期刊文献+
共找到2篇文章
< 1 >
每页显示 20 50 100
复杂钼精矿湿法冶金工艺研究 被引量:6
1
作者 李贺 王海北 王玉芳 《有色金属(冶炼部分)》 CAS 北大核心 2013年第7期31-34,共4页
对低品位含铼复杂钼精矿进行氧压分解、萃取工艺研究。考察反应时间、氧分压、球磨时间、液固比等因素对钼转化率和溶出率的影响。结果表明,在230℃、反应时间2.5h、氧分压600kPa、液固比6的条件下氧压分解,钼转化率可达到98%以上,溶出... 对低品位含铼复杂钼精矿进行氧压分解、萃取工艺研究。考察反应时间、氧分压、球磨时间、液固比等因素对钼转化率和溶出率的影响。结果表明,在230℃、反应时间2.5h、氧分压600kPa、液固比6的条件下氧压分解,钼转化率可达到98%以上,溶出率为20%左右。氧压分解液采用分步萃取法回收钼、铼,铼萃取率和反萃率分别达到97%和99%以上,钼萃取率和反萃率分别达到99%和97%以上。 展开更多
关键词 复杂钼精矿 湿法冶金 氧压分解 萃取
在线阅读 下载PDF
Acid leaching decarbonization and following pressure oxidation of carbonic refractory gold ore 被引量:3
2
作者 张杜超 肖庆凯 +3 位作者 刘伟锋 陈霖 杨天足 刘又年 《Journal of Central South University》 SCIE EI CAS CSCD 2016年第7期1584-1590,共7页
Carbonate decomposition of carbonic refractory gold ore and the following pressure oxidation were studied.In the carbonate decomposition procedure,the effects of liquid-to-solid ratio and reaction time on decompositio... Carbonate decomposition of carbonic refractory gold ore and the following pressure oxidation were studied.In the carbonate decomposition procedure,the effects of liquid-to-solid ratio and reaction time on decomposition ratio of carbonate were investigated.The experimental result shows that the decomposition ratio of carbonate is 98.24%under the conditions of liquid-to-solid ratio of 5:1,Fe^(3+)concentration of 20 g/L,sulfuric acid concentration of 20 g/L,reaction temperature of 80 ℃ and reaction time of 2 h.Then,the slurry obtained from carbonate decomposition was put into the titanium autoclave for pressure oxidation leaching.Effects of liquid-to-solid ratio,temperature,time and oxygen partial pressure on sulfur oxidation ratio were studied during pressure oxidation.With the prolonged time,pyrite and arsenopyrite are oxidized to ferric subsulfate,hydrated ferric sulfate and jarosite,resulting in the increasing residue ratio.The residue ratio and the sulfur content in the residue can be decreased by ferric subsulfate dissolution.The oxidation ratio of the sulfur is 99.35% under the conditions of oxidation time of 4 h,temperature of 210 ℃,oxygen partial pressure of 0.8 MPa and stirring speed of 600 r/min. 展开更多
关键词 carbonic refractory gold ore carbonate decomposition pressure oxidation ferric subsulfate dissolution
在线阅读 下载PDF
上一页 1 下一页 到第