奥氏体不锈钢深冷容器疲劳设计曲线探讨 被引量:8
1
作者 郑津洋 王振宇 +4 位作者 陆群杰 刘宝庆 李克明 吴英哲 徐平 《压力容器》 北大核心 2021年第5期26-34,共9页
现行压力容器标准中奥氏体不锈钢疲劳设计曲线均基于常温疲劳试验数据拟合得来,并未考虑低温对奥氏体不锈钢强度、疲劳寿命的影响。本文提出一种基于常温疲劳设计曲线和深冷力学性能,获取奥氏体不锈钢深冷疲劳设计曲线的方法。首先,在... 现行压力容器标准中奥氏体不锈钢疲劳设计曲线均基于常温疲劳试验数据拟合得来,并未考虑低温对奥氏体不锈钢强度、疲劳寿命的影响。本文提出一种基于常温疲劳设计曲线和深冷力学性能,获取奥氏体不锈钢深冷疲劳设计曲线的方法。首先,在试验研究基础上整理分析了文献中77 K和4 K温度下的奥氏体不锈钢疲劳试验数据,并按ASME BPVCⅧ-2采用的Langer模型表征疲劳试验曲线;其次,根据低温对奥氏体不锈钢强度和塑性的影响规律,分别对Langer模型中的疲劳极限和塑性应变项系数进行修正,建立低温下Langer模型系数与温度的关联关系,提出了深冷疲劳试验曲线计算公式;最后,通过对比文献中110 K温度下材料疲劳试验数据,初步验证了深冷疲劳曲线计算方法的有效性。 展开更多
关键词 奥氏体不锈钢 深冷力学性能 疲劳设计曲线
在线阅读 下载PDF
Effect of quenching cooling rate on residual stress and microstructure evolution of 6061 aluminum alloy
2
作者 HUANG Ke YI You-ping +4 位作者 HUANG Shi-quan HE Hai-lin LIU Jie HUA Hong-en TANG Yun-jian 《Journal of Central South University》 SCIE EI CAS CSCD 2024年第7期2167-2180,共14页
In this study,the cooling rate was manipulated by quenching with water of different temperatures(30,60 and 100℃).Surface and internal residual stresses in the quenched 6061 aluminum alloy samples were measured using ... In this study,the cooling rate was manipulated by quenching with water of different temperatures(30,60 and 100℃).Surface and internal residual stresses in the quenched 6061 aluminum alloy samples were measured using hole-drilling and crack compliance methods,respectively.Then,the processability of the quenched samples was evaluated at cryogenic temperatures.The mechanical properties of the as-aged samples were assessed,and microstructure evolution was analyzed.The surface residual stresses of samples W30℃,W60℃and W100℃is−178.7,−161.7 and−117.2 MPa,respectively along x-direction,respectively;and−191.2,−172.1 and−126.2 MPa,respectively along y-direction.The sample quenched in boiling water displaying the lowest residual stress(~34%and~60%reduction in the surface and core).The generation and distribution of quenching residual stress could be attributed to the lattice distortion gradient.Desirable plasticity was also exhibited in the samples with relatively low quenching cooling rates at cryogenic temperatures.The strengthes of the as-aged samples are 291.2 to 270.1 MPa as the quenching water temperature increase from 30℃to 100℃.Fine and homogeneous β"phases were observed in the as-aged sample quenched with boiling water due to the clusters and Guinier-Preston zones(GP zones)premature precipitated during quenching process. 展开更多
关键词 6061 aluminum alloy residual stress cooling rate cryogenic cooling mechanical properties microstructure evolution