Methoxy poly(ethylene glycol)-poly(D,L-lactide) block copolymers (PEG-PLA) were prepared through ring-opening polymerization.The oil in water suspension method was used to prepare block copolymer micelles. The critica...Methoxy poly(ethylene glycol)-poly(D,L-lactide) block copolymers (PEG-PLA) were prepared through ring-opening polymerization.The oil in water suspension method was used to prepare block copolymer micelles. The critical micelle concentration (CMC) by fluorescence spectroscopy was 0.0056 mg·ml -1 . The physical state of the inner core region of micelles was characterized with 1HNMR. The size of indomethacin (IMC) loaded micelles measured by dynamic light scattering (DLS) showed narrow monodisperse size distribution and the average diameters were less than 50 nm. In addition, the nanoparticles with relatively high drug loading content (DLC) were obtained.展开更多
为得到聚乳酸的最佳制备工艺,利用微波辐射技术实现D,L-丙交酯开环聚合制备聚乳酸,实验考查了催化剂种类和用量,微波辐照功率和时间等工艺参数对产物分子量的影响,以及反应过程中体系温度的变化.研究表明,以连续微波炉作为反应器,催化剂...为得到聚乳酸的最佳制备工艺,利用微波辐射技术实现D,L-丙交酯开环聚合制备聚乳酸,实验考查了催化剂种类和用量,微波辐照功率和时间等工艺参数对产物分子量的影响,以及反应过程中体系温度的变化.研究表明,以连续微波炉作为反应器,催化剂Sn(Oct)2用量为丙交酯单体用量的0.56%(质量分数),在功率为90 W的连续微波辐射下反应10 m in,可获得粘均分子量(Mη)为15.92×104的聚乳酸(PDLLA).与家用微波炉相比,采用连续微波炉反应器,可在较短的反应时间内获得较高产率的聚乳酸产物.展开更多
文摘Methoxy poly(ethylene glycol)-poly(D,L-lactide) block copolymers (PEG-PLA) were prepared through ring-opening polymerization.The oil in water suspension method was used to prepare block copolymer micelles. The critical micelle concentration (CMC) by fluorescence spectroscopy was 0.0056 mg·ml -1 . The physical state of the inner core region of micelles was characterized with 1HNMR. The size of indomethacin (IMC) loaded micelles measured by dynamic light scattering (DLS) showed narrow monodisperse size distribution and the average diameters were less than 50 nm. In addition, the nanoparticles with relatively high drug loading content (DLC) were obtained.
文摘为得到聚乳酸的最佳制备工艺,利用微波辐射技术实现D,L-丙交酯开环聚合制备聚乳酸,实验考查了催化剂种类和用量,微波辐照功率和时间等工艺参数对产物分子量的影响,以及反应过程中体系温度的变化.研究表明,以连续微波炉作为反应器,催化剂Sn(Oct)2用量为丙交酯单体用量的0.56%(质量分数),在功率为90 W的连续微波辐射下反应10 m in,可获得粘均分子量(Mη)为15.92×104的聚乳酸(PDLLA).与家用微波炉相比,采用连续微波炉反应器,可在较短的反应时间内获得较高产率的聚乳酸产物.