO2, Al2O3, S and higher content of CaO and MgO, which could improve the strength of sinter ore when partially substituting for coke breeze in sintering. Semi-coke features well-development porous structure and higher reaction activity, which predicts that the sintering speed could be elevated to some extent when employing it as a partial replacement of coke breeze, so the studies further suggest that the potential adverse effect of the high reactivity on sintering process could be weakened by adequately coarsening the semi-coke's particle size.展开更多
基金Project(50925417) supported by the National Funds for Distinguished Young Scientists,ChinaProject(50830301) supported by the Key program of the National Natural Science Foundation of ChinaProject(2012BAC12B03) supported by the National 12th Five-year Plan for Science and Technology Support,China
文摘A newly isolated bacterium was screened out for its survival on medium with 6 000 mg/L kraft lignin as the sole carbon source and energy, and identified as Pandoraea sp. by 16S rRNA gene sequence analysis. The biodegradation experiment was carried out in mineral salt medium, containing 5 000 mg/L kraft lignin as only carbon and energy at pH 8.0 and 30℃. Under these conditions, significant reduction in color and lignin content by the strain was observed after incubation for 5 d. The strain attains maximum reduction capability in color (44.6%) and lignin content (39.9%) within 5 d of incubation, and reduced chemical oxygen demand(COD) from initial concentration 7 399 to 3 980 mg/L at maximum reduction level of 46.2% on the 4th day. The total ion chromatograph (TIC) of compounds presented in the chloroform extract of control and bacterial treated samples shows the formation of several lignin-related aromatic compounds including some small molecular lignin fragments, indicating a strong destruction in the lignin structure.
基金Project(2011GH561685)supported by the China Torch Program
文摘Solid wastes derived from metallurgical industries pose a significant threat to environment. The utilization and disposal of these solid wastes are the major concern in the world. Semi-coke generated in coal-based direct reduction process of iron ore is a by-product and its suitable utilization is not available so far. In order to handle it properly, the characteristics of this by-product were comprehensively investigated. A series of analysis methods were used to demonstrate its mineral compositions, petrography and physico-chemical properties. The results reveal that the semi-coke has poor washability. The fixed carbon content of semi-coke reaches 76.11% and the gross calorific value is 28.10 MJ/kg, both of which are similar to those of traditional sinter coke breeze. Also, semi-coke ash possesses lower content of SiO2, Al2O3, S and higher content of CaO and MgO, which could improve the strength of sinter ore when partially substituting for coke breeze in sintering. Semi-coke features well-development porous structure and higher reaction activity, which predicts that the sintering speed could be elevated to some extent when employing it as a partial replacement of coke breeze, so the studies further suggest that the potential adverse effect of the high reactivity on sintering process could be weakened by adequately coarsening the semi-coke's particle size.