EAB zeolite was successfully prepared and applied to selective adsorption of Li^(+),Na^(+)and K^(+)ions.The physical and chemical properties of the adsorbent were characterized by X-ray diffraction(XRD),X-ray fluoresc...EAB zeolite was successfully prepared and applied to selective adsorption of Li^(+),Na^(+)and K^(+)ions.The physical and chemical properties of the adsorbent were characterized by X-ray diffraction(XRD),X-ray fluorescence(XRF),scanning electron microscope(SEM)and thermogravimetry(TG)methods.The ion exchange behaviours for Li^(+),Na^(+)and K^(+)ions in monomcomponent and multicomponent solutions were studied.In independent ion exchange,the ion exchange capacities ratiosα(/Na/Li)andα(K/Li)were 3.8 and 6.2,respectively.In competitive ion exchange,the selectivitiesβ(Na/Li)andβ(K/Li)increased with the initial concentrations and reached 409 and 992 when the initial concentrations was 100 mmol/L.The thermodynamic study results showed that Gibbs free energy change(ΔGΘ)of ion exchange reaction between Li-EAB and K^(+)was-34.96 kJ/mol,indicating that ion exchange of K^(+)ions was more energetically favourable than Li^(+)ions.The calculation results showed that the energy barriers of ion exchange increased in the order K^(+)Na^(+)<Li^(+).The study shows that EAB zeolite is potential to be used in the separation of alkali ions.展开更多
The 3D hollow hierarchi-cal architectures tend to be designed for inhibiting stack of MXene flakes to obtain satisfactory lightweight,high-e cient and broadband absorbers.Herein,the hollow NiCo compound@MXene networks...The 3D hollow hierarchi-cal architectures tend to be designed for inhibiting stack of MXene flakes to obtain satisfactory lightweight,high-e cient and broadband absorbers.Herein,the hollow NiCo compound@MXene networks were prepared by etching the ZIF 67 template and subsequently anchoring the Ti_(3)C_(2)Tx nanosheets through electrostatic self-assembly.The electromagnetic parameters and microwave absorption property can be distinctly or slightly regulated by adjusting the filler loading and decoration of Ti_(3)C_(2)Tx nanoflakes.Based on the synergistic e ectsof multi-components and special well-constructed structure,NiCo layered double hydroxides@Ti_(3)C_(2)Tx(LDHT-9)absorber remarkably achieves unexpected e ective absorption bandwidth(EAB)of 6.72 GHz with a thickness of 2.10 mm,covering the entire Ku-band.After calcination,transition metal oxide@Ti_(3)C_(2)Tx(TMOT-21)absorber near the percolation threshold possesses minimum reflection loss(RLmin)value of-67.22 dB at 1.70 mm within a filler loading of only 5 wt%.This work enlightens a simple strategy for constructing MXene-based composites to achieve high-e cient microwave absorbents with lightweight and tunable EAB.展开更多
文摘EAB zeolite was successfully prepared and applied to selective adsorption of Li^(+),Na^(+)and K^(+)ions.The physical and chemical properties of the adsorbent were characterized by X-ray diffraction(XRD),X-ray fluorescence(XRF),scanning electron microscope(SEM)and thermogravimetry(TG)methods.The ion exchange behaviours for Li^(+),Na^(+)and K^(+)ions in monomcomponent and multicomponent solutions were studied.In independent ion exchange,the ion exchange capacities ratiosα(/Na/Li)andα(K/Li)were 3.8 and 6.2,respectively.In competitive ion exchange,the selectivitiesβ(Na/Li)andβ(K/Li)increased with the initial concentrations and reached 409 and 992 when the initial concentrations was 100 mmol/L.The thermodynamic study results showed that Gibbs free energy change(ΔGΘ)of ion exchange reaction between Li-EAB and K^(+)was-34.96 kJ/mol,indicating that ion exchange of K^(+)ions was more energetically favourable than Li^(+)ions.The calculation results showed that the energy barriers of ion exchange increased in the order K^(+)Na^(+)<Li^(+).The study shows that EAB zeolite is potential to be used in the separation of alkali ions.
基金supported by the National Natural Science Foundation of China(No.52073010)Beijing Natural Science Foundation(2214069)。
文摘The 3D hollow hierarchi-cal architectures tend to be designed for inhibiting stack of MXene flakes to obtain satisfactory lightweight,high-e cient and broadband absorbers.Herein,the hollow NiCo compound@MXene networks were prepared by etching the ZIF 67 template and subsequently anchoring the Ti_(3)C_(2)Tx nanosheets through electrostatic self-assembly.The electromagnetic parameters and microwave absorption property can be distinctly or slightly regulated by adjusting the filler loading and decoration of Ti_(3)C_(2)Tx nanoflakes.Based on the synergistic e ectsof multi-components and special well-constructed structure,NiCo layered double hydroxides@Ti_(3)C_(2)Tx(LDHT-9)absorber remarkably achieves unexpected e ective absorption bandwidth(EAB)of 6.72 GHz with a thickness of 2.10 mm,covering the entire Ku-band.After calcination,transition metal oxide@Ti_(3)C_(2)Tx(TMOT-21)absorber near the percolation threshold possesses minimum reflection loss(RLmin)value of-67.22 dB at 1.70 mm within a filler loading of only 5 wt%.This work enlightens a simple strategy for constructing MXene-based composites to achieve high-e cient microwave absorbents with lightweight and tunable EAB.