Tribological behavior of hot-pressed boron carbide with oxidation 被引量:1
1
作者 WANG Ling sen,WU Fang,ZHANG Jin sheng,FAN Yi,LIU Bo wei,GAO You (State Key Laboratory for Powder Metallurgy, Central South University, Changsha 410083, China) 《Journal of Central South University of Technology》 EI 2001年第2期89-93,共5页
The oxidation behavior at 973 1 273 K and the effect of oxidation on the room temperature tribological properties of hot pressed boron carbide ceramic were investigated. Oxidized samples were studied by X ray diffract... The oxidation behavior at 973 1 273 K and the effect of oxidation on the room temperature tribological properties of hot pressed boron carbide ceramic were investigated. Oxidized samples were studied by X ray diffractometer and scanning electron microscopy. It is demonstrated that the oxidation results in the formation of a thin transparent B 2O 3 film, and the oxide film is severely cracked during cooling due to the thermal expansion mismatch between the oxide film and B 4C substrate. B 2O 3 reacts with moisture in air to form boric acid, which is a kind of solid lubricant. The sliding friction factors of oxidized B 4C pair are about 0.05 0.08, compared to 0.25 0.35 of the as received B 4C pair. When the oxidation temperature is up to 1 273 K, severe unstability and increase of friction factor are observed. Visual inspection of the wear track reveals that the lubricant film is broken and some debris particles occur on and around the rubbing surfaces, because the friction interface is rough by the severe etching of grain boundaries. 展开更多
关键词 OXIDATION boron carbide friction factor boron oxide boron acid
在线阅读 下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部