The hydraulic roll-bending device was studied, which was widely used in modem cold rolling mills to regulate the strip flatness. The loaded roll gap crown mathematic model and the strip crown mathematic model of the r...The hydraulic roll-bending device was studied, which was widely used in modem cold rolling mills to regulate the strip flatness. The loaded roll gap crown mathematic model and the strip crown mathematic model of the reversing cold rolling process were established, and the deformation model of roll stack system of the 6-high 1 250 mm high crown (HC) reversing cold rolling mill was built by slit beam method. The simulation results show that, the quadratic component of strip crown decreases nearly linearly with the increase of the work roll bending force, when the shifting value of intermediate roll is determined by the rolling process. From the first pass to the fifth pass of reversing rolling process, the crown controllability of bending force is gradually weakened. Base on analyzing the relationship among the main factors associated with roll-bending force in reversing multi-pass rolling, such as strip width and rolling force, a preset mathematic model of bending force is developed by genetic algorithm. The simulation data demonstrate that the relative deviation of flatness criterions in each rolling pass is improved significantly and the mean relative deviation of all five passes is decreased from 25.1% to 1.7%. The model can keep good shape in multi-pass reversing cold rolling process with the high prediction accuracy and can be used to guide the production process.展开更多
The dynamic model of cold rolling mill based on strip flatness and thickness integrated control was proposed,containing the following sub-models:the rolling process model,the dynamic model of rolls along axial directi...The dynamic model of cold rolling mill based on strip flatness and thickness integrated control was proposed,containing the following sub-models:the rolling process model,the dynamic model of rolls along axial direction,and the compensation model.Based on the rule of volume flow rate,the dynamic rolling process model was built.The work roll and backup roll were taken as elastic continuous bodies,the effect of shear and moment of inertia were taken into consideration,and then the dynamic model of rolls was built.The two models were coupled together,and the dynamic model of rolling mill was built.In the dynamic model,the thermal expansion of the rolls,the wear of the rolls and other related parameters can not be considered.In order to compensate the dynamic model,the coupled static model of rolls and strip was applied.Then,according to the inner relationship of these models,the dynamic model and the compensation model were coupled,and the dynamic model of rolling mill based on the strip flatness and thickness integrated control was built.The dynamic simulation of the rolling process was made,and the dynamic thickness and the dynamic flatness information were obtained.This model not only provides a theory basis for the virtual rolling,but also provides a platform for the application of advanced control theory.展开更多
A high-precision shape detecting system of cold rolling strip is developed to meet industrial application, which mainly consists of the shape detecting roller, the collecting ring, the digital signal processing (DSP...A high-precision shape detecting system of cold rolling strip is developed to meet industrial application, which mainly consists of the shape detecting roller, the collecting ring, the digital signal processing (DSP) shape signal processing board and the shape control model. Based on the shape detecting principle, the shape detecting roller is designed with a new integral structure for improving the precision of shape detecting and avoiding scratching strip surface. Based on the DSP technology, the DSP shape signal processing circuit board is designed and embedded in the shape detecting system for the reliability and stability of shape signal processing. The shape detecting system was successfully used in Angang 1 250 mm HC 6-high reversible cold rolling mill. The precision of shape detecting is 0.2 I and the shape deviation is controlled within 6 1 after the close loop shape control is input.展开更多
In order to know the cause of cracks in cold rolling of QSn6.5 0.1 copper alloy strip, a lot of experiments and analysis were done. The microstructure changes of QSn6.5 0.1 were investigated by means of metallurgical ...In order to know the cause of cracks in cold rolling of QSn6.5 0.1 copper alloy strip, a lot of experiments and analysis were done. The microstructure changes of QSn6.5 0.1 were investigated by means of metallurgical microscope. The morphology of cracks and surface defects were examined using scanning electron microscope. Macroscopic residual stresses produced in every process during manufacturing in the QSn6.5 0.1 strip were measured by X ray diffraction method and hole drilling method. The results show that the cracks in the QSn6.5 0.1 cold rolling strip were caused due to the derivation of metallurgical defects, such as SnO 2, S, fine looses,the inverse segregation unable to clear up when milling, and the accumulation of all kinds of resi dual stresses. When the accumulation of the residual stress reaches the material′s breaking strength, the cracks will be generated. Several measures to avoid the development of these kinds of cracks were put forward, such as: controlling the casting technology, improving homogenization annealing procedure (680 ℃/7 h) and milling quality(using the second milling when necessary), working out a more reasonable rolling technology to ensure intermediate annealing in time.展开更多
Aiming at accuracy control of the thermal crown of work rolls in cold rolling,new parameters such as regulation domain and control-efficiency factors were proposed and a numerical analysis model of the thermal crown o...Aiming at accuracy control of the thermal crown of work rolls in cold rolling,new parameters such as regulation domain and control-efficiency factors were proposed and a numerical analysis model of the thermal crown of work rolls was established using finite difference method to study roll's thermal deformation.Based on simulation results,the influences of control-efficiency factors on thermal crown are presented and the thermal crown of work rolls is analyzed after taking sub-cooling of sprinkling beam into consideration.It has been found that the control-efficiency factor of any position on the roll's surface is linear function of the temperature and the control ability of water temperature is stronger than other control parameters.In addition,the verification of the model has been carried out based on the producing technology data in some factories and the numerical simulation results coincide well with the experimental data.Therefore,this work has important value for on-line control of roll's crown in cold rolling.展开更多
Due to the complexity of investigating deformation mechanisms in helical rolling(HR) process with traditional analytical method, it is significant to develop a 3D finite element(FE) model of HR process. The key formin...Due to the complexity of investigating deformation mechanisms in helical rolling(HR) process with traditional analytical method, it is significant to develop a 3D finite element(FE) model of HR process. The key forming conditions of cold HR of bearing steel-balls were detailedly described. Then, by taking steel-ball rolling elements of the B7008 C angular contact ball bearing as an example, a completed 3D elastic-plastic FE model of cold HR forming process was established under SIMUFACT software environment. Furthermore, the deformation characteristics in HR process were discovered, including the forming process, evolution and distribution laws of strain, stress and damage based on Lemaitre relative damage model. The results reveal that the central loosening and cavity defects in HR process may have a combined effect of large negative hydrostatic pressure(positive mean stress)caused by multi-dimensional tensile stresses, high level transverse tensile stress, and circular-alternating shear stress in cross section.展开更多
This article examines the influence of annealing temperature on fracture toughness and forming limit curves of dissimilar aluminum/silver sheets.In the cold roll bonding process,after brushing and acid washing,the pre...This article examines the influence of annealing temperature on fracture toughness and forming limit curves of dissimilar aluminum/silver sheets.In the cold roll bonding process,after brushing and acid washing,the prepared surfaces are placed on top of each other and by rolling with reduction more than 50%,the bonding between layers is established.In this research,the roll bonding process was done at room temperature,without the use of lubricants and with a 70%thickness reduction.Then,the final thickness of the Ag/Al bilayer sheet reached 350μm by several stages of cold rolling.Before cold rolling,it should be noted that to decrease the hardness created due to plastic deformation,the roll-bonded samples were subjected to annealing heat treatment at 400℃for 90 min.Thus,the final samples were annealed at 200,300 and 400℃for 90 min and cooled in a furnace to examine the annealing temperature effects.The uniaxial tensile and microhardness tests measured mechanical properties.Also,to investigate the fracture mechanism,the fractography of the cross-section was examined by scanning electron microscope(SEM).To evaluate the formability of Ag/Al bilayer sheets,forming limit curves were obtained experimentally through the Nakazima test.The resistance of composites to failure due to cracking was also investigated by fracture toughness.The results showed that annealing increases the elongation and formability of the Ag/Al bilayer sheet while reduces the ultimate tensile strength and fracture toughness.However,the changing trend is not the same at different temperatures,and according to the results,the most significant effect is obtained at 300℃and aluminum layers.It was also determined that by increasing annealing temperature,the fracture mechanism from shear ductile with small and shallow dimples becomes ductile with deep cavities.展开更多
Electroshocking treatment(EST),an efficient and rapid material treatment method,promotes microstructure evolution and improves mechanical properties.This study incorporates EST into the conventional cold rolling-quenc...Electroshocking treatment(EST),an efficient and rapid material treatment method,promotes microstructure evolution and improves mechanical properties.This study incorporates EST into the conventional cold rolling-quenching tempering process of M50 steel and investigates the influence and mechanism of applying EST at different stages of the process on the microstructure and mechanical properties.Scanning electron microscope(SEM),transmission electron microscope(TEM),and X-ray diffraction(XRD)were used to characterize the effect of EST on microstructure.The results show that EST can refine the grains of M50(average reduction of 10.1%in grain size),homogenize the grain size distribution,reduce the dislocation density(20.9%in average),promote the dissolution of carbides in the matrix and distribute them more uniformly along the grain boundaries,resulting in the improvement of mechanical properties.The mechanical properties of the specimen with the process flow of rolling-quenching-tempering-electroshocking showed excellent performance,with an increase in hardness of 1.4%,tensile strength of 17.7%,and elongation at break of 24.3%as compared to the specimen without EST.The tensile properties of the specimen with the process flow of rolling electroshocking-quenching-tempering showed the best performance,with an increase in tensile strength of 30.0%and elongation at break of 30.7%as compared to the specimen without EST.展开更多
Wire-arc additive manufacture(WAAM)has great potential for manufacturing of Al-Cu components.However,inferior mechanical properties of WAAM deposited material restrict its industrial application.Inter-layer cold rolli...Wire-arc additive manufacture(WAAM)has great potential for manufacturing of Al-Cu components.However,inferior mechanical properties of WAAM deposited material restrict its industrial application.Inter-layer cold rolling and thermo-mechanical heat treatment(T8)with pre-stretching deformation between solution and aging treatment were adopted in this study.Their effects on hardness,mechanical properties and microstructure were analyzed and compared to the conventional heat treatment(T6).The results show that cold rolling increases the hardness and strengths,which further increase with T8 treatment.The ultimate tensile strength(UTS)of 513 MPa and yield stress(YS)of 413 MPa can be obtained in the inter-layer cold-rolled sample with T8 treatment,which is much higher than that in the as-deposited samples.The cold-rolled samples show higher elongation than that of as-deposited ones due to significant elimination of porosity in cold rolling;while both the T6 and T8 treatments decrease the elongation.The cold rolling and pre-stretching deformation both contribute to the formation of dense and dispersive precipitatedθ′phases,which inhibits the dislocation movement and enhances the strengths;as a result,T8 treatment shows better strengthening effect than the T6 treatment.The strengthening mechanism was analyzed and it was mainly related to work hardening and precipitation strengthening.展开更多
基金Project(20050311890) supported by the Science and Technology Development Foundation of University of Science and Technology Beijing,China
文摘The hydraulic roll-bending device was studied, which was widely used in modem cold rolling mills to regulate the strip flatness. The loaded roll gap crown mathematic model and the strip crown mathematic model of the reversing cold rolling process were established, and the deformation model of roll stack system of the 6-high 1 250 mm high crown (HC) reversing cold rolling mill was built by slit beam method. The simulation results show that, the quadratic component of strip crown decreases nearly linearly with the increase of the work roll bending force, when the shifting value of intermediate roll is determined by the rolling process. From the first pass to the fifth pass of reversing rolling process, the crown controllability of bending force is gradually weakened. Base on analyzing the relationship among the main factors associated with roll-bending force in reversing multi-pass rolling, such as strip width and rolling force, a preset mathematic model of bending force is developed by genetic algorithm. The simulation data demonstrate that the relative deviation of flatness criterions in each rolling pass is improved significantly and the mean relative deviation of all five passes is decreased from 25.1% to 1.7%. The model can keep good shape in multi-pass reversing cold rolling process with the high prediction accuracy and can be used to guide the production process.
基金Project(E2012203177)supported by the Natural Science Foundation of Hebei Province,ChinaProject(2011BAF15B01)supported by the National Science and Technology Support Plan of China+1 种基金Project(E2006001038)supported by Great Natural Science Foundation of Hebei Province,ChinaProject(NECSR-201202)supported by Open Project Program of National Engineering Research Center for Equipment and Technology of Cold Strip Rolling,China
文摘The dynamic model of cold rolling mill based on strip flatness and thickness integrated control was proposed,containing the following sub-models:the rolling process model,the dynamic model of rolls along axial direction,and the compensation model.Based on the rule of volume flow rate,the dynamic rolling process model was built.The work roll and backup roll were taken as elastic continuous bodies,the effect of shear and moment of inertia were taken into consideration,and then the dynamic model of rolls was built.The two models were coupled together,and the dynamic model of rolling mill was built.In the dynamic model,the thermal expansion of the rolls,the wear of the rolls and other related parameters can not be considered.In order to compensate the dynamic model,the coupled static model of rolls and strip was applied.Then,according to the inner relationship of these models,the dynamic model and the compensation model were coupled,and the dynamic model of rolling mill based on the strip flatness and thickness integrated control was built.The dynamic simulation of the rolling process was made,and the dynamic thickness and the dynamic flatness information were obtained.This model not only provides a theory basis for the virtual rolling,but also provides a platform for the application of advanced control theory.
基金Foundation item: Project(2009AA04Z143) supported by the National High Technology Research and Development Program of ChinaProject (E2011203004) supported by Natural Science Foundation of Hebei Province, ChinaProjects(2011BAF15B03, 2011BAF15B02) supported by the National Science Plan of China
文摘A high-precision shape detecting system of cold rolling strip is developed to meet industrial application, which mainly consists of the shape detecting roller, the collecting ring, the digital signal processing (DSP) shape signal processing board and the shape control model. Based on the shape detecting principle, the shape detecting roller is designed with a new integral structure for improving the precision of shape detecting and avoiding scratching strip surface. Based on the DSP technology, the DSP shape signal processing circuit board is designed and embedded in the shape detecting system for the reliability and stability of shape signal processing. The shape detecting system was successfully used in Angang 1 250 mm HC 6-high reversible cold rolling mill. The precision of shape detecting is 0.2 I and the shape deviation is controlled within 6 1 after the close loop shape control is input.
文摘In order to know the cause of cracks in cold rolling of QSn6.5 0.1 copper alloy strip, a lot of experiments and analysis were done. The microstructure changes of QSn6.5 0.1 were investigated by means of metallurgical microscope. The morphology of cracks and surface defects were examined using scanning electron microscope. Macroscopic residual stresses produced in every process during manufacturing in the QSn6.5 0.1 strip were measured by X ray diffraction method and hole drilling method. The results show that the cracks in the QSn6.5 0.1 cold rolling strip were caused due to the derivation of metallurgical defects, such as SnO 2, S, fine looses,the inverse segregation unable to clear up when milling, and the accumulation of all kinds of resi dual stresses. When the accumulation of the residual stress reaches the material′s breaking strength, the cracks will be generated. Several measures to avoid the development of these kinds of cracks were put forward, such as: controlling the casting technology, improving homogenization annealing procedure (680 ℃/7 h) and milling quality(using the second milling when necessary), working out a more reasonable rolling technology to ensure intermediate annealing in time.
基金Project(2007BAF02B12)supported by the National Science Technology Support Program of ChinaProjects(E2011203090,E2012203028)supported by the Natural Science Foundation of Hebei Province,China
文摘Aiming at accuracy control of the thermal crown of work rolls in cold rolling,new parameters such as regulation domain and control-efficiency factors were proposed and a numerical analysis model of the thermal crown of work rolls was established using finite difference method to study roll's thermal deformation.Based on simulation results,the influences of control-efficiency factors on thermal crown are presented and the thermal crown of work rolls is analyzed after taking sub-cooling of sprinkling beam into consideration.It has been found that the control-efficiency factor of any position on the roll's surface is linear function of the temperature and the control ability of water temperature is stronger than other control parameters.In addition,the verification of the model has been carried out based on the producing technology data in some factories and the numerical simulation results coincide well with the experimental data.Therefore,this work has important value for on-line control of roll's crown in cold rolling.
基金Project(2011CB706605)supported by the National Basic Research Program of ChinaProject(IRT13087)supported by the Innovative Research Team Development Program of Ministry of Education of ChinaProject(2012-86)supported by the Grant from the High-end Talent Leading Program of Hubei Province,China
文摘Due to the complexity of investigating deformation mechanisms in helical rolling(HR) process with traditional analytical method, it is significant to develop a 3D finite element(FE) model of HR process. The key forming conditions of cold HR of bearing steel-balls were detailedly described. Then, by taking steel-ball rolling elements of the B7008 C angular contact ball bearing as an example, a completed 3D elastic-plastic FE model of cold HR forming process was established under SIMUFACT software environment. Furthermore, the deformation characteristics in HR process were discovered, including the forming process, evolution and distribution laws of strain, stress and damage based on Lemaitre relative damage model. The results reveal that the central loosening and cavity defects in HR process may have a combined effect of large negative hydrostatic pressure(positive mean stress)caused by multi-dimensional tensile stresses, high level transverse tensile stress, and circular-alternating shear stress in cross section.
基金Project(4013311)supported by the National Science Foundation of Iran(INSF)。
文摘This article examines the influence of annealing temperature on fracture toughness and forming limit curves of dissimilar aluminum/silver sheets.In the cold roll bonding process,after brushing and acid washing,the prepared surfaces are placed on top of each other and by rolling with reduction more than 50%,the bonding between layers is established.In this research,the roll bonding process was done at room temperature,without the use of lubricants and with a 70%thickness reduction.Then,the final thickness of the Ag/Al bilayer sheet reached 350μm by several stages of cold rolling.Before cold rolling,it should be noted that to decrease the hardness created due to plastic deformation,the roll-bonded samples were subjected to annealing heat treatment at 400℃for 90 min.Thus,the final samples were annealed at 200,300 and 400℃for 90 min and cooled in a furnace to examine the annealing temperature effects.The uniaxial tensile and microhardness tests measured mechanical properties.Also,to investigate the fracture mechanism,the fractography of the cross-section was examined by scanning electron microscope(SEM).To evaluate the formability of Ag/Al bilayer sheets,forming limit curves were obtained experimentally through the Nakazima test.The resistance of composites to failure due to cracking was also investigated by fracture toughness.The results showed that annealing increases the elongation and formability of the Ag/Al bilayer sheet while reduces the ultimate tensile strength and fracture toughness.However,the changing trend is not the same at different temperatures,and according to the results,the most significant effect is obtained at 300℃and aluminum layers.It was also determined that by increasing annealing temperature,the fracture mechanism from shear ductile with small and shallow dimples becomes ductile with deep cavities.
基金Project(G202403)supported by the Open Foundation of The State Key Laboratory of Refractories and Metallurgy,ChinaProject(2022CFB378)supported by the Natural Science Foundation of Hubei Province,China+2 种基金Project(B 17034)supported by 111 Project,ChinaProject(IRT_17R83)supported by the Innovative Research Team Development Program of Ministry of Education of ChinaProject(P2024-026)supported by the Open Foundation of The State Key Laboratory of Materials Processing and Die&Mould Technology,China。
文摘Electroshocking treatment(EST),an efficient and rapid material treatment method,promotes microstructure evolution and improves mechanical properties.This study incorporates EST into the conventional cold rolling-quenching tempering process of M50 steel and investigates the influence and mechanism of applying EST at different stages of the process on the microstructure and mechanical properties.Scanning electron microscope(SEM),transmission electron microscope(TEM),and X-ray diffraction(XRD)were used to characterize the effect of EST on microstructure.The results show that EST can refine the grains of M50(average reduction of 10.1%in grain size),homogenize the grain size distribution,reduce the dislocation density(20.9%in average),promote the dissolution of carbides in the matrix and distribute them more uniformly along the grain boundaries,resulting in the improvement of mechanical properties.The mechanical properties of the specimen with the process flow of rolling-quenching-tempering-electroshocking showed excellent performance,with an increase in hardness of 1.4%,tensile strength of 17.7%,and elongation at break of 24.3%as compared to the specimen without EST.The tensile properties of the specimen with the process flow of rolling electroshocking-quenching-tempering showed the best performance,with an increase in tensile strength of 30.0%and elongation at break of 30.7%as compared to the specimen without EST.
基金Project(ZZYJKT2024-08)supported by the State Key Laboratory of Precision Manufacturing for Extreme Service Performance,ChinaProject(2022JB11GX004)supported by Selection of the best Candidates to Undertake Key Research Projects by Dalian City,ChinaProject(201806835007)supported by China Scholarship Council。
文摘Wire-arc additive manufacture(WAAM)has great potential for manufacturing of Al-Cu components.However,inferior mechanical properties of WAAM deposited material restrict its industrial application.Inter-layer cold rolling and thermo-mechanical heat treatment(T8)with pre-stretching deformation between solution and aging treatment were adopted in this study.Their effects on hardness,mechanical properties and microstructure were analyzed and compared to the conventional heat treatment(T6).The results show that cold rolling increases the hardness and strengths,which further increase with T8 treatment.The ultimate tensile strength(UTS)of 513 MPa and yield stress(YS)of 413 MPa can be obtained in the inter-layer cold-rolled sample with T8 treatment,which is much higher than that in the as-deposited samples.The cold-rolled samples show higher elongation than that of as-deposited ones due to significant elimination of porosity in cold rolling;while both the T6 and T8 treatments decrease the elongation.The cold rolling and pre-stretching deformation both contribute to the formation of dense and dispersive precipitatedθ′phases,which inhibits the dislocation movement and enhances the strengths;as a result,T8 treatment shows better strengthening effect than the T6 treatment.The strengthening mechanism was analyzed and it was mainly related to work hardening and precipitation strengthening.