Grain boundary precipitate induced PFZ formation to improve the ductility of extruded Mg-Gd-Y-Nd-Zr alloy after ageing
1
作者 GAO Ze-xi LIU Chu-ming +4 位作者 JIANG Shu-nong YANG Da-ling WAN Ying-chun GAO Yong-hao CHEN Zhi-yong 《Journal of Central South University》 2025年第3期693-705,共13页
An increase in RE element content in Mg alloys promotes the grain boundary precipitate,which affects the mechanical properties.However,the influence of grain boundary precipitates on microstructure of Mg-RE alloys dur... An increase in RE element content in Mg alloys promotes the grain boundary precipitate,which affects the mechanical properties.However,the influence of grain boundary precipitates on microstructure of Mg-RE alloys during ageing and their role on ductility of the aged alloy is unclear.In this work,hot extrusion and ageing treatment were performed for Mg-9Gd-2Y-xNd-0.2Zr(x=1 wt.%and 3 wt.%)alloys,and grain boundary precipitates were formed in the extruded Mg-9Gd-2Y-3Nd-0.2Zr alloy due to the increase of Nd content.The extruded alloys exhibit a complete dynamic recrystallization(DRX)microstructure and a texture with the<0001>orientation parallel to the extrusion direction(ED).In addition,a large amount of fiber microstructures distributed by the second phase along the ED were formed in the Mg-9Gd-2Y-3Nd-0.2Zr alloy,while only a small amount of the second phase was observed in the Mg-9Gd-2Y-1Nd-0.2Zr alloy.After ageing treatment,a large amount ofβ'phase precipitated inside the grains.The strength of the Mg-9Gd-2Y-1Nd-0.2Zr alloy increased from 202 MPa to 275 MPa but the elongation decreased from 12.8%to 2.6%,and the strength of the Mg-9Gd-2Y-3Nd-0.2Zr alloy increased from 212 MPa to 281 MPa but the elongation decreased from 13.7%to 6.2%.Among them,the Mg-9Gd-2Y-3Nd-0.2Zr alloy showed good overall mechanical properties,especially the elongation of the aged alloy was 58%higher than that of the Mg-9Gd-2Y-1Nd-0.2Zr alloy.The increase in ductility of the aged Mg-9Gd-2Y-3Nd-0.2Zr alloy attributed to the grain boundary precipitate promotes the formation of a large number of precipitation free zones(PFZs)with widths of 130-150 nm during ageing treatment. 展开更多
关键词 Mg alloy grain boundary precipitate precipitation free zone DUCTILITY
在线阅读 下载PDF
Al-Zn-Mg-Cu合金的局部腐蚀行为与Zn、Mg含量的关系 被引量:8
2
作者 谢娟 孟立春 +3 位作者 陈江华 杨修波 刘吉梓 刘春辉 《中国有色金属学报》 EI CAS CSCD 北大核心 2017年第12期2473-2482,共10页
研究了峰值时效状态下,不同Zn、Mg含量(质量分数)对高Cu含量(2.0%~2.5%)的Al-Zn-Mg-Cu合金耐局部腐蚀能力的影响,利用透射电镜和扫描电镜表征了合金局部腐蚀行为与其微观结构之间的关系。结果表明:对Mg含量不同的两组目标合金,Zn含量降... 研究了峰值时效状态下,不同Zn、Mg含量(质量分数)对高Cu含量(2.0%~2.5%)的Al-Zn-Mg-Cu合金耐局部腐蚀能力的影响,利用透射电镜和扫描电镜表征了合金局部腐蚀行为与其微观结构之间的关系。结果表明:对Mg含量不同的两组目标合金,Zn含量降低,合金的耐局部腐蚀能力变差;对应比较Mg含量不同的两组合金,初始阶段低Mg组合金的耐晶间腐蚀能力较差,但深度发展阶段低Mg组合金的耐晶间腐蚀能力较好;前期阶段高Mg组合金的耐剥蚀能力较好,但后期深度腐蚀阶段,高Mg组合金的耐剥蚀能力变得较差。 展开更多
关键词 AL-ZN-MG-CU合金 局部腐蚀 微观组织 晶界无沉淀析出带 连续体颗粒
在线阅读 下载PDF