Characterization and recycling of nickel- and chromium-contained pickling sludge generated in production of stainless steel 被引量:13
1
作者 李小明 谢庚 +2 位作者 HOJAMBERDIEV Mirabbos 崔雅茹 赵俊学 《Journal of Central South University》 SCIE EI CAS 2014年第8期3241-3246,共6页
Pickling sludge generated during the neutralization of pickling wastewater with calcium hydroxide in stainless steel pickling process was characterized using X-ray fluorescence spectrometry, X-ray diffractometry, scan... Pickling sludge generated during the neutralization of pickling wastewater with calcium hydroxide in stainless steel pickling process was characterized using X-ray fluorescence spectrometry, X-ray diffractometry, scanning electron microscopy, thermogravimetry and differential scanning calorimetry, etc. The major compositions of pickling sludge are CaF2, CaSO4, Me(OH), (M: Fe, Cr, Ni), and the content of CaF2 is high in the sludge. The melting point of pickling sludge is about 1350℃ and the viscosity is about 0.14 Pa.s at 1450 ℃, which are comparatively lower than those of normal refining slag. After heat treatment, the contents of sulfur and fluorine in the pickling sludge were reduced, confirming the thermal decomposition of sulfate in the sludge. Fluorine in the sludge is reduced by the gaseous SiF4 and A1F3 generated through the reactions of CaF2 with SiO2 and Al2O3. The preliminary results from the reduction test indicate that the sulfur content in the steel is not affected by the presence of sulfur in the sludge. The recovery of nickel is about 40%, and the chromium content changes marginally due to the protective atmosphere under the reduction condition of chromic oxide. The pickling sludge is a potential auxiliary material for the production of stainless steel. 展开更多
关键词 stainless steel pickling sludge CHARACTERIZATION RECYCLING SULFUR FLUORINE
在线阅读 下载PDF
Acid-pickling plates and strips speed control system by microwave heating based on self-adaptive fuzzy PID algorithm 被引量:7
2
作者 杨彪 彭金辉 +3 位作者 郭胜惠 张世敏 李玮 何涛 《Journal of Central South University》 SCIE EI CAS 2012年第8期2179-2186,共8页
Double self-adaptive fuzzy PID algorithm-based control strategy was proposed to construct quasi-cascade control system to control the speed of the acid-pickling process of titanium plates and strips. It is very useful... Double self-adaptive fuzzy PID algorithm-based control strategy was proposed to construct quasi-cascade control system to control the speed of the acid-pickling process of titanium plates and strips. It is very useful in overcoming non-linear dynamic behavior, uncertain and time-varying parameters, un-modeled dynamics, and couples between the automatic turbulence control (ATC) and the automatic acid temperature control (AATC) with varying parameters during the operation process. The quasi-cascade control system of inner and outer loop self-adaptive fuzzy PID controller was built, which could effectively control the pickling speed of plates and strips. The simulated results and real application indicate that the plates and strips acid pickling speed control system has good performances of adaptively tracking the parameter variations and anti-disturbances, which ensures the match of acid pickling temperature and turbulence of flowing with acid pickling speed, improving the surface quality of plates and strips acid pickling, and energy efficiency. 展开更多
关键词 self-adaptive fuzzy PID algorithm microwave heating acid pickling plates and strips mixed-acid media
在线阅读 下载PDF
Corrosion leaking of preheater weldment in alumina factories
3
作者 张利 陈文汨 +1 位作者 龚竹青 刘红召 《Journal of Central South University of Technology》 EI 2005年第4期443-447,共5页
Stress corrosion cracking (SCC) and anticorrosion measures of TU42C weld-joint were studied by constant load experiments and pickling experiments. The results show that in 40%(mass fraction) NaOH solution at 110℃, ca... Stress corrosion cracking (SCC) and anticorrosion measures of TU42C weld-joint were studied by constant load experiments and pickling experiments. The results show that in 40%(mass fraction) NaOH solution at 110℃, caustic SCC occurs in TU42C weld-joints at the applied potential of-1020mV(vs SCE) for 3d while at the potential of-950mV(vs SCE) for 10d. All the cracks are intergranular. In the 10% sulfuric acid, the cracks have the most negative self-corrosion potential-432.5mV(vs SCE) and are active to be further corroded by the acid. Because of the same corrosion behaviour as the lab weldment, preheater’s cracking in alumina factories is attributed to the combining actions of previous caustic SCC in Bayer solutions and continuous acid corrosion by pickling with the addition of RD. The following measures are effective to prevent the corrosion failure of preheater, such as postweld heat treatment at 620℃ to relax the residual weld stress, addition of CC3 and L826 as the corrosion inhibitors to improve the pickling and cleaning by the high pressure water instead of by pickling. 展开更多
关键词 stress corrosion crackingl constant load experimentl pickling corrosion inhibitor postweld heat treatment