CuO added Pb_(0.92)Sr_(0.06)Ba_(0.02)(Mg_(1/3)Nb_(2/3))_(0.25)(Ti_(0.53)Zr_(0.47))_(0.75)O_3 ceramics sintered with Ag electrodes at 900℃ for multilayer piezoelectric actuator 被引量:1
1
作者 Muhammad Adnan Qaiser Ahmad Hussain +4 位作者 徐玉青 汪尧进 王一平 杨颖 袁国亮 《Chinese Physics B》 SCIE EI CAS CSCD 2017年第3期539-544,共6页
CuO added Pb0.92Sr0.06Ba0.02(Mg1/3Nb2/3)0.25(Ti0.53Zr0.47)0.75O3 ceramics were studied to prepare high-quality multilayer piezoelectric actuators with pure Ag electrodes at 900 ℃. CuO addition not only reduced th... CuO added Pb0.92Sr0.06Ba0.02(Mg1/3Nb2/3)0.25(Ti0.53Zr0.47)0.75O3 ceramics were studied to prepare high-quality multilayer piezoelectric actuators with pure Ag electrodes at 900 ℃. CuO addition not only reduced the sintering temperature significantly from 1260 ℃ to 900 ℃ but also improved the ceramic density to 7.742 g/cm3. The 0.7 wt.% CuO added ceramic sintered at 900 ℃ shows the remnant polarization (Pr) of 40 μC/cm2, 0.28% strain at 40 kV/cm, and the piezoelectric coefficient (d33) of 630 pC/N. This ceramic shows a strong relaxor characteristic with a Curie temperature of 200 ℃. Furthermore, the 0.7 wt.% CuO added ceramic and pure Ag electrodes were co-fired at 900 ℃ to prepare a high-quality multilayer piezoelectric actuator with a d33 of over 450 pC/N per ceramic layer. 展开更多
关键词 piezoelectric ceramics low-temperature co-fired ceramic multilayer piezoelectric actuators
在线阅读 下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部